journal article·2011-03

Morphologies of oxide growth and exfoliation in superheater and reheater tubing of steam boiler

Ian G. Wright, R. Barry Dooley

Materials at High Temperatures· Volume 28· Issue 1
Publisher page

Abstract

The intent of this paper is to present the current state of knowledge concerning the development of the oxide morphologies associated with scales grown in steam on alloys used in the superheater and reheater circuits of conventional fossil and heat recovery steam generator plants, and the influence of those morphologies on the scale exfoliation behaviour. Scale development is described for three classes of alloy: standard 1 – 9 wt%Cr ferritic steels, using T22 as an example; the ferritic-martensitic steel T91; and the 300-series austenitic steels, represented by TP304 and TP347, for which coarse-and fine-grained versions are examined. Detailed information on oxidation mechanisms is combined with extensive knowledge of alloy behaviour in boiler service in an effort to allow engineers and materials scientists to gain an understanding of similarities and differences, as well as to appreciate the likely contributions of major parameters that influence oxide growth and exfoliation behaviour.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. 10.1179/095066010X1264689872816510.1179/095066010X12646898728165 ↗
2. Wright I.G. · EPRI Rep. No · 2007 · 1013666
3. Dooley, R.B. and Paterson, S.J. (2003) Oxide growth and exfoliation in steam: plant experience. Paper presented at the EPRI-NPL workshop on scale growth and exfoliation in steam plant. National Physical Laboratory, UK, September 3-5,2003.
4. Mayer, P. and Manolescu, A.V. (1983) The role of structural and compositional factors in corrosion of ferritic steels in steam. In: Rapp, R.A. (ed.), High-temperature corrosion, pp. 368-379. Intl. Corrosion Conf. Series NACE-6, NACE, Houston, Texas.
5. 10.3184/096034009X46434810.3184/096034009X464348 ↗
6. Manning M.I. · 1980
7. Sabau A.S. · J Appl. Phys · 2009 · 106
8. 10.1007/s11085-009-9188-410.1007/s11085-009-9188-4 ↗
9. Rehn I.M · 1981
10. The original release of the schematic diagrams of the evolution of oxide morphologies was made in: Dooley, R.B. and Wright, I.G., Oxide growth and exfoliation. Proc. intl. conf on boiler tube and HRSG tube failures and inspections. Baltimore, Maryland, April 19-21, 2010.
11. Nishimura, N., Komai, N., Hirayama, Y. and Masuyama, F. (2003) Japanese experiences with steam oxidation on advanced heat-resistant steel tubes in power boilers. EPR1 workshop on scale growth and exfoliation in steam plant. National Physical Laboratory, UK, September 3-5, 2003.
12. Dooley R.B. · PowerPlant Chem · 2009 · 11 · 132 —151
13. Dooley, R.B. and Anderson, R. (2009) Combined Cycle J. 115-130.
14. Sabau, A.S., Shingledecker, J.P. and Wright, I.G. (2010) Steam-side oxide scale exfoliation behavior in superheaters and reheaters: differences in the behavior of alloys T22, T91, and TP347 based on computer simulation results. Proc. 6th inconf on advances in materials and technology for fossilpower plants. Santa Fe, NM, 9/7-9/10/2010.
15. Armitt J. · 1978
16. Osgerby, S.J. and McCartney, L.N. (2002) Steam oxidation of 9-12Cr martensitic steels: characterisation and modeling the spalling of oxide scale. In: Lecomte-Beckers, J., Carton, M., Schubert, E and Ennis, P.J. (eds.), Materials for advanced power engineering 2002, pp. 1613-1620. Forschungszentrum Jfilich GmbH.
17. Nimura, H., Ohgami, M., Naoi, H. and Fujita, T. (1994) Properties of 9Cr-1.8W steel with high creep strength for USC boiler piping and tubing applications. In: Coutsouradis, D. et al. (eds.), Materials for advanced power engineering, Part I, pp. 361-372. Kluwer Academic Publishers, Dordrecht, Netherlands.10.1007/978-94-011-1048-8_28 ↗
18. ASME boiler and pressure vessel code, Section II part D, 2008.
19. Kutsumi H. · Tetsu-to-Hagane · 2002 · 86 · 42
20. Wright, I.G. (2009) Oxidation of candidate alloys in steam at 17 bar. Final report on phase 1 efforts in support of the US. Consortium Program on Boiler Materials for Ultra-Super-critical Coal Power Plants. ORNL/TM-2009/232, November 2009.
21. Sabau, A.S. and Wright, I.G. (2010) Prediction of oxide scale exfoliation in steam tubes. Proc. boiler tube and HRSG tube failures and inspections international conference. Baltimore, MD, April 2010.
22. Kinoshita K. · NICK Technical Bull · 1974 · TD–49
23. Lucks C.F. · 1951
24. Touloukian, Y.S. et al. (1979) Thermophysical properties of matter (now Thermophysical properties of matter database) https://cindasdata.com
25. Kinoshita K. · Trans. JISI · 1975 · 15 · 334
26. Matsuo H. · 2005
27. Nishiyama, Y, Iseda, A., Yoshizawa, M., Matsumoto, S. and Igarashi, M. (2010) Effect of grain size on steam oxidation for shot-peened stainless steels, paper No. 34. Proc. 6th interna-tional conference on advances in materials and technology for fossil power plants. Santa Fe, NM, 9/7/2010 to 9/10/2010.
28. 10.1016/0010-938X(81)90024-X10.1016/0010-938X(81)90024-X ↗
29. 10.1007/BF0066526710.1007/BF00665267 ↗
30. 10.5006/1.358525110.5006/1.3585251 ↗
31. Montgomery M. · VGB Kraftswerkstechnik · 1995 · 75 · 235
32. Kan, T., Sawaragi, Y, Yamadera, Y. and Okada, H. (1998) Properties and experiences of a new austenitic stainless steel Super304H (0.1C —18Cr— 9Ni— 3Cu—Nb —N) for boiler tube application. In: Lecomte-Beckers, J., Schubert, E and Ennis, P.J. (eds.), Materials for advanced power engineering 1998, pp. 441-450. Forschungszentrum Mich.
33. Montgomery M · 2004 · 461
34. 10.1179/mht.2005.03010.1179/mht.2005.030 ↗