Detection of microstructural changes of 9% Cr‐martensitic steels during heat treatment and aging by polarization tests

Sven Schmigalla, Kevin G. Abstoss, Sabine Schultze, Peter Mayr

Materials and Corrosion· Volume 71· Issue 1

Abstract

Abstract 9–12% chromium martensitic steels are widely used as pipe material in steam power plants. Their good creep behavior is based on a finely adjusted microstructure, which is strengthened by precipitates. During long‐term use at higher temperatures degredation mechanisms occur, which affect the initial microstructure. Subgrain and precipitate coarsening as well as phase formation like Laves‐phase ((Fe, Cr)2(Mo, W)) proceed and lead to a reduced creep resistance. For lifetime assessment a nearly nondestructive electrochemical test method would be beneficial to identify microstructural changes during periodical inspections. The paper is focussed on the usability of an adapted electrochemical potentiodynamic reactivation (EPR)‐method and deals with the adjustment of test conditions like electrolyte composition and polarization parameters. The results obtained under optimized test conditions show a clear indication of precipitate formation by changing the characteristics of the EPR‐curves for the well established alloy T/P91 (X10CrMoVNb9‐1) as well as for the boron containing advanced alloy MARBN (X10CrWCoVNb9‐3‐3).
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institut für Korrosions‐ und Schadensanalyse Dr.‐Ing. Sabine Schultze Magdeburg Germany

Chemnitz University of Technology, Institute of Joining and Assembly Chemnitz Germany

Funding

Bundesministerium für Wirtschaft und Energie

References (15)

Show source-provided references
1. 10.1179/174892306X9973210.1179/174892306X99732 ↗
2. 10.1016/j.calphad.2007.04.00110.1016/j.calphad.2007.04.001 ↗
3. 10.1179/mst.1992.8.12.106310.1179/mst.1992.8.12.1063 ↗
4. 10.1088/1468-6996/9/1/01300210.1088/1468-6996/9/1/013002 ↗
5. 10.1016/j.matchar.2003.09.01210.1016/j.matchar.2003.09.012 ↗
6. 10.2355/isijinternational.42.89410.2355/isijinternational.42.894 ↗
7. 10.2355/isijinternational.42.Suppl_S6710.2355/isijinternational.42.Suppl_S67 ↗
8. 10.1016/j.ijpvp.2006.09.01310.1016/j.ijpvp.2006.09.013 ↗
9. 10.1179/174892406X16062410.1179/174892406X160624 ↗
10. S.Komazaki T.Miura T.Mitsueda presented at 3rd Int. ECCC Conference Rome Italy 5th–7th May 2014 p. 75.
11. 10.3795/KSME-A.2006.30.8.96510.3795/KSME-A.2006.30.8.965 ↗
12. ISO 12732:2006: Corrosion of metals and alloys – Electrochemical potentiokinetic reactivation measurement using the double loop method (based on Cihal's method)2006.
13. 10.1002/maco.20130727610.1002/maco.201307276 ↗
14. 10.1016/j.electacta.2004.01.06110.1016/j.electacta.2004.01.061 ↗
15. 10.1002/maco.1976027080410.1002/maco.19760270804 ↗