Abstract

Nanostructured Fe‐18Cr‐2Si alloys were developed by a combination of mechanically alloying (MA) and spark plasma sintering (SPS) process. SPS was carried out in vacuum at three different temperatures (900, 1000, and 1100 °C) with a fixed holding time of 10 min and an applied pressure of 50 MPa. Potentiodynamic polarization (PDP), linear polarization resistance (LPR), and electrochemical impedance spectroscopy (EIS) were used to study the effect of sintering temperature on the electrochemical properties of newly developed nanostructured ferritic Fe‐18Cr‐2Si alloy. XRD results showed that, after sintering, crystallite size increased with increasing sintering temperature and maximum crystallite size was 23.64 nm. The results showed that with increasing sintering temperature, corrosion resistance was increased in terms of pitting potential (Epit), passive current density (ip), and polarization resistance (Rp). The improved corrosion resistance was found to be closely related with the densification of the sintered alloys.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering King Fahd University of Petroleum & Minerals (KFUPM) Dhahran 31261 Kingdom of Saudi Arabia

Funding

King Fahd University of petroleum & Minerals

References (26)

Show source-provided references
1. 10.1016/S0026-0657(98)85082-010.1016/S0026-0657(98)85082-0 ↗
2. 10.1016/S0022-3115(00)00137-910.1016/S0022-3115(00)00137-9 ↗
3. 10.1016/j.jnucmat.2004.04.20310.1016/j.jnucmat.2004.04.203 ↗
4. 10.3184/09603400378274907110.3184/096034003782749071 ↗
5. 10.1016/j.jpowsour.2005.02.08410.1016/j.jpowsour.2005.02.084 ↗
6. 10.1016/j.matchar.2006.10.00810.1016/j.matchar.2006.10.008 ↗
7. 10.1016/S0026-0657(01)80712-810.1016/S0026-0657(01)80712-8 ↗
8. 10.1023/A:102300032951410.1023/A:1023000329514 ↗
9. 10.1007/BF0066480410.1007/BF00664804 ↗
10. 10.4028/www.scientific.net/MSF.426-432.435510.4028/www.scientific.net/MSF.426-432.4355 ↗
11. 10.1016/j.jmatprotec.2007.02.00510.1016/j.jmatprotec.2007.02.005 ↗
12. 10.1016/S0010-938X(98)00047-X10.1016/S0010-938X(98)00047-X ↗
13. 10.1016/0010-938X(96)00039-X10.1016/0010-938X(96)00039-X ↗
14. 10.5006/1.358502010.5006/1.3585020 ↗
15. 10.1002/maco.1991042080410.1002/maco.19910420804 ↗
16. 10.1016/0079-6425(89)90001-710.1016/0079-6425(89)90001-7 ↗
17. 10.1016/j.corsci.2014.11.04110.1016/j.corsci.2014.11.041 ↗
18. Gupta R. K. · Int. J. Electrochem. Sci · 2013 · 8 · 679110.1016/S1452-3981(23)14806-1 ↗
19. 10.1016/j.jmatprotec.2007.03.01410.1016/j.jmatprotec.2007.03.014 ↗
20. 10.1016/j.corsci.2012.04.02110.1016/j.corsci.2012.04.021 ↗
21. 10.1016/j.jallcom.2016.05.11010.1016/j.jallcom.2016.05.110 ↗
22. 10.1016/j.powtec.2016.05.04110.1016/j.powtec.2016.05.041 ↗
23. 10.1016/j.jallcom.2014.01.08710.1016/j.jallcom.2014.01.087 ↗
24. 10.1016/j.electacta.2013.04.10510.1016/j.electacta.2013.04.105 ↗
25. 10.1016/S0010-938X(98)00122-X10.1016/S0010-938X(98)00122-X ↗
26. 10.1016/S0008-8846(98)00008-810.1016/S0008-8846(98)00008-8 ↗