Comparative study of conventional and glass fiber modified ceramic shells
Source abstract
Abstract
Investment casting (IC) is well known to produced castings with excellent surface finish quality and close dimensional accuracy. Shell cracking is the foremost cause of casting rejection in the IC process. There are many causes of shell cracking in the IC process. However, the leading cause is poor shell strength. The shells having poor strength would produce defects on the final cast part and degraded the mechanical properties of the part. In this research work, the main objective was to improve ceramic shell strength by adding glass fibers to the backup coat ceramic slurry. It can be observed that the addition of glass fibers enhanced the flexural strength of the modified shell when compared to that of the conventional shell. The highest flexural strength was exhibited by the shell, which was modified with 0.50 wt.% of glass fibers. Fiber-reinforced modified ceramic shells had a larger bonded area between the fibers modified ceramic slurry and stucco coating. FE-SEM was used to analyze the microstructure characterization. Permeability and inner layer roughness of conventional and modified shells were measured and compared with conventional shells. XRD analysis was carried out with 0.50 wt.% of glass-fibers of unfired and fired shells at 700°C, 800°C & 900°C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Additive Manufacturing and 3D Printing Technologies · Innovations in Concrete and Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical and Industrial Engineering, Indian Institute of Technology Roorkee, Roorkee, India
Department of Mechanical Engineering, G H Raisoni Institute of Business Management Jalgaon, Jalgaon, India
References (18)
Show source-provided references
1. 10.1016/j.jmatprotec.2012.06.00310.1016/j.jmatprotec.2012.06.003 ↗
2. 10.1179/09679780222500331610.1179/096797802225003316 ↗
3. 10.1007/s12206-012-1218-510.1007/s12206-012-1218-5 ↗
4. 10.1016/j.jeurceramsoc.2020.07.01310.1016/j.jeurceramsoc.2020.07.013 ↗
5. 10.1080/10426914.2010.49612510.1080/10426914.2010.496125 ↗
6. 10.1016/j.jeurceramsoc.2021.09.02210.1016/j.jeurceramsoc.2021.09.022 ↗
7. 10.1016/j.compstruct.2018.09.07210.1016/j.compstruct.2018.09.072 ↗
8. Jones, S. Improved Sol Based Ceramic Moulds for Use in Investment Casting. Doctoral dissertation, University of Birmingham, UK, 1993.
9. 10.1016/j.ceramint.2018.01.13110.1016/j.ceramint.2018.01.131 ↗
10. 10.1007/s12666-020-01872-510.1007/s12666-020-01872-5 ↗
11. 10.1016/S0955-2219(02)00153-X10.1016/S0955-2219(02)00153-X ↗
12. 10.1016/S0924-0136(02)00907-X10.1016/S0924-0136(02)00907-X ↗
13. 10.1016/S0955-2219(02)00153-X10.1016/S0955-2219(02)00153-X ↗
14. 10.1016/j.ceramint.2018.06.06310.1016/j.ceramint.2018.06.063 ↗
15. 10.1007/s40962-018-00297-710.1007/s40962-018-00297-7 ↗
16. 10.1016/j.ceramint.2013.06.02710.1016/j.ceramint.2013.06.027 ↗
17. 10.1016/j.jmatprotec.2011.03.00210.1016/j.jmatprotec.2011.03.002 ↗
18. 10.1007/s00170-017-0735-x10.1007/s00170-017-0735-x ↗