journal article·1989-03

Fireside corrosion in dutch waste incinerations

N. Bolt, A. S. De Clercq, E. J. A. Vogellar

Materials and Corrosion· Volume 40· Issue 3
Publisher page

Abstract

Abstract The total installed capacity in the (eleven) Dutch waste incineration plants is 3.6 × 106 t/y. About 70% of the waste is household, the remainder industrial and coarse waste. From the view point of fireside corrosion the furnace atmosphere may be characterized as follows: flue gas temperature 800–1000 °C, excess ait 50% PHCl 10−3–10−5 bar, P 10−4 bar. Two case histories concerning superheater failures are described. It has been found that fire side corrosion failures do occur in Dutch waste incinerators but they account for only part of the unforeseen plant unavailability. Improvements can be achieved by optimizing burning conditions, slag transport, gratings and, if necessary, by installation of more corrosion‐resistant tube materials in (certain parts of) the boiler.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Recycled Aggregate Concrete Performance

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.