Abstract

Alkali silicate activated slag (AAS) most commonly develops high strength, but is usually accompanied by fast setting. In this study, slag was activated by a potassium silicate solution possessing different moduli (Ms = 0.7 and 1). The workability of the alkali activated slag mortar, at 4 and 20 min, was assessed by means of a mini-slump test. The sample with an Ms of 1 was not workable after 20 min. Calcium formate was subsequently added to extend the workable time of the mortar but this lowered its compressive strength. Ultrasonic measurements indicated a slower solid phase development in the AAS paste, in the presence of calcium formate, which was associated with a decreased amount of C–S–H gel in the hydrates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Komljenović M (2015) Mechanical strength and Young’s modulus of alkali-activated cement-based binders. In: Pacheco-Torgal F (ed) Handbook of alkali-activated cements, mortars and concretes. Woodhead Publishing, Cambridge, pp 171–21510.1533/9781782422884.2.171 ↗
2. Tänzer R, Buchwald A, Stephan D (2015) Effect of slag chemistry on the hydration of alkali-activated blast-furnace slag. Mater Struct 48(3):629–64110.1617/s11527-014-0461-x ↗
3. Haha MB, Lothenbach B, Le Saout G, Winnefeld F (2011) Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag—part I: effect of MgO. Cem Concr Res 41(9):955–96310.1016/j.cemconres.2011.05.002 ↗
4. Haha MB, Lothenbach B, Le Saout G, Winnefeld F (2012) Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag—part II: effect of Al2O3. Cem Concr Res 42(1):74–8310.1016/j.cemconres.2011.08.005 ↗
5. Wang S-D, Scrivener KL, Pratt PL (1994) Factors affecting the strength of alkali-activated slag. Cem Concr Res 24(6):1033–104310.1016/0008-8846(94)90026-4 ↗
6. Krizan D, Zivanovic B (2002) Effects of dosage and modulus of water glass on early hydration of alkali–slag cements. Cem Concr Res 32(8):1181–118810.1016/S0008-8846(01)00717-7 ↗
7. Dakhane A, Peng Z, Marzke R, Neithalath N (2014) Comparative analysis of the influence of sodium and potassium silicate solutions on the kinetics and products of slag activation. Adv Civ Eng Mater 3(1):371–38710.1520/ACEM20140005 ↗
8. Tänzer R, Jin Y, Stephan D (2017) Alkali activated slag binder: effect of cations from silicate activators. Mater Struct 50(1):110.1617/s11527-016-0961-y ↗
9. Shi C, Krivenko PV, Roy DM (2006) Alkali-activated cements and concretes: theory and application. Taylor & Francis, London10.4324/9780203390672 ↗
10. Zhang Z, Zhou D, Li F, Pan Z, Yang N (2008) Selection of retarder of alkali activated slag cement. Concrete 8:63–68 (in Chinese)
11. Brough AR, Holloway M, Sykes J, Atkinson A (2000) Sodium silicate-based alkali-activated slag mortars. Part II. The retarding effect of additions of sodium chloride or malic acid. Cem Concr Res 30(9):1375–137910.1016/S0008-8846(00)00356-2 ↗
12. Chang JJ, Yeih W, Hung CC (2005) Effects of gypsum and phosphoric acid on the properties of sodium silicate-based alkali-activated slag pastes. Cement Concr Compos 27(1):85–9110.1016/j.cemconcomp.2003.12.001 ↗
13. Gong C, Yang N (2000) Effect of phosphate on the hydration of alkali-activated red mud–slag cementitious material. Cem Concr Res 30(7):1013–101610.1016/S0008-8846(00)00260-X ↗
14. Kalina L, Bílek V, Novotný R, Mončeková M, Másilko J, Koplík J (2016) Effect of Na3PO4 on the hydration process of alkali-activated blast furnace slag. Materials 9:(5)10.3390/ma9050395 ↗
15. Schultze W (1995) Dispersions-Silikatsysteme: Grundlagen - Formulierungen - Problemlösungen. Expert-Verlag, Renningen-Malmsheim
16. Snellings R (2013) Solution-Controlled Dissolution of Supplementary Cementitious Material Glasses at pH 13: The Effect of Solution Composition on Glass Dissolution Rates. J Am Ceram Soc 96(8):2467–247510.1111/jace.12480 ↗
17. Suraneni P, Palacios M, Flatt RJ (2016) New insights into the hydration of slag in alkaline media using a micro-reactor approach. Cem Concr Res 79:209–21610.1016/j.cemconres.2015.09.015 ↗
18. DIN EN 1015-3 (2007) Prüfverfahren für Mörtel für Mauerwerk – Teil 3: Bestimmung der Konsistenz von Frischmörtel (mit Ausbreittisch). 2004th ed; 91.100.10. Deutsches Institut für Normung e. V, Berlin, Germany
19. DIN EN 196-1 (2015) Prüfverfahren für Zement – Teil 1: Bestimmung der Festigkeit. 2015th ed; 91.100.10. Deutsches Institut für Normung e. V, Berlin, Germany
20. von Daake H, Stephan D (2016) Setting of cement with controlled superplasticizer addition monitored by ultrasonic measurements and calorimetry. Cement Concr Compos 66:24–3710.1016/j.cemconcomp.2015.11.004 ↗
21. Alonso MM, Gismera S, Blanco MT, Lanzón M, Puertas F (2017) Alkali-activated mortars: workability and rheological behaviour. Constr Build Mater 145:576–58710.1016/j.conbuildmat.2017.04.020 ↗
22. Fernández-Jiménez A, Puertas F (1997) Alkali-activated slag cements: kinetic studies. Cem Concr Res 27(3):359–36810.1016/S0008-8846(97)00040-9 ↗
23. Trtnik G, Turk G, Kavčič F, Bosiljkov VB (2008) Possibilities of using the ultrasonic wave transmission method to estimate initial setting time of cement paste. Cem Concr Res 38(11):1336–134210.1016/j.cemconres.2008.08.003 ↗
24. Silverstein RM, Webster FX, Kiemle DJ (2005) Spectrometric identification of organic compounds, 7th edn. Wiley, Hoboken
25. Yu P, Kirkpatrick RJ, Poe B, McMillan PF, Cong X (1999) Structure of calcium silicate hydrate (C–S–H): near-, mid-, and far-infrared spectroscopy. J Am Ceram Soc 82(3):742–74810.1111/j.1151-2916.1999.tb01826.x ↗
26. Fernandez-Jimenez A, Puertas F (2003) Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements. Adv Cem Res 15(3):129–13610.1680/adcr.2003.15.3.129 ↗
27. Mohassab Y, Sohn HY (2015) Analysis of slag chemistry by FTIR-RAS and Raman spectroscopy: effect of water vapor content in H2–H2O–CO–CO2 mixtures relevant to a novel green ironmaking technology. Steel Res Int 86(7):740–75210.1002/srin.201400186 ↗
28. Garbev K, Beuchle G, Schweike U, Merz D, Dregert O, Stemmermann P (2014) Preparation of a novel cementitious material from hydrothermally synthesized C–S–H phases. J Am Ceram Soc 97(7):2298–230710.1111/jace.12920 ↗
29. Pang LSK, Vassallo AM, Phong-anant D, Wilson MA (1993) A study of slag in laboratory, pilot and commercial scale furnaces using FTIR microscopy, electron microscopy and NMR spectroscopy. Fuel Process Technol 33(1):13–3210.1016/0378-3820(93)90055-9 ↗
30. Myers RJ, Bernal SA, San Nicolas R, Provis JL (2013) Generalized structural description of calcium-sodium aluminosilicate hydrate gels: the cross-linked substituted tobermorite model. Langmuir 29(17):5294–530610.1021/la4000473 ↗
31. Le Saoût G, Ben Haha M, Winnefeld F, Lothenbach B, Jantzen C (2011) Hydration degree of alkali-activated slags. A 29Si NMR study. J Am Ceram Soc 94(12):4541–454710.1111/j.1551-2916.2011.04828.x ↗
32. Zhang L, Glasser FP (2000) Critical examination of drying damage to cement pastes. Adv Cem Res 12(2):79–8810.1680/adcr.2000.12.2.79 ↗
33. Gruskovnjak A, Lothenbach B, Holzer L, Figi R, Winnefeld F (2006) Hydration of alkali-activated slag: comparison with ordinary Portland cement. Adv Cem Res 18(3):119–12810.1680/adcr.2006.18.3.119 ↗
34. Gruskovnjak A, Lothenbach B, Winnefeld F, Münch B, Figi R, Ko S-C et al (2011) Quantification of hydration phases in supersulfated cements: review and new approaches. Adv Cem Res 23(6):265–27510.1680/adcr.2011.23.6.265 ↗
35. Mu J, Perlmutter DD (1981) Thermal decomposition of carbonates, carboxylates, oxalates, acetates, formates, and hydroxides. Thermochim Acta 49(2–3):207–21810.1016/0040-6031(81)80175-X ↗