Corrosion dependence of an AlMgSi alloy under MgCl2 solution drop on initial concentration and humidity
Source abstract
Abstract
Abstract The corrosion behavior of an Al–0.63Mg–0.28Si alloy under MgCl2 solution droplets with different initial concentration in environments of 33, 75, and 88% relative humidity (RH) was studied using a Kelvin probe. The available cathodic limiting current associated with oxygen reduction was highly dependent on the environment RH and initial concentration. In the 33% RH environment, metastable pitting was the main form of corrosion. In some cases at 75 and 88% RH, the potential baseline decreased slowly by hundreds of mV and remained at the lower value, indicating stable filiform‐like corrosion grew. The initiation time of the stable corrosion was determined by the environment RH and initial concentration. With increasing initial concentration or decreasing environment RH, the available cathodic limiting current decreased, stable corrosion was difficult to occur. The stable corrosion could occur outside the drop and/or inside the drop, which was dependent on not only the cathodic limiting current but also the environment RH.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. 10.1016/S0010-938X(00)00009-310.1016/S0010-938X(00)00009-3 ↗
2. 10.1016/0013-4686(95)00438-610.1016/0013-4686(95)00438-6 ↗
3. 10.1149/1.183757810.1149/1.1837578 ↗
4. 10.1016/j.corsci.2003.10.00510.1016/j.corsci.2003.10.005 ↗
5. Shi Y. Y. · Bull. Electrochem. · 2004 · 20 · 261
6. 10.1016/S0010-938X(97)00124-810.1016/S0010-938X(97)00124-8 ↗
7. 10.1016/S0010-938X(03)00130-610.1016/S0010-938X(03)00130-6 ↗
8. 10.1016/j.electacta.2006.01.05010.1016/j.electacta.2006.01.050 ↗
9. 10.1016/j.corsci.2006.05.02710.1016/j.corsci.2006.05.027 ↗
10. 10.1016/j.elecom.2006.03.02410.1016/j.elecom.2006.03.024 ↗
11. 10.1016/j.mseb.2009.01.00310.1016/j.mseb.2009.01.003 ↗
12. 10.1016/j.corsci.2006.10.01710.1016/j.corsci.2006.10.017 ↗
13. A.Wythe M.Salagaras S.Knight G.McAdam T.Trueman in:Proceedings of 2009 Australasian Corrosion Association Meeting Coffs Harbour Australia 11/2009 Paper 039.
14. 10.1016/j.corsci.2011.02.03510.1016/j.corsci.2011.02.035 ↗
15. 10.1149/1.241136210.1149/1.2411362 ↗
16. 10.1016/0010-938X(90)90032-Z10.1016/0010-938X(90)90032-Z ↗
17. 10.1016/0010-938X(90)90033-210.1016/0010-938X(90)90033-2 ↗
18. 10.1149/1.346785010.1149/1.3467850 ↗
19. 10.1108/0003559091092344610.1108/00035590910923446 ↗
20. 10.1016/j.corsci.2010.02.03110.1016/j.corsci.2010.02.031 ↗
21. 10.1149/1.210032810.1149/1.2100328 ↗
22. 10.1149/1.211410410.1149/1.2114104 ↗
23. S. T.Pride J. R.Scully J. L.Hudson in:ECS Proceedings on Corrosion in Electronic Materials PV 93‐1 The Electrochem. Soc. pp. 171–182 Fall1992.
24. 10.1002/(SICI)1521-4176(199808)49:8<569::AID-MACO569>3.0.CO;2-V10.1002/(SICI)1521-4176(199808)49:8<569::AID-MACO569>3.0.CO;2-V ↗
25. 10.1016/S0010-938X(97)83355-010.1016/S0010-938X(97)83355-0 ↗
26. 10.5006/1.328063510.5006/1.3280635 ↗
27. 10.1016/j.electacta.2004.01.03210.1016/j.electacta.2004.01.032 ↗
28. 10.5006/1.327815210.5006/1.3278152 ↗