journal article·2021-04

Evolution of microstructure, texture and mechanical properties of Fe–30Mn–11Al–1.2C low-density steel during cold rolling

P. Ren, X.P. Chen, C.Y. Wang, Y.X. Zhou, W.Q. Cao, Q. Liu

Publisher page

Abstract

Abstract In the past decades, the microstructure and properties of tensile deformed high Mn–Al–C lightweight steels were extensively studied due to their excellent combination of strength, ductility and low-density. However, the effects of cold rolling were barely reported. This study systematically investigated the evolution of microstructure and texture as well as mechanical properties during cold rolling of Fe–30Mn–11Al–1.2C (wt%) steel. The stacking fault energy (SFE) of the steel was estimated as ~108 mJ/m2. With cold rolling, the yield strength of the steel was significantly enhanced and exceeding 2.0 GPa after 90% rolling reduction, which is attributed to the gradual refinement of the microstructure. Different deformation substructures were formed approximately in the sequence of Taylor lattice, microbands, nano-twins, shear bands and dislocation cells. This means the dislocation glide mode changes from planar to wavy glide with increasing rolling reduction. Among these structures, twining is widely believed to be impossible by tensile deformation due to the high SFE. But it happened during cold rolling with relatively low resolved shear stress, which may be attributed to the occurrence of short range order (SRO) in austenitic matrix and local stress concentration. The rolling texture of the steel was weak and characterized by the transition from “copper-type” to “brass-type” after 50% rolling reduction. The dislocation planar glide and deformation twining play an important role in texture evolution.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. A literature review of age hardening Fe-Mn-Al-C alloys
2. A general perspective of Fe–Mn–Al–C steels10.1007/s10853-018-2551-6 ↗
3. An overview of the effects of alloying elements on the properties of lightweight Fe-(15–35) Mn-(5–12) Al-(0.3–1.2) C steel10.1007/s11837-018-2837-9 ↗
4. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
5. Fe–Al–Mn–C lightweight structural alloys: a review on the microstructures and mechanical properties10.1088/1468-6996/14/1/014205 ↗
6. Deformation mechanisms in ultrahigh-strength and high-ductility nanostructured FeMnAlC alloy10.1016/j.jallcom.2013.10.153 ↗
7. Effect of aging treatment on microstructure and intrinsic mechanical behavior of Fe–31.4Mn–11.4Al–0.89C lightweight steel10.1016/j.jallcom.2015.10.016 ↗
8. On the deformation behavior of κ-carbide-free and κ-carbide-containing high-Mn light-weight steel10.1016/j.actamat.2016.10.006 ↗
9. Strengthening and strain hardening mechanisms in a precipitation-hardened high-Mn lightweight steel10.1016/j.actamat.2017.08.049 ↗
10. Alloy Design, Combinatorial Synthesis, and Microstructure–Property Relations for Low-Density Fe-Mn-Al-C Austenitic Steels10.1007/s11837-014-1032-x ↗
11. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels
12. Microband-induced plasticity in a high Mn–Al–C light steel10.1016/j.msea.2008.05.042 ↗
13. Tensile deformation of low-density Fe–Mn–Al–C austenitic steels at ambient temperature10.1016/j.scriptamat.2012.09.031 ↗
14. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel10.1016/j.actamat.2016.06.037 ↗
15. Effects of Al on microstructure and tensile properties of C-bearing high Mn TWIP steel10.1016/j.actamat.2011.12.004 ↗
16. Control of strain hardening behavior in high-Mn austenitic steels10.1007/s40195-014-0084-9 ↗
17. Factors influencing the tensile behavior of a Fe–28Mn–9Al–0.8C steel10.1016/j.msea.2008.12.055 ↗
18. Origin of extended tensile ductility of a Fe-28Mn-10Al-1C steel10.1007/s11661-009-9862-9 ↗
19. The brass-type texture – How close are we to understand it?10.4028/www.scientific.net/MSF.702-703.216 ↗
20. The brass-type texture and its deviation from the copper-type texture10.1016/j.pmatsci.2008.09.002 ↗
21. Overview No. 76 mechanism of deformation and development of rolling textures in polycrystalline f.c.c. Metals—III. The influence of slip inhomogeneities and twinning10.1016/0001-6160(88)90174-5 ↗
22. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys10.1016/j.msea.2004.01.059 ↗
23. Texture evolution of cold rolled and annealed Fe–24Mn–3Al–2Si–1Ni–0.06C TWIP steel10.1016/j.msea.2011.02.055 ↗
24. Cold rolling behaviour of an austenitic Fe–30Mn–3Al–3Si TWIP-steel: the importance of deformation twinning10.1016/j.actamat.2003.12.040 ↗
25. On the relation of microstructure and texture evolution in an austenitic Fe-28Mn-0.28C TWIP steel during cold rolling10.1007/s11661-012-1543-4 ↗
26. Microstructural analysis in the Fe-30.5Mn-8.0Al-1.2C and Fe-30.5Mn-2.1Al-1.2C steels upon cold rolling
27. Texture evolution in the Fe-30.5Mn-8.0Al-1.2C and Fe-30.5Mn-2.1Al-1.2C steels upon cold rolling
28. Comparative assessment of microstructure and texture in the Fe-30.5Mn-8.0Al-1.2C and Fe-30.5Mn-2.1Al-1.2C steels under cold rolling10.1590/0370-44672017700005 ↗
29. On the origin of planar slip in f.c.c. alloys10.1016/0001-6160(89)90143-0 ↗
30. Direct observation of dislocation plasticity in high-Mn lightweight steel by in-situ TEM10.1038/s41598-019-51586-y ↗
31. Combined strengthening from nanotwins and nanoprecipitates in an iron-based superalloy10.1016/j.actamat.2018.04.001 ↗
32. The conflicts between strength and toughness10.1038/nmat3115 ↗
33. A unique two-stage strength-ductility match in low solid-solution hardening Ni-Cr alloys: decisive role of short range ordering10.1016/j.scriptamat.2019.11.049 ↗
34. Stacking fault energy and plastic deformation of fully austenitic high manganese steels: effect of Al addition10.1016/j.msea.2010.02.058 ↗
35. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
36. Influence of shear banding on the formation of Brass-type textures in polycrystalline fcc metals with low stacking fault energy10.1016/j.jmst.2013.11.010 ↗
37. Impact of short-range clustering on the multistage work-hardening behavior in cu–Ni alloys10.3390/met9020151 ↗
38. A good strength-ductility match in cu-Mn alloys with high stacking fault energies: determinant effect of short range ordering10.1016/j.scriptamat.2017.02.010 ↗
39. Cold rolling texture of Ni-based L12 ordered intermetallic alloys10.2320/matertrans.47.1485 ↗
40. Rolling texture development in cu-Mn-alloys10.4028/www.scientific.net/MSF.157-162.679 ↗