journal article·2018-06

Comparative investigation on microstructures and mechanical properties of (TiB + TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems

Meng Yi, Xiangzhao Zhang, Guiwu Liu, Bo Wang, Haicheng Shao, Guanjun Qiao

Publisher page

Abstract

Abstract Two percentages of TiB + TiC reinforced Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems were fabricated by reactive hot-pressed sintering. Their microstructures and mechanical properties involving elastic modulus, Vickers hardness, bending strength and wear property were investigated comparatively. The experimental results show that needle-like TiB whiskers and near-equiaxed TiC particles are evenly distributed in the Ti-6Al-4V matrix. The mechanical properties of the (TiB + TiC)/Ti-6Al-4V composites are closely related with the nominal composition and synthesis system of TiB + TiC reinforcement and the microstructures of composites. With increasing the nominal volume fraction of reinforcement, both elastic modulus and Vickers hardness increase more or less and the bending strength decreases in varying degrees. A certain increase of pores in the composites with the sintering temperature increasing to 1300 °C can markedly affect the bending strength. Moreover, no matter what the sintering temperature and nominal volume fraction of reinforcement, the elastic modulus and Vickers hardness of composites from the Ti-TiB2-TiC system are higher than those from the Ti-B4C-C system. Similarly, the composites from the Ti-B4C-C system present better abrasion resistance than those from the Ti-TiB2-TiC system due to the difference of interfacial bonding between the TiC particles and Ti-6Al-4V matrix in the two kinds of composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
2. Stability of strengthening effect of in situ formed TiCp and TiBw on the elevated temperature strength of (TiCp+TiBw)/Ti composites10.1016/j.jallcom.2014.06.094 ↗
3. Processing-structure-property aspects of particulate- and whisker-reinforced titanium matrix composites10.1016/j.compscitech.2007.07.016 ↗
4. Microstructure and friction/wear behavior of (TiB + TiC) particulate-reinforced titanium matrix composites10.1016/j.wear.2014.05.013 ↗
5. Influence of (TiC + TiB) on the microstructure and tensile properties of Ti-B20 matrix alloy10.1016/j.jallcom.2014.12.056 ↗
6. In situ Al3Ti-Al2O3 intermetallic matrix composite: synthesis, microstructure, and compressive behavior10.1557/JMR.2000.0280 ↗
7. Effect of TRIPLEX heat treatment on tensile properties of in situ synthesized (TiB+La2O3)/Ti composite10.1016/j.msea.2010.05.065 ↗
8. Effect of microstructure on high temperature properties of in situ synthesized (TiB+La2O3)/Ti composite10.1016/j.matchar.2012.02.010 ↗
9. Growth mechanism of in situ synthesized TiBw in titanium matrix composites prepared by common casting technique10.1016/j.matchar.2007.07.016 ↗
10. In situ preparation of (TiB + TiC + Nd2O3)/Ti composites by powder metallurgy10.1016/j.jallcom.2008.01.124 ↗
11. Correlation of microstructure with high-temperature hardness of (TiC,TiN)/Ti-6Al-4V surface composites fabricated by high-energy electron-beam irradiation10.1016/j.surfcoat.2004.02.040 ↗
12. Effect of C coating on the interfacial microstructure and properties of SiC fiber-reinforced Ti matrix composites10.1016/j.msea.2006.04.029 ↗
13. High-temperature creep behavior of TiC particulate reinforced Ti-6Al-4V alloy composite10.1016/S1359-6454(02)00261-6 ↗
14. Effect of boron addition on microstructure and mechanical properties of TiC/Ti6Al4V composites10.1016/j.matdes.2011.10.040 ↗
15. Processing and mechanical properties of Ti-6Al-4V/TiC in situ composite fabricated by gas-solid reaction10.1016/S0921-5093(01)01858-5 ↗
16. Microstructural and mechanical characterization of a Ti6Al4V/TiC/10p composite processed by the BE-CHIP method10.1016/j.compscitech.2005.03.005 ↗
17. Microstructural characterization and mechanical properties of TiC/near-α Ti composite obtained at slow cooling rate10.1016/j.matchar.2016.06.006 ↗
18. Strengthening effect of in situ TiC particles in Ti matrix composite at temperature range for hot working10.1016/j.matchar.2016.09.010 ↗
19. Evidence for stable stoichiometric Ti2C at the interface in TiC particulate reinforced Ti alloy composites10.1016/S1359-6454(99)00453-X ↗
20. Microstructural characterisation and mechanical properties of spark plasma-sintered TiB2-reinforced titanium matrix composite10.1080/00325899.2016.1265805 ↗
21. TiBw-reinforced Ti composites: processing, properties, application prospects, and research needs10.1007/s11837-004-0127-1 ↗
22. Manufacturing process and mechanical properties of fine TiB dispersed Ti-6Al-4V alloy composites obtained by reaction sintering10.1016/S0921-5093(97)00814-9 ↗
23. Growth mechanism of in situ TiB whiskers in spark plasma sintered TiB/Ti metal matrix composites10.1021/cg050443k ↗
24. Comparative study of microstructures and mechanical properties of in situ Ti-TiB composites produced by selective laser melting, powder metallurgy and casting technologies10.1557/jmr.2014.122 ↗
25. Superior tensile strength and microstructure evolution of TiB whisker reinforced Ti60 composites with network architecture after β extrusion10.1016/j.matchar.2015.03.029 ↗
26. Mechanisms behind the superplastic behavior of as-extruded TiBw/Ti6Al4V composites with a network architecture10.1016/j.matchar.2015.03.036 ↗
27. Strengthening behavior of in situ-synthesized (TiC-TiB)/Ti composites by powder metallurgy and hot extrusion10.1016/j.matdes.2016.01.092 ↗
28. HREM study of TiB/Ti interfaces in a Ti-TiB-TiC in situ composite10.1016/S1359-6462(01)00663-7 ↗
29. Microstructure and mechanical properties of in situ TiB reinforced titanium matrix composites based on Ti-FeMo-B prepared by spark plasma sintering10.1016/j.compscitech.2004.05.013 ↗
30. Evolution of microstructure and phases in in situ processed Ti-TiB composites containing high volume fractions of TiB whiskers10.1557/JMR.1999.0571 ↗
31. Influence factors of ball milling process on BE powder for reaction sintering of TiB/Ti-4.0Fe-7.3Mo composite10.1016/j.jmatprotec.2006.07.014 ↗
32. Mechanical properties of Ti-6Al-4V/TiB composites with randomly oriented and aligned TiB reinforcements10.1016/S1359-6454(02)00510-4 ↗
33. Effect of Ti content and sintering temperature on the microstructures and mechanical properties of TiB reinforced titanium composites synthesized by SPS process10.1016/j.msea.2012.09.064 ↗
34. Role of powder metallurgical processing and TiB reinforcement on mechanical response of Ti-TiB composites10.1016/j.matlet.2014.12.126 ↗
35. Creep behavior of TiBw/Ti in-situ composite fabricated by reactive hot pressing10.1007/s11661-001-0359-4 ↗
36. Preparation of Ti-TiB-TiC & Ti-TiB composites by in-situ reaction hot pressing10.1016/S0921-5093(01)01412-5 ↗
37. Effect of B4C particle size on microstructure of in situ titanium matrix composites prepared by reactive processing of Ti-B4C system10.1016/j.scriptamat.2006.05.024 ↗
38. TEM characterization of symbiosis structure of in situ TiC and TiB prepared by reactive processing of Ti-B4C10.1016/j.matlet.2007.06.033 ↗
39. Dry sliding wear behavior of titanium-(TiB + TiC) in situ composite developed by spark plasma sintering10.1080/10402004.2014.993780 ↗
40. Microstructure and tensile properties of in situ synthesized (TiBw+TiCp)/Ti6242 composites10.1023/A:1017917631855 ↗
41. In situ technique for synthesizing (TiB + TiC)/Ti composites10.1016/S1359-6462(99)00087-1 ↗
42. Microstructure and tensile properties of in situ (TiB + TiC)/Ti6242 (TiB:TiC = 1:1) composites prepared by common casting technique10.1016/S0921-5093(01)00910-8 ↗
43. Effect of volume fraction of reinforcement on room temperature tensile property of in situ (TiB + TiC)/Ti matrix composites10.1016/j.matdes.2004.11.030 ↗
44. Creep rupture life of in situ synthesized (TiB + TiC)/Ti matrix composites10.1016/S1359-6462(01)00926-5 ↗
45. The effect of reinforcements on superplasticity of in situ synthesized (TiB + TiC)/Ti matrix composite10.1016/j.scriptamat.2006.01.044 ↗
46. Effect of (α+β) heat treatment on microstructure and mechanical properties of (TiB + TiC)/Ti-B20 matrix composite10.1016/j.matdes.2015.08.028 ↗
47. High temperature deformation behavior of melt hydrogenated (TiB + TiC)/Ti-6Al-4V composites10.1016/j.matdes.2017.02.075 ↗
48. Spark plasma sintering reaction synthesized TiB reinforced titanium matrix composites10.1016/j.compositesa.2004.09.003 ↗
49. Barin · 1995