The resistance of 20 Cr/25 Ni steels to carbon deposition. IV: The influence of alloy silicon content
Source abstract
Abstract
Abstract The carbon deposition behaviour of sheet specimens of nine experimental alloys, based on the composition of a 20 Cr/25 Ni/Nb stabilised steel but containing silicon in the range 0.0 to 2.23 w/o, has been studied. The tests were conducted in an environment of 75% CO/CO2 at 1 atmosphere total pressure at a temperature of 923 K. It was found that the resistance to carbon deposition increased with increasing silicon content. By using two heat treatments, it was shown, for steels containing ≲ 1.5 w/o Si, that the alloy's surface grain size was a key parameter in determining its response to carbon deposition; finegrained structures exhibited greater resistance than coarse‐grained. At the highest alloy silicon contents (1.8, 2.2 w/o), no effect of grain size was found. The results are interpreted in terms of the ease of formation of protective chromia and silica layers.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. 10.1016/S0010-938X(69)80097-110.1016/S0010-938X(69)80097-1 ↗
2. 10.1016/0025-5416(69)90047-010.1016/0025-5416(69)90047-0 ↗
3. 10.1016/S0010-938X(70)80061-010.1016/S0010-938X(70)80061-0 ↗
4. 10.1007/BF0065622510.1007/BF00656225 ↗
5. 10.1007/BF0065658010.1007/BF00656580 ↗
6. 10.1002/maco.1975026120510.1002/maco.19750261205 ↗
7. Walfe L. H.
8. van der Biest O. · 1980 · 681
9. 10.1002/maco.1987038030410.1002/maco.19870380304 ↗
10. 10.1002/maco.1987038040310.1002/maco.19870380403 ↗
11. R. A.Holm H. E.Evans:Werkst. Korros. this issue pp.219–224.