Towards a more effective and reliable salt crystallization test for porous building materials: state of the art
Source abstract
Abstract
The durability of building materials with respect to salt crystallization is commonly determined by accelerated weathering tests, carried out in the laboratory. An effective laboratory weathering test should assess the durability and, in the case of conservation of historic buildings, the compatibility of repair materials with those existing. Besides, the test should provide reliable results within a reasonable period of time, accelerating the deterioration process without however altering its mechanism. Despite several national and international standards, recommendations and guidelines, a commonly accepted testing protocol does not yet exist. Researchers often develop and apply their own procedure, a fact that complicates comparison between different studies. The RILEM Technical Committee 271 ASC has been set up with the scope of developing improved test procedures for the assessment of the behaviour of materials under the influence of salt crystallization, which should overcome the limitations of existing standards and recommendations. This paper constitutes one of the first results of the work of the Technical Committee. It critically reviews the literature on salt crystallization tests, identifies advantages and limitations of the several test protocols and provides new ideas for the development of improved salt crystallization procedures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Building materials and conservation · Conservation Techniques and Studies · Cultural Heritage Materials Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Goudie AS, Viles HA (1997) Salt weathering hazards. Wiley, Chichester
2. Charola AE (2000) Salts in the deterioration of porous materials: an overview. J Am Inst Conserv 39:327–34310.2307/3179977 ↗
3. Doehne E (2002) Salt weathering: a selective review, salt weathering: a selective review. Geol Soc Spec Pub 205(1):51–6410.1144/GSL.SP.2002.205.01.05 ↗
4. CEN (1999) EN 12370 Natural stone test methods. Determination of resistance to salt crystallization
5. RILEM (1980) Recommended tests to measure the deterioration of stone and to assess the effectiveness of treatment methods, Test V.1a—crystallization test by total immersion (for untreated stone); Test V.1b—crystallization test by total immersion (for treated stone); Test V.2—crystallization test by partial immersion. Mater Struct 13(75):175–253
6. RILEM TC 127-MS (1998) MS-A.1—determination of the resistance of wallettes against sulphates and chlorides. Mater Struct 31:2–910.1007/BF02486406 ↗
7. RILEM TC 127-MS (1998) MS-A.2—uni-directional salt crystallization test for masonry units. Mater Struct 31:10–1110.1007/BF02486407 ↗
8. WTA Merkblatt 2-9-04/D (2005) Sanierputzsysteme/Renovation mortar systems. WTA Publications, Stuttgart
9. West D (2000) Brard’s test into the 21st century: sodium sulphate soundness testing of dimension stone. In: McNally GH, Franklin BJ (eds) Sandstone city: Sydney’s dimension stone and other sandstone geomaterials. Proceedings of a symposium held on 7th July 2000, during the 15th Australian geological convention at the University of Technology, Sydney. Geological Society of Australia, Environmental, Engineering and Hydrology Specialist Group, Monograph 5, pp 138–148
10. Doehne E, Selwitz C, Carson D (2002) The damage mechanism of sodium sulphate in porous stone. In: Proceedings of the SALTeXPERT meeting, pp 27–146
11. Lubelli B, Van Hees RPJ, Nijland TG (2014) Salt crystallization damage: how realistic are existing ageing tests? In: De Clercq H (ed) Proceedings of the international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 259–273
12. Beck K, Al-Mukhtar M (2010) Evaluation of the compatibility of building limestones from salt crystallization experiments. Geol Soc Lond Spec Publ 333(1):111–118. https://doi.org/10.1144/sp333.1110.1144/sp333.11 ↗
13. Van Hees RPJ, Brocken HJP (2001) Interaction of the SBW treatment with Na2SO4, NaCl and NaNO3. In: De Witte E (ed) Salt compatibility of surface treatment (SCOST), final report, EU Contract No. ENV4-CT98-0710, pp 109–119
14. Van Hees RPJ, Brocken HJP (2004) Damage development to treated brick masonry in a long-term salt crystallisation test. Constr Build Mater 18(5):331–338. https://doi.org/10.1016/j.conbuildmat.2004.02.00610.1016/j.conbuildmat.2004.02.006 ↗
15. Wijffels T, Lubelli B (2006) Development of a new accelerated salt crystallization test. Heron 51(1):63–79
16. Velosa AL, Veiga MR (2006) Development of artificial ageing tests for renders: application to conservation mortars. In: Thompson G (ed) Proceedings of the 7th international masonry conference, British Masonry Society, London
17. Gonçalves TD (2007) Salt crystallisation in plastered or rendered walls. Ph.D. dissertation, Instituto Superior Técnico da Universidade Técnica de Lisboa
18. Fragata A, Veiga MR, Velosa A (2016) Substitution ventilated render systems for historic masonry: salt crystallization tests evaluation. Constr Build Mater 102(1):592–600. https://doi.org/10.1016/j.conbuildmat.2015.10.13010.1016/j.conbuildmat.2015.10.130 ↗
19. Franzoni E, Gentilini C, Santandrea M, Zanotto S, Carloni C (2017) Durability of steel FRCM-masonry joints: effect of water and salt crystallization. Mater Struct. https://doi.org/10.1617/s11527-017-1070-210.1617/s11527-017-1070-2 ↗
20. Groot CJWP (1993) Effect of water on mortar-brick bond. Ph.D. dissertation, Delft University of Technology
21. Wijffels TJ, Van Hees RPJ (2000) The influence of the loss of water of the fresh mortar to the substrate on the hygric characteristics of so-called restoration plaster. In: Verhoef L, Wittman F (eds) Proceedings of the international workshop on urban heritage and building maintenance VII, Aedificatio Publishers, Freiburg, pp 49–54
22. Smith BJ, McGreevy JP (1983) A simulation study of salt weathering in hot deserts. Geogr Ann Ser A 65(1–2):127–133. https://doi.org/10.1080/04353676.1983.1188007910.1080/04353676.1983.11880079 ↗
23. Cnudde V, De Boever W, Dewanckele J, De Kock T, Boone M, Boone MN et al (2013) Multi-disciplinary characterization and monitoring of sandstone (Kandla Grey) under different external conditions. Q J Eng Geol Hydrogeol 46(1):95–106. https://doi.org/10.1144/qjegh2012-00510.1144/qjegh2012-005 ↗
24. Akin M, Özsan A (2011) Evaluation of the long-term durability of yellow travertine using accelerated weathering tests. Bull Eng Geol Environ 70(1):101–114. https://doi.org/10.1007/s10064-010-0287-x10.1007/s10064-010-0287-x ↗
25. Kyriakou L, Theodoridou M, Ioannou I (2017) Assessment of the durability of lime renders with Phase Change Material (PCM) additives against salt crystallization. In: Laue S (ed) Proceedings of the fourth international conference on salt weathering of buildings and stone sculptures (SWBSS 2017), University of Applied Sciences, Potsdam, pp 81–89
26. Diaz Gonçalves T, Brito V, Musacchi J, Pel L, Saidov T, Delgado Rodrigues J, Costa D, Mimoso JM (2014) Drying of porous building materials possibly contaminated with soluble salts: summary and findings of the DRYMASS research project. In: De Clercq H (ed) Proceedings of the international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 1–15
27. Janvier-Badosa S, Beck K, Brunetaud X, Guirimand-Dufour A, Al-Mukhtar M (2015) Gypsum and spalling decay mechanism of tuffeau limestone. Environ Earth Sci 74(3):2209–2221. https://doi.org/10.1007/s12665-015-4212-210.1007/s12665-015-4212-2 ↗
28. Angeli M, Bigas J-P, Benavente D, Menéndez B, Hébert R, David C (2007) Salt crystallization in pores: quantification and estimation of damage. Environ Geol 52(2):205–213. https://doi.org/10.1007/s00254-006-0474-z10.1007/s00254-006-0474-z ↗
29. Dewanckele J, Boone MA, De Kock T, De Boever W, Brabant L, Boone MN et al (2013) Holistic approach of pre-existing flaws on the decay of two limestones. Sci Total Environ 447:403–414. https://doi.org/10.1016/j.scitotenv.2012.12.09410.1016/j.scitotenv.2012.12.094 ↗
30. Nunes C, Slížková Z, Křivanková D (2013) Lime-based mortars with linseed oil: sodium chloride resistance assessment and characterization of the degraded material. Period Mineral 82(3):411–427. https://doi.org/10.2451/2013pm002410.2451/2013pm0024 ↗
31. Bachmat Y, Bear J (1987) On the concept and size of a representative elementary volume (rev). In: Bear J, Corapcioglu MY (eds) Advances in transport phenomena in porous media. NATO ASI series (Series E: applied sciences), vol 128. Springer, Dordrecht
32. Al-Raoush R, Papadopoulos A (2010) Representative elementary volume analysis of porous media using X-ray computed tomography. Powder Technol 200(1–2):69–7710.1016/j.powtec.2010.02.011 ↗
33. ASTM Subcommittee D18.17 (2013) ASTM 5240 standard test method for evaluation of durability of rock for erosion control using sodium sulfate or magnesium sulfate
34. Steiger M, Asmussen S (2008) Crystallization of sodium sulfate phases in porous materials: the phase diagram Na2SO4–H2O and the generation of stress. Geochim Cosmochim Acta 72(17):4291–4306. https://doi.org/10.1016/j.gca.2008.05.05310.1016/j.gca.2008.05.053 ↗
35. Rodriguez-Navarro C, Doehne E, Sebastian E (2000) How does sodium sulfate crystallize? Implications for the decay and testing of building materials. Cem Concr Res 30(10):1527–1534. https://doi.org/10.1016/s0008-8846(00)00381-110.1016/s0008-8846(00)00381-1 ↗
36. Flatt RJ (2002) Salt damage in porous materials: how high supersaturations are generated. J Cryst Growth 242:435–454. https://doi.org/10.1016/s0022-0248(02)01429-x10.1016/s0022-0248(02)01429-x ↗
37. Desarnaud J, Bertrand F, Shahidzadeh-Bonn N (2013) Impact of the kinetics of salt crystallization on stone damage during rewetting/drying and humidity cycling. J Appl Mech 80(2):020911. https://doi.org/10.1115/1.400792410.1115/1.4007924 ↗
38. Goudie A, Cooke R, Evans I (1970) Experimental investigation of rock weathering by salts. Area 2(4):42–48
39. Kwaad FJPM (1970) Experiments on the granular disintegration of granite by salt action. Fysisch Geografisch Bodemkundig Laboratorium From Field to Laboratory 16:67–80
40. Cooke RU (1979) Laboratory simulation of salt weathering processes in arid environments. Earth Surf Process 4(4):347–359. https://doi.org/10.1002/esp.329004040510.1002/esp.3290040405 ↗
41. Wells T, Binning P, Willgoose G, Hancock G (2006) Laboratory simulation of the salt weathering of schist: 1. Weathering of schist blocks in a seasonally wet tropical environment. Earth Surf Proc Land 31(3):339–354. https://doi.org/10.1002/esp.124810.1002/esp.1248 ↗
42. Ruiz-Agudo E, Mees F, Jacobs P, Rodriguez-Navarro C (2007) The role of saline solution properties on porous limestone salt weathering by magnesium and sodium sulfates. Environ Geol 52(2):269–281. https://doi.org/10.1007/s00254-006-0476-x10.1007/s00254-006-0476-x ↗
43. Ioannou I, Fournari R, Petrou MF (2013) Testing the soundness of aggregates using different methodologies. Constr Build Mater 40:604–61010.1016/j.conbuildmat.2012.11.047 ↗
44. Balboni E, Espinosa-Marzal RM, Doehne E, Scherer GW (2010) Can drying and re-wetting of magnesium sulfate salts lead to damage of stone? Environ Earth Sci 63(7–8):1463–1473. https://doi.org/10.1007/s12665-010-0774-110.1007/s12665-010-0774-1 ↗
45. Espinosa-Marzal RM, Scherer GW (2011) Mechanisms of damage by salt. Geol Soc Lond Spec Publ 331(1):61–77. https://doi.org/10.1144/sp331.510.1144/sp331.5 ↗
46. Rodriguez-Navarro C, Doehne E (1999) Salt weathering: influence of evaporation rate, supersaturation and crystallization pattern. Earth Surf Proc Land 24(3):191–20910.1002/(SICI)1096-9837(199903)24:3<191::AID-ESP942>3.0.CO;2-G ↗
47. Gentilini C, Franzoni E, Bandini S, Nobile L (2012) Effect of salt crystallisation on the shear behaviour of masonry walls: an experimental study. Constr Build Mater 37:181–189. https://doi.org/10.1016/j.conbuildmat.2012.07.08610.1016/j.conbuildmat.2012.07.086 ↗
48. Stefanidou M, Papayanni I (1999) Resistance of repair mortars of historic structures to wetting-drying salt cycles. In: Arun G (ed) Proceedings of the international symposium studies on historical heritage (SHH07), Yıldız Technical University, Istanbul, pp 347–354
49. Steiger M (2005) Crystal growth in porous materials—I: the crystallization pressure of large crystals. J Cryst Growth 282(3–4):455–469. https://doi.org/10.1016/j.jcrysgro.2005.05.00710.1016/j.jcrysgro.2005.05.007 ↗
50. Lubelli B (2006) Sodium chloride damage to porous building materials. Ph.D. dissertation, Delft University of Technology
51. Gonçalves TD, Pel L, Rodrigues JD (2009) Influence of paints on drying and salt distribution processes in porous building materials. Constr Build Mater 23(5):1751–1759. https://doi.org/10.1016/j.conbuildmat.2008.08.00610.1016/j.conbuildmat.2008.08.006 ↗
52. Goudie AS (1986) Laboratory simulation of “the wick effect” in salt weathering of rock. Earth Surf Proc Land 11(3):275–285. https://doi.org/10.1002/esp.329011030510.1002/esp.3290110305 ↗
53. De Freece SN, Weber J, Charola AE (2005) Hygric behaviour of two of the most deteriorating salts: sodium sulphate and sodium carbonate. Restor Build Monum 11(2):79–86. https://doi.org/10.1515/rbm-2005-593810.1515/rbm-2005-5938 ↗
54. López-Arce P, Tagnit-Hammou M, Menéndez B, Mertz J-D, Kaci A (2016) Durability of stone-repair mortars used in historic buildings from Paris. Mater Struct 49(12):5097–5115. https://doi.org/10.1617/s11527-016-0846-010.1617/s11527-016-0846-0 ↗
55. Tingstad A (2008) Simulation of salt weathering in a closely replicated coastal environment. Geogr Ann Ser A 90(2):165–171. https://doi.org/10.1111/j.1468-0459.2008.00166.x10.1111/j.1468-0459.2008.00166.x ↗
56. Williams RGB, Robinson DA (1998) Weathering of sandstone by alunogen and alum salts. Q J Eng Geol 31:369–37310.1144/GSL.QJEG.1998.031.P4.10 ↗
57. Robinson DA, Williams RBG (2000) Experimental weathering of sandstone by combinations of salts. Earth Surf Proc Land 25:1309–131510.1002/1096-9837(200011)25:12<1309::AID-ESP139>3.0.CO;2-5 ↗
58. De Clercq H (2008)The effect of other salts on the crystallization damage to stone caused by sodium sulfate. In: Proceedings of the SWBSS2008 conference, Copenhangen, 2008, pp 307–315
59. De Clercq H, Jovanovic M, Linnow K, Steiger M (2013) Performance of limestones laden with mixed salt solutions of Na2SO4–NaNO3 and Na2SO4–K2SO4. Environ Earth Sci 69:1751–1761. https://doi.org/10.1007/s12665-012-2017-010.1007/s12665-012-2017-0 ↗
60. Godts S, Hendrickx R, De Clercq H (2014) The crystallization behavior of sodium magnesium sulfate in limestone. In: De Clercq H (ed) Proceedings of the third international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 167–182
61. Menéndez B, Petráňová V (2016) Effect of mixed vs single brine composition on salt weathering in porous carbonate building stones for different environmental conditions. Eng Geol 210:124–139. https://doi.org/10.1016/j.enggeo.2016.06.01110.1016/j.enggeo.2016.06.011 ↗
62. Arizzi A, Viles H, Cultrone G (2012) Experimental testing of the durability of lime-based mortars used for rendering historic buildings. Constr Build Mater 28(1):807–818. https://doi.org/10.1016/j.conbuildmat.2011.10.05910.1016/j.conbuildmat.2011.10.059 ↗
63. Benavente D, Martínez-Martínez J, Cueto N, García-del-Cura MA (2007) Salt weathering in dual-porosity building dolostones. Eng Geol 94(3–4):215–226. https://doi.org/10.1016/j.enggeo.2007.08.00310.1016/j.enggeo.2007.08.003 ↗
64. Alves C, Figueiredo C, Maurício A (2017) A critical discussion of salt weathering laboratory tests for assessment of petrological features susceptibility. Proc Earth Planet Sci 17:324–327. https://doi.org/10.1016/j.proeps.2016.12.08210.1016/j.proeps.2016.12.082 ↗
65. Graziani G, Sassoni E, Franzoni E (2016) Experimental study on the salt weathering resistance of fired clay bricks consolidated by ethyl silicate. Mater Struct 49(7):2525–2533. https://doi.org/10.1617/s11527-015-0665-810.1617/s11527-015-0665-8 ↗
66. Sassoni E, Graziani G, Franzoni E (2016) An innovative phosphate-based consolidant for limestone. Part 2: durability in comparison with ethyl silicate. Constr Build Mater 102:931–942. https://doi.org/10.1016/j.conbuildmat.2015.10.20210.1016/j.conbuildmat.2015.10.202 ↗
67. Goudie AS, Parker AG (1998) Experimental simulation of rapid rock block disintegration by sodium chloride in a foggy coastal desert. J Arid Environ 40(4):347–355. https://doi.org/10.1006/jare.1998.046510.1006/jare.1998.0465 ↗
68. Henriques FMA, Charola AE (2000) Development of lime mortars with improved resistance to sodium chloride crystallization. In: Fassina V (ed) Proceedings of the 9th international conference on deterioration and conservation of stone, vol 2. Elsevier, Venice, pp 335–342
69. Lubelli B, Nijland TG, Van Hees RPJ, Hacquebord A (2010) Effect of mixed in crystallization inhibitor on resistance of lime–cement mortar against NaCl crystallization. Constr Build Mater 24(12):2466–2472. https://doi.org/10.1016/j.conbuildmat.2010.06.01010.1016/j.conbuildmat.2010.06.010 ↗
70. Goudie AS (1999) Experimental salt weathering of limestones in relation to rock properties. Earth Surf Proc Land 24:175–72410.1002/(SICI)1096-9837(199908)24:8<715::AID-ESP4>3.0.CO;2-# ↗
71. Van Tri T, Beck K, Al-Mukhtar M (2006) Accelerated weathering tests on two highly porous limestones. Environ Geol 52(2):283–292. https://doi.org/10.1007/s00254-006-0532-610.1007/s00254-006-0532-6 ↗
72. Ioannou I, Hoff WD (2008) Water repellent influence on salt crystallisation in masonry. Proc Inst Civil Eng Constr Mater 161(1):17–23. https://doi.org/10.1680/coma.2008.161.1.1710.1680/coma.2008.161.1.17 ↗
73. Alves C, Figueiredo C, Maurício A, Braga MAS, Aires-Barros L (2011) Limestones under salt decay tests: assessment of pore network-dependent durability predictors. Environ Earth Sci 63(7–8):1511–1527. https://doi.org/10.1007/s12665-011-0915-110.1007/s12665-011-0915-1 ↗
74. Franzoni E, Gentilini C, Graziani G, Bandini S (2014) Towards the assessment of the shear behaviour of masonry in on-site conditions: a study on dry and salt/water conditioned brick masonry triplets. Constr Build Mater 65:405–416. https://doi.org/10.1016/j.conbuildmat.2014.05.00210.1016/j.conbuildmat.2014.05.002 ↗
75. Van Hees RPJ, Brocken H (2003) The salt crystallisation method. In: De Witte E (ed) Salt compatibility of surface treatment (SCOST), final report, EU Contract No. ENV4-CT98-0710, institution? city?, pp 35–37
76. Miquel A, Bromblet P, Vergès-Belmin V (2003) Compatibility of SBW treated substrates with Na2SO4. In: De Witte E (ed) Salt compatibility of surface treatment (SCOST), final report, EU Contract No. ENV4-CT98-0710, institution? city? pp 73–95
77. De Clerq H, De Witte E (2003) Interaction of the type of treatment with different types of salt. In: De Witte E (ed) Salt compatibility of surface treatment (SCOST), final report, EU Contract No. ENV4-CT98-0710, institution? city? pp 142–144
78. De Clercq H (2005) Performance of single materials treated with a water repellent and contaminated with a salt mix. In: Silfwerbrand J (ed) Proceedings of the 4th international conference on water repellent treatment of building materials (Hydrophobe IV), Aedificatio Publishers, Brussels, Aedificatio Publishers, Freiburg, pp 171–184
79. De Clercq H (2008) Performance of limestone contaminated with binary mixtures of sodium sulphate and treated with a water repellent. In: De Clercq H (ed) Proceedings of the 5th international conference on water repellent treatment of building materials (Hydrophobe V), Aedificatio Publishers, Brussels, pp 107–116
80. Vergès-Belmin V, Wijfels T, Gonçalves TD, Nasraoui M (2005) The COMPASS salt crystallization test as a way to figure out how salts migrate and accumulate in renovation plasters. In: Van Hees RPJ (ed) Compatibility of plasters and renders with salt loaded substrates in historic buildings, final report, EU Contract No. EVK4-CT-2001-0047-DGXII, institution? city? pp 157–168
81. López-Doncel R, Wedekind W, Leiser T, Molina-Maldonado S, Velasco-Sánchez A, Dohrmann R, Kral A, Wittenborn A, Aguillón-Robles A, Siegesmund S (2016) Salt bursting tests on volcanic tuff rocks from Mexico. Environ Earth Sci. https://doi.org/10.1007/s12665-015-4770-310.1007/s12665-015-4770-3 ↗
82. Cultrone G, Sebastián E, Huertas MO (2007) Durability of masonry systems: a laboratory study. Constr Build Mater 21(1):40–51. https://doi.org/10.1016/j.conbuildmat.2005.07.00810.1016/j.conbuildmat.2005.07.008 ↗
83. Sassoni E, Franzoni E, Graziani G, Sagripanti F (2014) Limestone resistance to sodium sulfate degradation after consolidation by hydroxyapatite and TEOS. In: De Clercq H (ed) Proceedings of the international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 335–345
84. Rivas T, Alvarez E, Mosquera MJ, Alejano L, Taboada J (2010) Crystallization modifiers applied in granite desalination: the role of the stone pore structure. Constr Build Mater 24(5):766–776. https://doi.org/10.1016/j.conbuildmat.2009.10.03110.1016/j.conbuildmat.2009.10.031 ↗
85. Aly N, Gomez-Heras M, Hamed A, Alvarez de Buergo M, Soliman F (2014) Porosity changes after different temperature regimes for a salt weathering simulation test on Mokkattam limestone (Egypt). In: De Clercq H (ed) Proceedings of the international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 247–25710.3989/mc.2015.00514 ↗
86. Goudie AS (1993) Salt weathering simulation using a single-immersion technique. Earth Surf Proc Land 18(4):369–376. https://doi.org/10.1002/esp.329018040610.1002/esp.3290180406 ↗
87. Flatt R et al (2017) Predicting salt damage in practice: a theoretical insight into laboratory tests. RILEM Tech Lett 2:108–11810.21809/rilemtechlett.2017.41 ↗
88. Angeli M, Hébert R, Menéndez B, David C, Bigas J-P (2010) Influence of temperature and salt concentration on the salt weathering of a sedimentary stone with sodium sulphate. Eng Geol 115(3–4):193–199. https://doi.org/10.1016/j.enggeo.2009.06.00110.1016/j.enggeo.2009.06.001 ↗
89. Espinosa-Marzal RM, Scherer GW (2012) Impact of in-pore salt crystallization on transport properties. Environ Earth Sci 69(8):2657–2669. https://doi.org/10.1007/s12665-012-2087-z10.1007/s12665-012-2087-z ↗
90. Derluyn H, Boone MA, Boone MN, De Kock T, Desarnaud J, Peetermans S, Molari L, De Miranda S, Shahidzadeh N, Cnudde V (2015) Salt crystallization dynamics in building rocks: a 4D study using laboratory X-ray micro-CT. In: Long B (ed) Proceedings of the 2nd international conference on tomography of materials and structures (ICTMS 2015), Québec, pp 565–568
91. Shahidzadeh-Bonn N, Rafaï S, Bonn D, Wegdam G (2008) Salt crystallization during evaporation: impact of interfacial properties. Langmuir 24(16):8599–8605. https://doi.org/10.1021/la800562910.1021/la8005629 ↗
92. Schäfer M, Steiger M (2002) A rapid method for the determination of cation exchange capacities of sandstones: preliminary data. Geol Soc Lond Spec Publ 205(1):431–439. https://doi.org/10.1144/gsl.sp.2002.205.01.3110.1144/gsl.sp.2002.205.01.31 ↗
93. Benavente D, García del Cura M, Bernabéu A, Ordóñez S (2001) Quantification of salt weathering in porous stones using an experimental continuous partial immersion method. Eng Geol 59(3–4):313–325. https://doi.org/10.1016/s0013-7952(01)00020-510.1016/s0013-7952(01)00020-5 ↗
94. Tsui N, Flatt RJ, Scherer GW (2003) Crystallization damage by sodium sulfate. J Cult Herit 4(2):109–115. https://doi.org/10.1016/s1296-2074(03)00022-010.1016/s1296-2074(03)00022-0 ↗
95. Delgado Rodrigues J, Ferreira Pinto A, Nunes C (2007) Preparation of aged samples for testing stone treatments. In: Proceedings of the 23th international convention Scienza e Beni Culturale—Il Consolidamento degli Apparati Architettonici e Decorativi, Arcadia Ricerche, Marghera Venezia, pp 597–605
96. Diaz Gonçalves T, Brito V (2014) Alteration kinetics of natural stones due to sodium sulfate crystallization: can reality match experimental simulations? Environ Earth Sci 72(6):1789–1799. https://doi.org/10.1007/s12665-014-3085-010.1007/s12665-014-3085-0 ↗
97. Stahlbuhk A, Nissen J, Linnow K, Steiger M (2014) Influence of the salt concentration on the damage potential of mirabilite and thenardite. In: De Clercq H (ed) Proceedings of the international conference on salt weathering of buildings and stone sculptures (SWBSS 2014), Aedificatio Publishers, Brussels, pp 35–48
98. Lubelli B, van Hees RPJ, Groot CJWP (2006) The effect of environmental conditions on sodium chloride damage. Stud Conserv 51(1):41–56. https://doi.org/10.1179/sic.2006.51.1.4110.1179/sic.2006.51.1.41 ↗
99. Lindström N, Heitmann N, Linnow K, Steiger M (2015) Crystallization behavior of NaNO3–Na2SO4 salt mixtures in sandstone and comparison to single salt behavior. Appl Geochem 63:116–132. https://doi.org/10.1016/j.apgeochem.2015.07.00710.1016/j.apgeochem.2015.07.007 ↗
100. Cnudde V, Cnudde JP, Dupuis C, Jacobs PJS (2004) X-ray micro-CT used for the localization of water repellents and consolidants inside natural building stones. Mater Charact 53:259–27110.1016/j.matchar.2004.08.011 ↗