journal article·2026-04-03

High‐Temperature Corrosion Behavior of Typical Steels in Novel NaNO 3 ‐KNO 3 ‐Ca(NO 3 ) 2 Molten Salt

Xinjun Xu, Jianguang Xu, Bo Li, Qingqing Yong, Kaijing Yuan, Zhongfeng Tang

Publisher page

Abstract

ABSTRACT The corrosion behavior and mechanism of typical steels in the novel proportion NaNO 3 ‐KNO 3 ‐Ca(NO 3 ) 2 (16‐48‐36 wt%, NKC) molten salt have been reported. Static corrosion tests of 347H stainless steel (347H), 321 stainless steel (321SS) and 20# carbon steel (20#CS) were conducted in NKC salt at 480°C for 360 h. Their annual corrosion rates are 10.5, 12.9, and 31.4 µm/year separately, and the corrosion resistance ranks as 347H > 321SS > 20#CS. Corrosion is primarily driven by selective oxidation and elemental dissolution. 347H forms a dense (Fe,Cr) 2 O 3 layer with a flat surface and minor granular products. 321SS undergoes chromium depletion and precipitation, resulting in the formation of Fe 2 O 3 and Fe‐Ni phases, which lead to uneven local corrosion. 20#CS develops a porous Fe 2 O 3 /Fe 3 O 4 mixed layer characterized by distinct pits and general corrosion. These findings provide new insights into steel corrosion and key data for material selection.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Thermal Expansion and Ionic Conductivity · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Energy and Materials Shanghai Polytechnic University Shanghai China

Shanghai Institute of Applied Physics Chinese Academy of Sciences Shanghai China

School of Shipping and Naval Architecture, Institute for New Energy Materials and Equipment in Transportation Chongqing Jiaotong University Chongqing China

Shanghai Institute of Microsystem and Information Technology Chinese Academy of Sciences Shanghai China

References (31)

Show source-provided references
1. Assessment of Liquid Metal Technology Status and Research Paths for Their Use as Efficient Heat Transfer Fluids in Solar Central Receiver Systems10.1016/j.solener.2013.03.025 ↗
2. The Value of Concentrating Solar Power and Thermal Energy Storage10.1109/TSTE.2010.2052078 ↗
3. Multi‐Objective Optimization of Operational Strategy and Capacity Configuration for Hybrid Energy System Combined With Concentrated Solar Power Plant10.1016/j.apenergy.2025.125860 ↗
4. Effect of Preheating on Thermal Stability of Molten Nitrate Salt10.1016/j.est.2024.110858 ↗
5. Corrosion Performance of Alloy 800H and Alloy 625 for Potential Use as Molten Salts Solar Receiver Materials in Concentrating Solar Power Tower Plants10.1016/j.est.2022.105824 ↗
6. On the Path Toward Day and Night Continuous Solar High Temperature Thermochemical Processes: A Review10.1016/j.rser.2020.110061 ↗
7. Thermal Energy Storage Systems for Concentrated Solar Power Plants10.1016/j.rser.2017.03.139 ↗
8. Digital Phase Diagram and Thermophysical Properties of KNO 3 ‐NaNO 3 ‐Ca(NO 3) 2 Ternary System for Solar Energy Storage10.1016/j.vacuum.2017.09.003 ↗
9. Thermodynamic Investigation of the Ca(NO3)2‐NaNO3‐KNO3 System for Solar Thermal Energy Storage10.1016/j.tca.2020.178608 ↗
10. A Review of High‐Temperature Molten Salt for Third‐Generation Concentrating Solar Power10.1002/ese3.2029 ↗
11. Assessment of Thermal Energy Storage Options in a Sodium‐Based CSP Plant10.1016/j.applthermaleng.2016.06.152 ↗
12. Molten Salt Power Towers Operating at 600–650°C: Salt Selection and Cost Benefits10.1016/j.solener.2018.01.063 ↗
13. Thermal Energy Storage in Solar Power Plants: A Review of the Materials, Associated Limitations, and Proposed Solutions10.3390/en12214164 ↗
14. Perspectives on Selected Alloys in Contact With Eutectic Melts for Thermal Storage: Nitrates, Carbonates and Chlorides10.1016/j.solener.2021.06.069 ↗
15. Thermal Stability and Durability of Solar Salt‐Based Nanofluids in Concentrated Solar Power Thermal Energy Storage: An Approach From the Effect of Diverse Metal Alloys Corrosion10.1016/j.est.2023.109715 ↗
16. Corrosion of Stainless Steels and Carbon Steel by Molten Mixtures of Commercial Nitrate Salts10.1361/10599490417542 ↗
17. A Simple Method for the Inhibition of the Corrosion of Carbon Steel by Molten Nitrate Salt for Thermal Storage in Concentrating Solar Power Applications10.1038/s41529-018-0055-0 ↗
18. Corrosion of Stainless Steels and Low‐Cr Steel in Molten Ca(NO3)2‐NaNO3‐KNO3 Eutectic Salt for Direct Energy Storage in CSP Plants10.1016/j.solmat.2015.05.004 ↗
19. Spray‐Graphitization as a Protection Method Against Corrosion by Molten Nitrate Salts and Molten Salts Based Nanofluids for Thermal Energy Storage Applications10.1016/j.solmat.2019.110024 ↗
20. Corrosion Performance of 316 Stainless Steel and Nodular Cast Iron 600‐3 in Molten Ca(NO3)2‐NaNO3‐KNO3 Salt10.1016/j.est.2022.106231 ↗
21. Evaluation of Thermal‐Physical Properties of Novel Multicomponent Molten Nitrate Salts for Heat Transfer and Storage10.3390/en15186591 ↗
22. Thermophysical Property Degradation and Structure Evolution of the NaNO3‐KNO3‐Ca(NO3)2 Molten Salts After Long‐Term High‐Temperature Heat Treatment10.1016/j.solmat.2025.113668 ↗
23. Excellent Corrosion Resistance of 316 Stainless Steel in Purified NaCl‐MgCl2 Eutectic Salt at High Temperature10.1016/j.corsci.2020.108473 ↗
24. Experimental Observation of Spin‐Phonon Coupling in Cr2O3 and Fe2O3 Solid Solution and Bandgap Engineering10.1016/j.mseb.2022.116084 ↗
25. High Temperature Oxidation Behavior of Flake and Spheroidal Graphite Cast Irons10.1007/s11085-011-9244-8 ↗
26. In‐Situ Monitoring of the Corrosion Behavior of Austempered Ductile Iron (ADI) under Cyclic Salt Spray Exposure10.1016/j.corsci.2021.109437 ↗
27. Improvement of the Corrosion Properties in Ternary Molten Nitrate Salts for Direct Energy Storage in CSP Plants10.1016/j.solener.2016.05.030 ↗
28. Corrosion Behavior of a High‐Carbon Austenitic Stainless Steel With Ultrafine Cr23C6 Precipitates in Molten FLiNaK Salt10.1016/j.corsci.2024.112660 ↗
29. Effect of Nb on High‐Temperature Corrosion Resistance of 304 Austenitic Stainless Steel in Molten Salt
30. Effect of Fillers on the Microstructure, Mechanical Properties, and Hot Corrosion Behavior of Nb Stabilized Austenitic Stainless Steel Welds10.1557/jmr.2016.492 ↗
31. Corrosion Resistance and Wear Behavior of Ni60/TiC and NbC Composite Coatings Prepared by Laser Cladding10.3390/ma18112459 ↗