Experimental studies on fly-ash erosion behavior of Ni-Cr based nanostructured thermal spray coating in boiler tubes
Source abstract
Abstract
Erosion study was performed on the uncoated and coated SA210Gr-C boiler tube substrates. This study was performed in a view to reducing the scaling on boiler water-wall and super-heater tubes. In the present work, the High Velocity Oxygen Fuel (HVOF) coating process was used to deposit nanostructured and conventional coatings on the boiler tube substrates. Fly-ash produced after the combustion of coal in an Indian thermal power station was used as erodent. The erosion loss of coated and uncoated substrates was recorded at a regular interval of 30 minutes. The study was conducted at 30°, 60°, and 90° impingement angles and at two different operating temperatures (300°C, 550°C). Surface morphology of eroded samples was analyzed using macro and micro imaging techniques, and surface roughness was also recorded for the eroded samples. The phases present in the eroded substrates were indexed using the X-Ray diffraction (XRD) analysis. HRTEM images of nanostructured coated samples at 550°C with varying impingement angles were analyzed. The result reveals that the nanostructure in the coating was retained even after high-temperature erosion test. Comparative study was made with nanostructured and conventional coatings against the uncoated materials.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Erosion and Abrasive Machining · High-Temperature Coating Behaviors · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Production Engineering, National Institute of Technology, Tiruchriappalli, Tamilnadu, India
References (25)
Show source-provided references
1. 10.1016/j.fuproc.2004.04.00210.1016/j.fuproc.2004.04.002 ↗
2. 10.1016/j.matdes.2004.10.00810.1016/j.matdes.2004.10.008 ↗
3. 10.1080/10426914.2013.85222210.1080/10426914.2013.852222 ↗
4. 10.1179/174329409X45116410.1179/174329409X451164 ↗
5. 10.1179/1743294414Y.000000041610.1179/1743294414Y.0000000416 ↗
6. 10.1179/174329409X40948610.1179/174329409X409486 ↗
7. 10.1179/1743294414Y.000000041910.1179/1743294414Y.0000000419 ↗
8. 10.1179/174329406X9840310.1179/174329406X98403 ↗
9. 10.1080/10426914.2011.55713510.1080/10426914.2011.557135 ↗
10. 10.1016/S0921-5093(02)00591-910.1016/S0921-5093(02)00591-9 ↗
11. 10.1080/10402004.2013.79753210.1080/10402004.2013.797532 ↗
12. 10.1016/S0043-1648(00)00540-810.1016/S0043-1648(00)00540-8 ↗
13. 10.1016/S0965-9773(99)00010-010.1016/S0965-9773(99)00010-0 ↗
14. 10.4028/www.scientific.net/MSF.343-346.26110.4028/www.scientific.net/MSF.343-346.261 ↗
15. 10.1080/10426914.2015.103790610.1080/10426914.2015.1037906 ↗
16. 10.1016/S0301-679X(00)00146-810.1016/S0301-679X(00)00146-8 ↗
17. 10.1016/j.wear.2014.06.00710.1016/j.wear.2014.06.007 ↗
18. 10.1016/S1003-6326(15)63755-410.1016/S1003-6326(15)63755-4 ↗
19. 10.1016/j.matdes.2013.10.00210.1016/j.matdes.2013.10.002 ↗
20. 10.1007/s12206-013-0326-110.1007/s12206-013-0326-1 ↗
21. Bhatia Rakesh · International Journal of Surface Engineering and Materials Technology · 2012 · 2 · 39
22. 10.1016/S0257-8972(99)00434-X10.1016/S0257-8972(99)00434-X ↗
23. 10.1016/S1674-4799(09)60092-310.1016/S1674-4799(09)60092-3 ↗
24. 10.1080/10426914.2014.97359910.1080/10426914.2014.973599 ↗
25. 10.1007/s11661-010-0587-610.1007/s11661-010-0587-6 ↗