Process parameter effects on residual stress and phase purity after microlaser-assisted machining of silicon
Source abstract
Abstract
Machining brittle materials, such as silicon, is expensive and often causes detrimental damage, but a relatively new technique, termed microlaser-assisted machining (micro-LAM), improves the efficacy of the machining process using traditional single point diamond turning with simultaneous laser assistance. Prior work shows it provides a smooth surface finish and reduces the likelihood of fracture by increasing the ductility of the material during the machining process. However, the quality of the finish and the utility of the machined silicon depends on having good phase purity and low residual stresses. Using Raman microspectroscopy and a wide range of micro-LAM machining parameters the current work has shown that the technique can give excellent results in terms of low residual stress, high phase purity, and good relative crystallinity. However, poor choice of process parameters can be very detrimental leading to high residual stresses (over 400 MPa) and multiple silicon phases being present.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, Rutgers University, Piscataway, NJ, USA
Micro-LAM, Inc., Portage, MI, USA
Funding
National Science Foundation · Rutgers CCOMC
References (22)
Show source-provided references
1. 10.1007/s11465-017-0444-z10.1007/s11465-017-0444-z ↗
2. 10.1007/s00170-016-8940-610.1007/s00170-016-8940-6 ↗
3. 10.1080/10426914.2016.114018610.1080/10426914.2016.1140186 ↗
4. 10.1080/10426914.2014.98420710.1080/10426914.2014.984207 ↗
5. 10.1016/S094-0136(02)00952-410.1016/S094-0136(02)00952-4 ↗
6. Chinn, R. E. Ceramography: Preparation and Analysis of Ceramic Microstructures, 1st ed.; Wiley-American Ceramic Society: Malden, MA, USA, 2002; p 230.
7. 10.115/1.194961410.115/1.1949614 ↗
8. 10.3103/S106345761305001810.3103/S1063457613050018 ↗
9. 10.1115/1.403539710.1115/1.4035397 ↗
10. 10.5772/1568310.5772/15683 ↗
11. 10.1115/1.289967610.1115/1.2899676 ↗
12. 10.1088/0268-1242/22/5/01910.1088/0268-1242/22/5/019 ↗
13. 10.1007/978-94-011-5050-7_3010.1007/978-94-011-5050-7_30 ↗
14. 10.4028/www.scientific.net/AMR.1017.17510.4028/www.scientific.net/AMR.1017.175 ↗
15. 10.1016/j.precisioneng.2011.12.00310.1016/j.precisioneng.2011.12.003 ↗
16. 10.1002/1527-2648(20020806)4:8<535::AID-ADEM535>3.0.CO;2-E10.1002/1527-2648(20020806)4:8<535::AID-ADEM535>3.0.CO;2-E ↗
17. 10.1063/1.139682810.1063/1.1396828 ↗
18. 10.1063/1.189844410.1063/1.1898444 ↗
19. 10.1063/1.347460410.1063/1.3474604 ↗
20. 10.1243/09544054JEM116110.1243/09544054JEM1161 ↗
21. 10.1088/0268-1242/14/10/31010.1088/0268-1242/14/10/310 ↗
22. Turrell, G.; Corset, J. Raman Microscopy: Developments and Applications; Elsevier Academic Press: San Diego, CA, USA, 1996; p 463.