journal article·1997-07

Stress corrosion cracking of Inconel 600 in aqueous solutions at elevated temperature Part II: Effects of chloride and sulphate ions on the electrochemical behaviour of Inconel 600

E. A. Ashour, F. Schneider, K. Mummert

Materials and Corrosion· Volume 48· Issue 7
Publisher page

Abstract

Abstract The influencing effects of temperature, potential and electrolyte composition on the electrochemical behaviour of Inconel 600 in aqueous solutions are presented. Considering these effects the connection between the data have been obtained from chemo‐mechanical fracture investigation on CT‐samples in Part I of this paper and pitting corrosion are discussed. The results have shown that chloride ions depassivate the surfaces of cracks locally and hinder the formation of a new protective oxide layer on the fracture surfaces. Furthermore, chloride promotes the dissolution of metal and initiates the cracking, respectively. The resulting crevice corrosion promotes an increase of hydrogen absorption by the metal. The increase of the hydrogen content of the metal influences the mechanical fracture behaviour. Contrary, sulphateions inhibit the initiation of corrosion mainly due to a hinderance of chloride ions adsorption on active sites of the fracture surfaces. The initiation of localized corrosion in the crevice region may be stimulated by chromate ions formed by oxidation of chromium from the oxide layer or the base metal in oxygen containing solutions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. 10.5006/0010-9312-35.12.55010.5006/0010-9312-35.12.550 ↗
2. 10.5006/0010-9312-36.9.44710.5006/0010-9312-36.9.447 ↗
3. 10.5006/1.358300110.5006/1.3583001 ↗
4. 10.1016/0022-3115(83)90327-610.1016/0022-3115(83)90327-6 ↗
5. W. H.Cullen M. J.Partridge J.PeterN.Paine:Proc. of the 6th Int. Symp. on Environmental Degradation of Materials in Nuclear Power Systems‐Water Reactors August 1 ‐5 Ed. byR. E.GoldandE. P.Simonen San Diego California (1993)197.
6. 10.1016/0010-938X(92)90016-V10.1016/0010-938X(92)90016-V ↗
7. 10.2320/matertrans1989.33.60410.2320/matertrans1989.33.604 ↗
8. 10.1002/maco.1997048030310.1002/maco.19970480303 ↗
9. 10.4028/www.scientific.net/MSF.185-188.27510.4028/www.scientific.net/MSF.185-188.275 ↗
10. Prazak M. · Z. Elektochem. · 1958 · 62 · 739
11. C. M.Chen K.Aral G. J.Theus: Computer‐Calculated Potential‐pH‐Diagrams up to 300°C EPRI‐NP 3137 (1983).
12. F.Schneider M.Herrich K.Mummert:Electrochemistry of Fe‐Cr and Fe‐Cr‐Ni alloys at 250°C:. The European Congress EURoCORR' 96 September 24‐26 NICE‐France (1996).
13. 10.5006/1.359388010.5006/1.3593880 ↗
14. Y.Horii K.Mabuchi H.Konno H.Takahasi M.Nagayama: 9th Int. Congr. on Metallic Corrosion Toronto1984 p.235.
15. K.Tanno H.Yashiro:Crevice corrosion of stainless steel in high temperature chloride solutions 10th Int. Congr. on Metallic Corrosion Madras (India)1987 p.3071.
16. 10.1016/0010-938X(91)90037-P10.1016/0010-938X(91)90037-P ↗
17. 10.1016/0010-938X(83)90063-X10.1016/0010-938X(83)90063-X ↗
18. 10.1002/maco.1993044110510.1002/maco.19930441105 ↗