Influence of potassium hydrogen tartrate on anodized film formed in environmental‐friendly electrolyte on AZ91D magnesium alloy
Source abstract
Abstract
Anodizing of AZ91D magnesium alloy in the alkaline borate‐potassium hydrogen tartrate (PHT) environmental friendly electrolyte was studied. The effect of PHT on the anodizing process and anodic film properties was investigated by scanning electron microscopy (SEM), X‐ray diffraction (XRD), energy dispersive spectrometry (EDS), and potentiodynamic polarization. The results showed that the anodizing parameters, surface morphology, thickness, phase structure, and corrosion resistance of the anodic film were strongly dependent on the concentration of PHT. Moreover, the anodizing mechanism of the AZ91D magnesium alloy in the presence of PHT was also studied. That is, by adsorption on the surface of magnesium alloy, PHT decreases the anodizing current density and make the anodizing condition moderate, which is conducive to the performance improvement of the anodic film.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemistry Tianshui Normal University Tianshui 741000 (P. R. China)
Department of Chemistry Zhejiang University Hangzhou 310027 (P. R. China)
References (39)
Show source-provided references
1. 10.1016/j.apsusc.2010.01.06910.1016/j.apsusc.2010.01.069 ↗
2. Taylor R. H. · Phys. Rev. B. · 2011 · 84 · 84
3. 10.1016/j.electacta.2006.12.08310.1016/j.electacta.2006.12.083 ↗
4. 10.1016/j.apsusc.2010.02.05810.1016/j.apsusc.2010.02.058 ↗
5. 10.1016/j.surfcoat.2011.08.06010.1016/j.surfcoat.2011.08.060 ↗
6. 10.1016/j.jallcom.2012.07.00310.1016/j.jallcom.2012.07.003 ↗
7. 10.1016/j.ceramint.2012.02.04010.1016/j.ceramint.2012.02.040 ↗
8. 10.1016/j.corsci.2012.08.05010.1016/j.corsci.2012.08.050 ↗
9. Hussein R. O. · Corros. Mater. · 2011 · 36 · 38
10. 10.1016/j.surfcoat.2009.01.03210.1016/j.surfcoat.2009.01.032 ↗
11. 10.1016/j.jallcom.2009.04.05310.1016/j.jallcom.2009.04.053 ↗
12. Costantinia A. · Chem. Engi. Trans. · 2012 · 26 · 453
13. 10.1134/S106377451106007110.1134/S1063774511060071 ↗
14. 10.1007/s10800-010-0251-210.1007/s10800-010-0251-2 ↗
15. 10.1016/j.apsusc.2006.08.02010.1016/j.apsusc.2006.08.020 ↗
16. 10.1016/j.electacta.2007.04.03010.1016/j.electacta.2007.04.030 ↗
17. 10.1016/j.jallcom.2009.08.04510.1016/j.jallcom.2009.08.045 ↗
18. 10.1016/j.jmatprotec.2009.04.00410.1016/j.jmatprotec.2009.04.004 ↗
19. 10.1016/S0010-938X(00)00116-510.1016/S0010-938X(00)00116-5 ↗
20. 10.1002/sia.314010.1002/sia.3140 ↗
21. 10.1016/j.apsusc.2007.05.08510.1016/j.apsusc.2007.05.085 ↗
22. 10.1016/j.apsusc.2007.02.01010.1016/j.apsusc.2007.02.010 ↗
23. 10.1016/j.apsusc.2008.11.00810.1016/j.apsusc.2008.11.008 ↗
24. 10.1016/j.tsf.2005.03.05010.1016/j.tsf.2005.03.050 ↗
25. 10.1016/j.matlet.2005.09.01510.1016/j.matlet.2005.09.015 ↗
26. 10.1016/j.elecom.2008.08.04810.1016/j.elecom.2008.08.048 ↗
27. 10.1016/j.corsci.2008.08.03810.1016/j.corsci.2008.08.038 ↗
28. 10.1002/maco.20070405010.1002/maco.200704050 ↗
29. 10.1016/S0257-8972(02)00342-010.1016/S0257-8972(02)00342-0 ↗
30. 10.1016/j.jallcom.2009.08.10410.1016/j.jallcom.2009.08.104 ↗
31. 10.1016/j.surfcoat.2010.04.05210.1016/j.surfcoat.2010.04.052 ↗
32. 10.1016/j.corsci.2004.07.03810.1016/j.corsci.2004.07.038 ↗
33. 10.1179/026708410X1250687324282210.1179/026708410X12506873242822 ↗
34. 10.1016/j.surfcoat.2010.08.03810.1016/j.surfcoat.2010.08.038 ↗
35. 10.1016/j.corsci.2005.08.00410.1016/j.corsci.2005.08.004 ↗
36. Fontana M. G. · 1996
37. 10.1016/j.matchemphys.2007.11.01210.1016/j.matchemphys.2007.11.012 ↗
38. 10.1016/j.matchemphys.2007.07.02710.1016/j.matchemphys.2007.07.027 ↗
39. 10.1016/j.surfcoat.2010.08.05910.1016/j.surfcoat.2010.08.059 ↗