Corrosion of aluminium in aliphatic amines and its inhibition by some dyes

J. D. Talati, N. H. Joshi

Materials and Corrosion· Volume 31· Issue 12
Publisher page

Abstract

Abstract Corrosion rates of aluminium alloys 2S, 3S, M57S and B26S in aqueous solutions of aliphatic amines and the inhibition efficiency of some dyes on the corrosion of 3S aluminium in these amines has been studied. The corrosion rate increases with the amine concentration up to 0.1 M and then decreases. The general order of corrosivity of amines is: tertiary < primary < secondary while for ethanolamines, the order is: tri‐ < di‐ < monoethanolamine. The order of corrosion susceptibility of different alloys in uninhibited amines M 57S < 2S < B26S < 3S. A rise in temperature increases the corrosion rate of 3S aluminium in 0.1 M amine with the energy of activation having an almost constant value of 48.9 kJ/mol in the temperature range 20–50° C. In 0.1 M methylamine, the inhibiting efficiency of different compounds (concentration 0.1%) increases in the order: alizarin red‐S (5.8%) < fluorescein sodium < eosin < congo red < phenol red < thymol blue < safranine‐T < methylene blue < rhodamine‐B (94.2%). The efficiency of rhodamine‐B for 3S aluminium in 0.1 M solutions of various amines in creases in the order: monoethanolamine (75.4%) < cyclohexylamine < n‐butylamine < triethylamine < n‐propylamine < diethylamine < trimethylamine < diethanolamine < ethylenediamine < triethanolamine < dimethylamine < ethylamine < methylamine (94.2%). The increase in corrosion potential of 3S aluminium in 0.1 M amine containing 0.1% rhodamine‐B and the galvanostatic polarization data indicate that the inhibitor has preponderant action on local anodes.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Material Properties and Applications · Corrosion Behavior and Inhibition · Advanced Energy Technologies and Civil Engineering Innovations

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. van Horn K. R. · 1967 · 274
2. Uhlig H. H. · 1961 · 46
3. Godard H. P. · 1967 · 14
4. Kirk‐Othmer · 1963 · 953
5. Laque F. L. · 1963 · 215
6. Evans U. R. · 1961 · 452
7. Hampel C. A. · 1963 · 129
8. S.Jiro S.Isao H.SeinoshinandH.Naomi: Japanese patent 7762 307
9. C. A. · 1978 · 88 · 9548j
10. Bell C. F. · 1977 · 131
11. 10.1002/maco.1959010020810.1002/maco.19590100208 ↗
12. Kato H. · Denki Kagaku · 1970 · 38 · 910.5796/kogyobutsurikagaku.38.9 ↗
13. H.Kotono F.Tanimoto Y.AizawaundT.Karamoto: Japanese patent 7367 142
14. C. A. · 1974 · 80 · 18568C
15. Yoshimura C. · Aruminyumu Kenkyu Kaishi · 1977 · 122 · 76
16. H.Yamada M.YoshizawaundT.Okamoto: Japanese patent 7260 496
17. C. A. · 1974 · 80 · 18575c
18. 10.1179/00070597479832126010.1179/000705974798321260 ↗
19. 10.1108/eb00696910.1108/eb006969 ↗
20. Vogel A. I. · 1975 · 441
21. 10.1179/00070597579832079210.1179/000705975798320792 ↗
22. Corr. Prev. Control. · 1977 · 24 · 6
23. Champion F. A. · 1963 · 191
24. Griffin R. W. · 1969 · 362
25. Rakoff H. · 1966 · 540
26. Uhlig H. H. · 1961 · 46
27. Bhastana C. T. · 1974 · 324
28. Gould E. S. · 1959 · 212
29. Bhastana C. T. · 1974 · 204
30. Lagowski J. J. · 1973 · 449
31. Adamson A. W. · 1973 · 639
32. Putilova I. N. · 1960 · 30
33. Hayakawa I. · Denki Kagaku · 1978 · 26 · 643
34. Machu W. · Werkstoffe u. Korrosion · 1975 · 8 · 3
35. 10.1149/1.349814810.1149/1.3498148 ↗
36. 10.1021/ie50531a03810.1021/ie50531a038 ↗
37. Mihara H. · Denki Kagaku · 1967 · 35 · 50210.5796/kogyobutsurikagaku.35.502 ↗
38. J. D.TalatiandN. H.Joshi: (Communicated).
39. Lucas H. J. · 1962 · 354
40. Siggia S. · 1967 · 417
41. Weast R. C. · 1962 · D‐87