journal article·2012-08

M2 Machine Gun Barrel Wear with SLAP Ammunition

Michael R. Hespos

Publisher page

Abstract

Abstract The M2 machine gun has a Stellite-lined barrel. When Saboted-Light-Armor-Penetrator (SLAP) ammunition is fired in M2 barrels, the bore often constricts below the minimum diameter in less than 2,500 rounds. The requirement is 10,000 rounds. When fired with ball ammunition, the M2 barrel exceeds that requirement. Although SLAP ammunition is not widely used, solving the wear issue with SLAP may improve the barrel life with ball ammunition. The following work is presented: a literature search, an analysis of the wear phenomenon and manufacturing process, as well as recommendations to improve M2 barrel life. Brief mention will be made of prototype small caliber gun barrels being fabricated and tested. Previous work and testing conducted herein find that the bore constriction is most likely caused by inadequate shrink fit during the barrel assembly process. That is, test results find some correlation between barrels with low round count and non-conforming barrel assembly. Keywords: Bore shrinkageGas seepageLiner bond strengthM2 barrel wearResidual stressRetainer torqueShear testShrink fitSLAP ammunitionStellite Notes This article not subject to U.S. copyright law.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electromagnetic Launch and Propulsion Technology · High-Velocity Impact and Material Behavior · Energetic Materials and Combustion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Hespos , M. Crazing of M2,50 Caliber Stellite Liner. Lab test results, June 30, 1995.
2. Desrochers , M. Proposal for Improvement of M2 .50 Caliber Machine Gun Performance with SLAP Ammunition. Facsimile, April 15, 1996.
3. Montgomery , J.S. ; de Rosset , W.S. Machine gun liner bond strength. ARL-CR-595, August 2007.
4. Ebihara , W.T. Structural stability of a cast Co-Cr-Mo-alloy during impulsive thermal-mechanical loading. AD 721895, December 1970.10.21236/AD0721895 ↗
5. Ebihara , W.T. Wear and erosion characteristics of a cast cobalt alloy. AD 759125, January 1973.10.21236/AD0759125 ↗
6. Gray , N. ; Giles , R. ; Bredbury , S. Erosion firing tests: Candidate tests of experimental caliber .50, M2 HB machine gun barrels. AD-E401797, June 1988.
7. Gray , N. ; Giles , R. ; Bredbury , S. Erosion firing tests: Candidate tests of experimental caliber .50, M2 HB machine gun barrels. AD-E401799, June 1988.
8. Hammer , A. ; DiBenedetto , J. ; Iyer , K. ; Ebihara , W. ; Thomsen , D. ; Leech , W. ; Chu , S. Gun barrel technology at Weapons Laboratory. Rock Island 1968–1971.
9. Harlow , R. ; Kimball , R. Aeronutronic advanced gun barrel development program. AD0714688, February 1970.
10. Ard , P. Research and development on coextrusion of bimetallic .220 swift and 25 mm gun barrels. Technical Report AFATL-TR-72–232, December 1972.
11. Rorabaugh D. · 1988
12. Krauss , G.Steels: Processing, Structure, and Performance., 5th ed. , ASM International , 2005 , 349 pp.
13. Garron , R. ; Hespos , M. Microscopy of P3A-9 barrel after firing 24,000 rounds. Internal ARDEC report, April 14, 2011.