The Influence of Chloride Concentration on the Kinetic Behaviour for the Initiation Stage of pitting corrosion on aluminium
Source abstract
Abstract
Abstract Experiments are performed to study the influence of applied potential and chloride concentration on the kinetic behaviour of pitting corrosion initiation for unalloyed aluminium. A potentiostatic method is used at 30°C in deaerated solutions of sodium chloride. The pitting potential, Ep, is determined by the extrapolation method described by Broli, Holtan and Midjo, and a relation between Ep and chloride concentration is found. Kinetic interpretations such as the influence of applied potential and chloride concentration on the induction time are given.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. 10.1179/00070597379832218910.1179/000705973798322189 ↗
2. 10.5006/0010-9312-30.12.42710.5006/0010-9312-30.12.427 ↗
3. Aa.BroliandH.Holtan:Corros. Sci. In press.
4. Aa.Broli H.HoltanandM.Midjo: 25th Meeting of ISE Brighton September1974.
5. 10.1016/0010-938X(73)90002-410.1016/0010-938X(73)90002-4 ↗
6. 10.1016/S0010-938X(71)80035-510.1016/S0010-938X(71)80035-5 ↗
7. 10.1016/S0010-938X(65)90581-010.1016/S0010-938X(65)90581-0 ↗
8. 10.1002/maco.1965016110210.1002/maco.19650161102 ↗
9. 10.1002/maco.1969020010310.1002/maco.19690200103 ↗
10. 10.1149/1.240775610.1149/1.2407756 ↗
11. 10.1149/1.242380110.1149/1.2423801 ↗
12. 10.1016/0010-938X(69)90017-110.1016/0010-938X(69)90017-1 ↗
13. 10.5006/0010-9312-27.12.50610.5006/0010-9312-27.12.506 ↗
14. Szklarska‐Śmiałlowska Z. · Bull. Akad. Pol. Sci. ser. sci. chim. · 1965 · 13 · 221
15. 10.1038/2161299a010.1038/2161299a0 ↗
16. Engell H. J. · Arch. Eisenhüttenwes. · 1971 · 30 · 23910.1002/srin.195902838 ↗
17. 10.1002/maco.1971022090610.1002/maco.19710220906 ↗
18. 10.1016/S0010-938X(72)80083-010.1016/S0010-938X(72)80083-0 ↗
19. 10.1016/0013-4686(71)85152-610.1016/0013-4686(71)85152-6 ↗
20. 10.1179/00070597279832299110.1179/000705972798322991 ↗
21. 10.1016/S0010-938X(72)80100-810.1016/S0010-938X(72)80100-8 ↗
22. 10.1016/S0010-938X(69)80116-210.1016/S0010-938X(69)80116-2 ↗
23. 10.1016/S0010-938X(67)80103-310.1016/S0010-938X(67)80103-3 ↗
24. 10.1002/maco.1966017050210.1002/maco.19660170502 ↗
25. 10.1016/S0010-938X(68)80162-310.1016/S0010-938X(68)80162-3 ↗
26. Videm K. · 1972
27. Böhni H. · Schweizer Arch. · 1962 · 36 · 41
28. 10.1524/zpch.1962.34.1_4.08710.1524/zpch.1962.34.1_4.087 ↗
29. J. R.Galvele S. M.de De Micheli I. L.Müller S. B.De WexlerandJ. L.Alanis:U. R. Evans Int. Conf. Local. Corros. Williamsburg Virginia December1971.
30. 10.1002/jctb.501008060210.1002/jctb.5010080602 ↗
31. 10.5006/0010-9312-28.1.110.5006/0010-9312-28.1.1 ↗
32. Kolotyrkin Ya. M. · Dokl. Akad. Nauk. SSSR · 1963 · 48 · 1106
33. 10.1149/1.242414610.1149/1.2424146 ↗
34. 10.5006/0010-9312-20.4.129t10.5006/0010-9312-20.4.129t ↗
35. Ashworth V. · Corros. Sci. · 1970 · 10 · 48
36. 10.5006/0010-9312-19.8.26110.5006/0010-9312-19.8.261 ↗
37. Pourbaix M. · 1967
38. Aa.Broli H.HoltanandT. B.Andreassen: In preparation.