On the Use of Ball Milling for the Production of Ceramic Powders
Source abstract
Abstract
In the present research work, the mixture of boron carbide and graphite ceramic powders with a theoretical composition of 50% each by weight were mechanically alloyed in a laboratory ball mill with different milling times of 12.5, 25, 50, 75, and 100 h. The investigation was carried out on the morphologies and densities of ball-milled powders. Morphology results revealed that ball milling is a very dominant and dynamic practice for preparation of two different powders into single entity powder having appropriate and consistent morphology. The results of density measurement showed that with milling times, density increased initially and then reduced with further increase in milling times. The density is reduced by 1.68% as the milling time increased from 0 to 100 h.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. 10.1016/S0079-6425(99)00010-910.1016/S0079-6425(99)00010-9 ↗
2. 10.1016/j.matlet.2012.04.09810.1016/j.matlet.2012.04.098 ↗
3. 10.1201/978020302064710.1201/9780203020647 ↗
4. 10.1016/j.cattod.2010.11.03110.1016/j.cattod.2010.11.031 ↗
5. 10.1016/j.matlet.2009.10.07010.1016/j.matlet.2009.10.070 ↗
6. 10.1016/j.matdes.2011.03.01810.1016/j.matdes.2011.03.018 ↗
7. 10.1016/S0043-1648(96)07496-010.1016/S0043-1648(96)07496-0 ↗
8. 10.1016/S0043-1648(98)00192-610.1016/S0043-1648(98)00192-6 ↗
9. 10.1080/1042691070145175410.1080/10426910701451754 ↗
10. 10.1016/j.matdes.2012.02.01310.1016/j.matdes.2012.02.013 ↗
11. 10.1016/j.wear.2012.01.00910.1016/j.wear.2012.01.009 ↗
12. 10.1016/j.matdes.2012.09.01510.1016/j.matdes.2012.09.015 ↗
13. 10.1016/j.matdes.2008.04.01410.1016/j.matdes.2008.04.014 ↗
14. 10.1016/j.compscitech.2010.06.01310.1016/j.compscitech.2010.06.013 ↗
15. 10.1016/j.matdes.2009.11.01510.1016/j.matdes.2009.11.015 ↗
16. 10.1016/j.matdes.2010.04.05310.1016/j.matdes.2010.04.053 ↗
17. 10.1016/j.matdes.2011.05.01010.1016/j.matdes.2011.05.010 ↗
18. 10.1177/002199830934638610.1177/0021998309346386 ↗
19. 10.1016/j.matdes.2011.01.02110.1016/j.matdes.2011.01.021 ↗
20. Basavaraju S. · International Journal Of Innovative Research in Science Engineering And Technology · 2012 · 1 · 107
21. Altinkok N. · International Journal of Science and Advanced Technology · 2012 · 2 · 78
22. 10.1016/j.matdes.2013.04.02910.1016/j.matdes.2013.04.029 ↗
23. 10.1016/j.jmrt.2013.02.00510.1016/j.jmrt.2013.02.005 ↗
24. 10.1016/j.msea.2014.06.02410.1016/j.msea.2014.06.024 ↗
25. 10.1016/j.matdes.2013.02.03810.1016/j.matdes.2013.02.038 ↗
26. 10.1016/j.jmrt.2013.10.00410.1016/j.jmrt.2013.10.004 ↗
27. 10.1016/0043-1648(94)06577-210.1016/0043-1648(94)06577-2 ↗
28. 10.1016/0043-1648(95)06801-510.1016/0043-1648(95)06801-5 ↗
29. 10.1088/0953-8984/3/20/00410.1088/0953-8984/3/20/004 ↗
30. 10.4028/www.scientific.net/MSF.235-238.56510.4028/www.scientific.net/MSF.235-238.565 ↗
31. 10.1016/0966-9795(95)92680-X10.1016/0966-9795(95)92680-X ↗
32. 10.4028/www.scientific.net/MSF.235-238.12110.4028/www.scientific.net/MSF.235-238.121 ↗
33. 10.4028/www.scientific.net/MSF.225-227.46510.4028/www.scientific.net/MSF.225-227.465 ↗
34. Sajjadi, S.A.; Ezatpour, H.R.; Beygi, H. Microstructure and mechanical properties of Al–Al2O3micro- and nano-composites fabricated by stir casting.Proceeding of 14th National Conference On Material Science And Engineering(Tehran, Iran), 2010, 325–332.10.1016/j.msea.2011.08.052 ↗
35. 10.1038/scientificamerican0576-4010.1038/scientificamerican0576-40 ↗
36. 10.1023/A:100433480550510.1023/A:1004334805505 ↗
37. 10.1002/app.1995.07057051310.1002/app.1995.070570513 ↗
38. Sang H.N. · Journal of Korean Nuclear Society · 2002 · 34 · 60
39. 10.1081/AMP-12003865610.1081/AMP-120038656 ↗