Abstract

In this paper, Al2O3/cerium oxide composite films were prepared on the surface of aluminum by anodic oxidation and chemical solution deposition. The aluminum was firstly anodized in sulfuric acid, then treated with different concentrations of Ce(NO3)3 · 6H2O solution at different temperatures. X‐ray diffraction (XRD), energy dispersive spectrometer (EDS), scanning electron microscope (SEM), electrochemical impedance spectroscopy (EIS), and electrochemical polarization tests were used to characterize the properties of the composite films. The results indicate that the Al2O3/cerium oxide composite films successfully form on 1060 Al alloy, and the best condition of film‐forming is 2 g/L Ce(NO3)3 · 6H2O and 50 °C. Al2O3/cerium oxide composite film under this condition has a uniform, smooth, and pyknotic surface topography and optimal corrosion resistance. The corrosion density at that time is 1.106 × 10−6 A/cm2 and the corrosion potential is −0.458 V.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Mechanical and Electrical Engineering Harbin Engineering University Harbin 15001 P. R. China

College of Materials Science and Chemical Engineering Harbin Engineering University Harbin 15001 P. R. China

Funding

National Natural Science Foundation of China

References (34)

Show source-provided references
1. 10.1016/j.surfcoat.2015.07.00210.1016/j.surfcoat.2015.07.002 ↗
2. 10.1016/j.apsusc.2014.02.01910.1016/j.apsusc.2014.02.019 ↗
3. 10.1080/10408436.2014.91736810.1080/10408436.2014.917368 ↗
4. 10.1002/maco.20080507410.1002/maco.200805074 ↗
5. 10.1002/maco.20150873610.1002/maco.201508736 ↗
6. 10.1002/maco.20050392610.1002/maco.200503926 ↗
7. 10.1002/maco.20160936910.1002/maco.201609369 ↗
8. 10.1002/1521-4176(200109)52:9<661::AID-MACO661>3.0.CO;2-410.1002/1521-4176(200109)52:9<661::AID-MACO661>3.0.CO;2-4 ↗
9. 10.1134/S107042721801001910.1134/S1070427218010019 ↗
10. 10.1002/maco.20130727010.1002/maco.201307270 ↗
11. 10.1002/maco.20100563110.1002/maco.201005631 ↗
12. 10.1016/j.apsusc.2009.04.00810.1016/j.apsusc.2009.04.008 ↗
13. 10.1016/j.optlastec.2014.08.01410.1016/j.optlastec.2014.08.014 ↗
14. 10.1116/1.59065110.1116/1.590651 ↗
15. 10.1016/j.corsci.2005.10.01710.1016/j.corsci.2005.10.017 ↗
16. 10.1016/j.surfcoat.2018.04.05210.1016/j.surfcoat.2018.04.052 ↗
17. 10.1016/j.surfcoat.2015.10.04210.1016/j.surfcoat.2015.10.042 ↗
18. 10.1002/maco.1997048020210.1002/maco.19970480202 ↗
19. 10.1002/maco.20181010910.1002/maco.201810109 ↗
20. 10.1002/maco.20181032710.1002/maco.201810327 ↗
21. 10.1016/j.matchar.2011.01.01210.1016/j.matchar.2011.01.012 ↗
22. 10.1002/pssa.20170089210.1002/pssa.201700892 ↗
23. 10.1002/adhm.20170090410.1002/adhm.201700904 ↗
24. 10.1016/j.corsci.2011.10.04110.1016/j.corsci.2011.10.041 ↗
25. 10.1016/j.apsusc.2009.08.05610.1016/j.apsusc.2009.08.056 ↗
26. 10.1016/j.surfcoat.2012.05.07110.1016/j.surfcoat.2012.05.071 ↗
27. 10.1016/j.mseb.2013.10.00110.1016/j.mseb.2013.10.001 ↗
28. 10.1016/j.corsci.2015.03.02110.1016/j.corsci.2015.03.021 ↗
29. 10.1016/j.surfcoat.2015.12.02410.1016/j.surfcoat.2015.12.024 ↗
30. 10.1002/sia.150710.1002/sia.1507 ↗
31. Hu J. · App. Surf. Sci · 2007 · 253 · 8897
32. 10.1016/S0040-6090(02)01038-610.1016/S0040-6090(02)01038-6 ↗
33. 10.1016/j.surfcoat.2004.05.01210.1016/j.surfcoat.2004.05.012 ↗
34. 10.1016/j.corsci.2014.06.02310.1016/j.corsci.2014.06.023 ↗