High temperature oxidation of a commercial Cr‐Mn austenitic steel in air
Source abstract
Abstract
Abstract The oxidation of an austenitic steel containing 18% chromium and 12.3% manganese at 800‐1000°C in air occurs at a slower rate than that of a steel containing 9.5% chromium and 17.5% manganese. However, the rate of corrosion of this 18% chromium alloy is still large in comparison with the case of formation of a continuous chromia scale at the base of the scale layer. This result is attributed to the negative effect of the manganese on the thermodynamic stability of Cr2O3.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 10.1007/BF0065589910.1007/BF00655899 ↗
2. Zackay V. F. · Trans. ASM · 1956 · 48 · 509
3. 1964
4. 10.1149/1.241104510.1149/1.2411045 ↗
5. Giggins C. S. · Trans. Met. Soc. AIME · 1969 · 245 · 2495
6. 10.1007/BF0065657210.1007/BF00656572 ↗
7. Bénard J. · 1964
8. 10.1149/1.240427510.1149/1.2404275 ↗
9. 10.1007/BF0065812410.1007/BF00658124 ↗
10. 10.1149/1.242419810.1149/1.2424198 ↗
11. 10.1016/S0010-938X(67)80003-910.1016/S0010-938X(67)80003-9 ↗
12. 10.1002/maco.1970021110510.1002/maco.19700211105 ↗
13. 10.1007/BF0060348510.1007/BF00603485 ↗
14. I. G.Wright:Metals and Ceramics Information Center Rep. 72‐07 Battelle's Columbus Lab. Columbus Ohio June1972.
15. 10.1007/BF0060654210.1007/BF00606542 ↗
16. 10.1088/0034-4885/39/5/00110.1088/0034-4885/39/5/001 ↗
17. 10.5006/1.358193110.5006/1.3581931 ↗