Investigation of the SCC behaviour of alloy 2024 using the slow strain rate technique

Reinhold Braun

Materials and Corrosion· Volume 44· Issue 3
Publisher page

Abstract

Abstract The stress corrosion cracking (SCC) behaviour of 2024 plate in T351 and T851 tempers was investigated in short transverse direction performing accelerated tests under constant deformation, constant load and slow strain rate conditions. Corrosive media used were: aqueous 3.5% NaCl solution, an aqueous solution of 2% NaCl + 0.5% Na2CrO4at pH 3 (according to LN 65666), an aqueous solution of 3% NaCl + 0.3% H2O2, and substitute ocean water according to ASTM D1141. Alternate immersion tests in 3.5% NaCl solution indicated the low SCC resistance of the alloy 2024‐T351 as well as the improved SCC behaviour due to aging to T851 condition. Similar results were obtained from constant load tests under permanent immersion conditions in the acidified chloride‐chromate solution, in 3% NaCl solution with peroxide, and in substitute ocean water, whereas no SCC failure was observed with specimens which were permanently immersed in 3.5% NaCl solution. Using the slow strain rate method, 3% NaCl + 0.3% H2O2and substitute ocean water were found to be effective synthetic environments. The other two electrolytes did not promote severe stress corrosion cracking with alloy 2024‐T351. The SCC behaviour of 2024‐T851 was difficult to determine employing the slow strain rate technique. Large scatter in data, observed even in inert environment, and the low elongation of the aged material, exacerbated by a further degradation of ductility due to pitting and intergranular corrosion, precluded an evaluation.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. R. N.Parkins: in:Stress Corrosion Cracking ‐ The Slow Strain Rate Technique ASTM STP 665 G. M.UgianskyandJ. H.Payer Eds. American Society for Testing and Materials 1979 p.5.10.1520/STP38106S ↗
2. 10.5006/0010-9312-34.1.3210.5006/0010-9312-34.1.32 ↗
3. G. M.Ugiansky C. E.Johnson D. S.Thompson E. H.Gillespie: in:Stress Corrosion Cracking ‐ The Slow Strain Rate Technique ASTM STP 665 G. M.UgianskyandJ. H.Payer Eds. American Society for Testing and Materials 1979 p.254.10.1520/STP665-EB ↗
4. H.Buhl: in:Stress Corrosion Cracking ‐ The Slow Strain Rate Technique ASTM STP 665 G. M.UgianskyandJ. H.Payer Eds. American Society for Testing and Materials 1979 p.333.10.1520/STP38125S ↗
5. 10.5006/1.359385310.5006/1.3593853 ↗
6. Buhl H. · Aluminium · 1984 · 60 · E704
7. N. J. H.Holroyd G. M.Scamans: in:Environment‐Sensitive Fracture: Evaluation and Comparison of Test Methods ASTM STP 821 S. W.Dean E. N.Pugh andG. M.Ugiansky Eds. American Society for Testing and Materials Philadelphia 1984 p.202.
8. 10.1007/BF0267228410.1007/BF02672284 ↗
9. Scamans G. M. · 1979 · 464
10. Pistulka W. · Aluminium · 1977 · 53 · 366
11. H. F.de Jong J. W. G. A.Berkelaar:Delft University of Technology Department of Aerospace Engineering Report LR‐433 April1984.
12. Brungs D. · Aluminium · 1971 · 47 · 189
13. Hinton B. R. W. · Corrosion · 1989 · 89
14. Lifka B. W. · Aluminium · 1987 · 63 · 1256
15. Hollingsworth E. H. · 1987 · 583
16. J. G.Craig R. C.Newman M. R.Jarrett N. J. H.Holroyd: 4th International Aluminium Lithium Conference Paris G. Champier B. Dubost D. Miannay L. Sabetay Eds. Les éditions de physique Les Ulis 1987 p.C3–825.
17. Moran J. P. · 1989 · 1187
18. Craig J. G. · 1987 · 313
19. 10.1002/maco.1990041100210.1002/maco.19900411002 ↗
20. Braun R. · 1992 · 697
21. 10.1002/maco.1992043030410.1002/maco.19920430304 ↗
22. R.Braun: Proceedings of the Int. Conf. on Corrosion‐Deformation Interaction Fontainebleau France October 5‐7 1992 to be published.
23. 10.1002/maco.1992043090810.1002/maco.19920430908 ↗
24. 10.1002/maco.1991042020610.1002/maco.19910420206 ↗
25. H.Buhl R.Braun C.Yuan J.Helin: “Fracture Properties of 7010 and 7050 Aluminium Alloys under Inert and Aggressive Environmental Conditions” DLR‐FB 91‐35 DLR Köln 1991.
26. Braun R. · 1992 · 807
27. L.Schra W. G. J. 'tHart: National Aerospace Laboratory NLR Technical Report 88012 U Amsterdam The Netherlands 1988.
28. S. C.Dexter: in:The Use of Synthetic Environments for Corrosion Testing ASTM STP 970 P. E.FrancisandT. S.Lee Eds. American Society for Testing and Materials Philadelphia 1988 p.217.10.1520/STP26014S ↗