In this research nucleation effect of Ti-6Al-4 V powder on grain size and tensile strength of Al-12.1% Si eutectic alloy was studied. Metal powder produced from Ti-6Al-4 V machining chips by meshes of 50 and 140 and weight percentages of 0.1, 0.15, 0.2, and 0.25 were used. The microstructure by mesh 50 with 0.15 wt% consists of grain with average size of 6 µm, tensile strength and elongation equal to 492 MPa and 7.25%, respectively. By mesh 140 with 0.15 wt% the considered values are equal to 10 µm, 540 MPa, and 8.82%, respectively. Before refinement the needle-plate-like eutectic silicon is distributed arbitrarily. The morphology of the eutectic silicon is changed from needle-plate to a fibrous form with addition of 0.15 wt% of mesh 50 and finally changes its morphology from a needle-plate to a globular form after adding 0.15 wt% of mesh 140, which is fully modified. SEM/EDX micro-analyzing shows that TiAl3 compound has been formed, which is the major factor in grain size modification and tensile strength increasing. This phase is formed prior to solidification of Al–Si alloy makes it an efficient nucleation site for aluminum grains upon solidification.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. 10.1016/j.matchar.2008.01.00810.1016/j.matchar.2008.01.008 ↗
2. 10.1016/j.matchar.2008.10.01210.1016/j.matchar.2008.10.012 ↗
3. Junga H. · Journal of Alloys and Compounds · 2008 · 622
4. 10.1016/j.scriptamat.2007.08.02610.1016/j.scriptamat.2007.08.026 ↗
5. 10.1016/j.msea.2006.04.01210.1016/j.msea.2006.04.012 ↗
6. 10.1016/S0142-9612(98)00217-810.1016/S0142-9612(98)00217-8 ↗
7. 10.1016/S0142-9612(00)00274-X10.1016/S0142-9612(00)00274-X ↗
8. 10.1016/S0142-9612(01)00040-010.1016/S0142-9612(01)00040-0 ↗
9. 10.1016/j.matdes.2008.10.01610.1016/j.matdes.2008.10.016 ↗
10. 10.1016/j.jmatprotec.2007.12.12110.1016/j.jmatprotec.2007.12.121 ↗
11. 10.1016/j.msea.2007.07.00810.1016/j.msea.2007.07.008 ↗
12. 10.1016/j.scriptamat.2007.06.02910.1016/j.scriptamat.2007.06.029 ↗
13. 10.1016/j.msea.2006.10.02510.1016/j.msea.2006.10.025 ↗
14. 10.1016/j.jallcom.2007.07.03810.1016/j.jallcom.2007.07.038 ↗
15. 10.1016/j.jmatprotec.2007.03.09910.1016/j.jmatprotec.2007.03.099 ↗
16. 10.1016/S0142-9612(99)00206-910.1016/S0142-9612(99)00206-9 ↗
17. Iqbal N. · Journal of Non-Crystalline Solids · 2007 · 106
18. 10.1016/j.jmps.2007.02.00710.1016/j.jmps.2007.02.007 ↗
19. 10.1016/j.msea.2006.11.16610.1016/j.msea.2006.11.166 ↗
20. 10.1016/j.msea.2006.12.07710.1016/j.msea.2006.12.077 ↗
21. 10.1016/j.msea.2006.06.08110.1016/j.msea.2006.06.081 ↗
22. 10.1016/j.actamat.2006.11.00910.1016/j.actamat.2006.11.009 ↗