Thermal Shock Endurance of Porous Steel with Plasma Sprayed ZrO2Coating
Source abstract
Abstract
Abstract A new thermal shock resistant material has been developed by plasma spraying ZrO3 (stabilized with 7 wt% CaO) on porous steel. When the porosity of the substrate steel is more than 25% and a Ni-Cr undercoating is applied, the ZrO2 coating cracks but does not spall off by water quenching from 1125°C to 25°C. Because the cracks are produced regularly, the water quenching test is considered as a new heat treatment method for high thermal shock endurance of the ZrO2 coatings. This material has gas penetrating capability, and may be used as a permanent casting mold.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Boch , P. , J. F. Coudert , and C. Gault ,Ceramic Materials and Components for Engines, Springer Verlag , Saarbruecken DEU , p. 682 , ( 1986 ).
2. 10.1016/0040-6090(82)90018-910.1016/0040-6090(82)90018-9 ↗
3. Shimizu Y. · Journal of Japan Thermal Spraying Society · 1991 · 28 · 20
4. 10.1080/1042691930893485110.1080/10426919308934851 ↗
5. Haas H. · Deutscher Verlag ruer Schweisstcchnik · 1985 · 98 · 103
6. Steffens , H.D. , Z. Babiak , and U. Fischer ,Second International Conference on Surface Engineering, Welding Institute, Cambridge , U.K. , p. 471 , ( 1987 ).
7. Morgan V.T. · Metal Powder Report · 1986 · 41 · 39
8. Kamijo E. · Chemical Engineering · 1981 · 26 · 746
9. Harada R. · Application H 4–69126 · 1992
10. 10.1557/PROC-251-14110.1557/PROC-251-141 ↗
11. Elstner I. · Sprechsaal fuer Keramik Glas Email Silikate · 1982 · 115 · 549
12. Agapiou J.S. · International Journal of Powder Metallurgy · 1988 · 24 · 47
13. Kopp W.-U. · Praktische Metallographie · 1985 · 22 · 490