Abstract
High-temperature corrosion has been a critical issue for coal-fired boiler steels, particularly Cr-containing steels SA213-T22, for many decades. Hot combustion gases containing CO2, CO, N2, and unburnt carbon particles play a significant role in the degradation of oxide scale due to reduction reactions. However, carbide precipitation can occur in the oxide layer by carburisation reactions. The effects of reduction and carburisation on the oxide scale of SA213-T22 steel in a simulated combustion atmosphere by carbothermic reduction were investigated and compared with ferritic stainless steels SS430. The two steels were oxidised under an air atmosphere at 750 °C for 48 hours and heated afterwards in graphite powder at 950–1350 °C for 30–60 minutes. After the oxidation test, a thick porous oxide layer of Fe2O3 was found on the SA213-T22 and a thin Fe-Cr-Mn oxide film was found on SS430 as shown by X-ray diffraction analysis. Most oxide scales on SS430 were reduced and destroyed by carbothermic reduction at 1350 °C but the oxide scale on SA213-T22 transformed to compact mixed phases of Fe-C and Fe-C-Cr-O by carburisation and carbon diffusion. The compact oxide layer with heat resistant carbides can increase wear resistance and might withstand corrosive atmospheres in coal-fire boiler plants.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials and Production Technology Engineering, Faculty of Engineering, King Mongkut’s University of Technology North Bangkok, Bangkok, Thailand
High Temperature Corrosion Research Centre, Department of Materials and Production Technology Engineering, Faculty of Engineering, King Mongkut’s University of Technology North Bangkok, Bangkok, Thailand
Funding
King Mongkut’s University of Technology North Bangkok
References (38)
Show source-provided references
1. 10.1016/B978-034069135-9/50017-510.1016/B978-034069135-9/50017-5 ↗
2. 10.1016/B978-0-8155-2041-2.10010-410.1016/B978-0-8155-2041-2.10010-4 ↗
3. 10.3184/096034012X1326974850279210.3184/096034012X13269748502792 ↗
4. 10.1016/j.engfailanal.2020.10440210.1016/j.engfailanal.2020.104402 ↗
5. 10.1108/eb01992010.1108/eb019920 ↗
6. 10.1016/B978-0-08-099998-2.00003-510.1016/B978-0-08-099998-2.00003-5 ↗
7. 10.1016/j.fuproc.2015.01.02810.1016/j.fuproc.2015.01.028 ↗
8. 10.1016/j.coal.2017.05.00710.1016/j.coal.2017.05.007 ↗
9. 10.1016/S1350-6307(01)00040-110.1016/S1350-6307(01)00040-1 ↗
10. 10.1533/9780857093806.2.14510.1533/9780857093806.2.145 ↗
11. 10.1016/j.engfailanal.2014.11.01210.1016/j.engfailanal.2014.11.012 ↗
12. 10.1016/j.conbuildmat.2018.04.15810.1016/j.conbuildmat.2018.04.158 ↗
13. 10.1016/j.resconrec.2019.10442710.1016/j.resconrec.2019.104427 ↗
14. Babich A · 2016
15. Pierson: HO · 1996
16. 10.1533/9781845693787.3.26410.1533/9781845693787.3.264 ↗
17. 10.1016/j.surfcoat.2012.04.03910.1016/j.surfcoat.2012.04.039 ↗
18. 10.4028/www.scientific.net/KEM.856.2110.4028/www.scientific.net/KEM.856.21 ↗
19. Laranjo RD. Thermodynamic analysis in the production of chromium carbide from the reduction of chromium oxide with methane-containing gas. Int. J. Eng. Technol. 2018;4(2):227–232.
20. 10.1016/j.ijrmhm.2010.01.00110.1016/j.ijrmhm.2010.01.001 ↗
21. 10.1002/maco.20050393310.1002/maco.200503933 ↗
22. 10.4236/jmmce.2010.9805310.4236/jmmce.2010.98053 ↗
23. 10.5006/1.328783810.5006/1.3287838 ↗
24. 10.1016/j.ijhydene.2007.12.06710.1016/j.ijhydene.2007.12.067 ↗
25. 10.1007/s11085-013-9432-910.1007/s11085-013-9432-9 ↗
26. 10.1016/j.corsci.2018.11.02310.1016/j.corsci.2018.11.023 ↗
27. Pinder LW, Dawson K, Tatlock GJ, Mahi FT. High temperature corrosion of low alloy steels in reference module. In: materials science and materials engineering. Elsevier; 2017. p. 165.10.1016/B978-0-12-803581-8.10308-X ↗
28. 10.1007/s11663-004-0001-010.1007/s11663-004-0001-0 ↗
29. 10.2355/isijinternational.47.158510.2355/isijinternational.47.1585 ↗
30. 10.2355/isijinternational.42.60910.2355/isijinternational.42.609 ↗
31. 10.1179/000844311X1294929172801410.1179/000844311X12949291728014 ↗
32. 10.1007/s11771-016-3182-110.1007/s11771-016-3182-1 ↗
33. 10.2355/isijinternational.47.138710.2355/isijinternational.47.1387 ↗
34. 10.1088/1757-899X/965/1/01202410.1088/1757-899X/965/1/012024 ↗
35. 10.1007/BF0265194110.1007/BF02651941 ↗
36. 10.1007/s11663-005-0034-z10.1007/s11663-005-0034-z ↗
37. 10.1016/j.corsci.2011.02.02110.1016/j.corsci.2011.02.021 ↗
38. Kubaschewski O · 1979 · 24