journal article·2002-07

High temperature corrosion of cracking tubes

H. J. Grabke, D. Jakobi

Materials and Corrosion· Volume 53· Issue 7
Publisher page

Abstract

Coils for pyrolysis cracking of hydrocarbons are made of centrifugically cast FeNiCr-alloys and exposed to very severe conditions, high temperatures > 1050°C, oxidizing flue gases at the outside and carburizing atmosphere at the inside. Two tube sections have been investigated after some years operation. In the first case the tube wall was thoroughly carburized, the big size of the internal carbides indicated service at too high temperatures > 1100°C. At such temperatures the protective chromia scale fails by conversion to carbides, allowing ingress of carbon. At the outer wall surface obviously Cr was lost by evaporation as CrO2(OH)2 and CrO3 which is significant at high pO2 and high temperature. In the second case the tube had been operated at more moderate temperature, but showed creep cavities indicating loss of creep strength. This is due to repeated oxidation and loss of the scale by thermal cycling, this process has caused formation of a carbide denuded zone of considerable width at the outer side somewhat less wide at the inner wall. Besides oxide spallation, at the outer wall also evaporation will have played a role.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metal Alloys Wear and Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Grabke · Werkst. Korros. · (197 · 27 · 29110.1002/maco.19760270502 ↗
2. Schnaas · Oxid. Metals · (197 · 12 · 38710.1007/BF00612086 ↗
3. H. J. Grabke, A. Schnaas: In: W. Betteridge et al. (eds.) Alloy 800, North-Holland, Amsterrdam, 1978, pp. 195-21110.1007/BF00612086 ↗
4. Schnaas · Werkst. Korros. · (197 · 29 · 63510.1002/maco.19780291002 ↗
5. Grabke · Werkst. Korros. · (197 · 30 · 79410.1002/maco.19790301104 ↗
6. Steinkusch · Werkst. Korros. · (197 · 30 · 83710.1002/maco.19790301202 ↗
7. Ledjeff · Werkst. Korros. · (197 · 30 · 11
8. Ledjeff · Werkst. Korros. · (198 · 31 · 2
9. Chu · Oxid. Metals · (198 · 15 · 33110.1007/BF01058833 ↗
10. Hemtenmacher · Werkst. Korros. · (198 · 34 · 33310.1002/maco.19830340703 ↗
11. Hemptenmacher · Werkst. Korros. · (198 · 35 · 24710.1002/maco.19840350602 ↗
12. Grabke · Werkst. Korros. · (198 · 34 · 49510.1002/maco.19830341002 ↗
13. Wolf · Solid State Commun. · (198 · 54 · 510.1016/0038-1098(85)91021-X ↗
14. Grabke · Mater. Sci. Eng. · (198 · 87 · 22
15. Wolf · Oxid. Metals · (198 · 29 · 28910.1007/BF00751801 ↗
16. Rahmel · Mater. & Corr. · (199 · 49 · 22110.1002/(SICI)1521-4176(199804)49:4<221::AID-MACO221>3.0.CO;2-X ↗
17. H. J. Grabke: Carburization - A High Temperature Corrosion Phenomenon, MTI Publication No. 52, Materials Technology Inst. of the Chemical Process Industries, Inc. St. Louis, 1998.
18. H. Lange: Dissertation, RWTH Aachen 1983.
19. H. Asteman, J. E. Svensson, L. G. Johansson, M. Norell: Oxid. Metals 52 (1999) 95, 54 (2000) 11.10.1023/A:1018875024306 ↗
20. C. W. Wilke Diehl, P. C. Zeltzer, C. Willrich Klein: Trouble Shooting in a Modern Cracker Plant-Case Study, 3rd European Etylene Symposium, 21/22 May 2001, Nümbrecht.