journal article·2021-09

Mechanical properties, corrosion behavior and cytotoxicity of Ti-6Al-4V alloy fabricated by laser metal deposition

Xing Zhou, Dake Xu, Shujiang Geng, Yongqiang Fan, Meixia Liu, Qiang Wang, Fuhui Wang

Publisher page

Abstract

Abstract Ti-6Al-4V (TC4) is a widely used biomaterial due to the combination of excellent mechanical properties, corrosion resistance and biological properties. Laser metal deposition (LMD), an efficient and rapid additive manufacturing technology, is very suitable for biomaterial Ti alloy based implants for a customized design. The microstructure evolution and mechanical properties of TC4 samples fabricated by LMD with different scanning approaches were systematically studied in comparison with its wrought counterpart. Large-area mapping (LAM) electron backscatter diffraction (EBSD) results show that the one-way scanning produces finer grains and stronger texture index in the 〈0001〉 direction than those of the cross scanning equivalents. Moreover, the former has higher ultimate tensile strength and plasticity. Electrochemical experiments and in vitro biosafety evaluations were carried out to verify the feasibility of TC4 for long-term services in the body with respect to MC3T3-E1 cells. This work could promote the employment of LMD to build high-quality metal implants for medical applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. The use of titanium for medical applications in the USA10.1016/0921-5093(96)10243-4 ↗
2. Fatigue behavior of Ti-6Al-4V cellular structures fabricated by additive manufacturing technique10.1016/j.jmst.2018.09.066 ↗
3. The effects of crystallographic orientation on fatigue crack initiation behavior in Ti-6Al-4V10.1016/j.ijfatigue.2018.07.039 ↗
4. Microstructure and compression properties of 3D powder printed Ti-6Al-4V scaffolds with designed porosity: experimental and computational analysis10.1016/j.msec.2016.09.040 ↗
5. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation
6. Strain hardening of titanium alloy Ti6Al4V sheets with prior heat treatment and cold working10.1016/j.msea.2016.03.094 ↗
7. A strategy to improve the work-hardening behavior of Ti–6Al–4V parts produced by additive manufacturing10.1080/21663831.2016.1245681 ↗
8. An experimental study of wire EDM on Ti-6Al-4V alloy10.1016/j.mspro.2014.07.517 ↗
9. Additive manufacturing of Ti–6Al–4V parts through laser metal deposition (LMD): process, microstructure, and mechanical properties10.1016/j.jallcom.2019.04.255 ↗
10. Review of in-situ process monitoring and in-situ metrology for metal additive manufacturing10.1016/j.matdes.2016.01.099 ↗
11. A review of 3D printing technology for medical applications10.1016/j.eng.2018.07.021 ↗
12. Effect of scanning strategies on residual stress and mechanical properties of selective laser melted Ti6Al4V10.1016/j.msea.2017.11.103 ↗
13. Effect of laser scanning strategies on texture, physical and mechanical properties of laser sintered maraging steel10.1016/j.msea.2018.07.089 ↗
14. Influence of deposition strategy on the microstructure and fatigue properties of laser metal deposited Ti-6Al-4V powder on Ti-6Al-4V substrate10.1016/j.ijfatigue.2019.105236 ↗
15. Effect of scanning strategy on grain structure and crystallographic texture of Inconel 718 processed by selective laser melting10.1016/j.jmst.2018.02.002 ↗
16. Building direction dependence of corrosion resistance property of Ti–6Al–4V alloy fabricated by Electron beam melting10.1016/j.corsci.2017.08.008 ↗
17. Cytotoxicity study of some Ti alloys used as biomaterial10.1016/j.msec.2008.10.021 ↗
18. Mechanical properties, in vitro corrosion resistance and biocompatibility of metal injection molded Ti-12Mo alloy for dental applications10.1016/j.jmbbm.2018.08.038 ↗
19. Investigation on the properties of borate bonding agents: Ti6Al4V-porcelain bonding, chemical durability and preliminary cytotoxicity10.1016/j.msec.2018.04.078 ↗
20. Effect of scanning strategy on mechanical properties of selective laser melted Inconel 71810.1016/j.msea.2019.03.007 ↗
21. In-vitro study of the bioactivity and cytotoxicity response of Ti surfaces modified by Nb and Mo diffusion treatments10.1016/j.surfcoat.2017.12.009 ↗
22. Image distortions in SEM and their influences on EBSD measurements10.1016/j.ultramic.2006.07.003 ↗
23. Large-field EBSD mapping: application to the microstructure of a friction stir welding nugget10.1007/s00604-003-0148-4 ↗
24. Effective inhibition of nickel release by tantalum-implanted TiNi alloy and its cyto-compatibility evaluation in vitro10.1007/s10853-010-5104-1 ↗
25. Microstructure evolution and EBSD analysis of a graded steel fabricated by laser additive manufacturing10.1016/j.vacuum.2017.03.021 ↗
26. Effects of annealing on the microstructure and mechanical properties of selective laser melted AlSi7Mg alloy10.1016/j.msea.2018.10.047 ↗
27. Influence of surface wettability on competitive protein adsorption and initial attachment of osteoblasts10.1088/1748-6041/4/4/045002 ↗
28. The influence of surface microroughness and hydrophilicity of titanium on the up-regulation of TGFβ/BMP signalling in osteoblasts10.1016/j.biomaterials.2010.09.025 ↗
29. Improvement in antibacterial properties and cytocompatibility of titanium by fluorine and oxygen dual plasma-based surface modification10.1016/j.apsusc.2018.08.194 ↗
30. The influence of heat treatment on the microstructure of products manufactured by direct laser deposition using titanium alloy Ti-6Al-4V
31. Texture and crystal orientation in Ti-6Al-4V builds fabricated by shaped metal deposition10.1007/s11661-010-0255-x ↗
32. Comparative study of fatigue properties of Ti-6Al-4V specimens built by electron beam melting (EBM) and selective laser melting (SLM)10.1016/j.matchar.2018.03.028 ↗
33. Microstructure and phase transformation of Ti-6Al-4V
34. Material properties of Ti6Al4V parts produced by laser metal deposition10.1016/j.phpro.2012.10.056 ↗
35. Additive manufacturing of strong and ductile Ti-6Al-4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
36. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
37. Effect of grain size on Hall-Petch relationship during rolling process of reinforcement bar
38. A high strength low alloy steel fabricated by direct laser deposition10.1016/j.vacuum.2018.12.030 ↗
39. Microbiologically influenced corrosion behavior of S32654 super austenitic stainless steel in the presence of marine Pseudomonas aeruginosa biofilm10.1016/j.jmst.2017.03.002 ↗
40. Effect of Nb addition on the stability and biological corrosion resistance of Ti-Zr alloy passivation films10.1016/j.corsci.2020.108696 ↗
41. Characteristics of oxide films on Ti-(10–75)Ta alloys and their corrosion performance in an aerated Hank’s balanced salt solution10.1016/j.apsusc.2019.145013 ↗
42. Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes10.1016/j.corsci.2016.06.009 ↗
43. Effect of grain size on corrosion of nanocrystalline copper in NaOH solution10.1016/j.corsci.2010.06.029 ↗
44. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
45. Corrosion of ultra-fine grained copper fabricated by equal-channel angular pressing10.1016/j.corsci.2008.01.024 ↗
46. Corrosion behaviour of hot-pressed and die-upset nanocrystalline NdFeB-based magnets10.1016/S0304-8853(02)00286-X ↗
47. Grain size distribution effects on the corrosion behaviour of materials10.1016/j.corsci.2012.04.040 ↗
48. The enhancement of microstructure on the passive and pitting behaviors of selective laser melting 316L SS in simulated body fluid10.1016/j.apsusc.2018.10.150 ↗
49. An investigation on the continuous and uniform thin membrane passive film formed on sputtered nanocrystalline stainless steel10.1016/j.corsci.2015.11.031 ↗
50. Impedance spectroscopy as a technique for studying the spontaneous passivation of metals in electrolytes10.1016/0013-4686(95)00464-5 ↗
51. Effect of vanadium and titanium on the phase composition and corrosion resistance of a high-carbon alloy of the system Fe-C-Mn-Cr10.1007/BF00775037 ↗
52. Impact of the phase composition and structural state on the corrosion and mechanical strength of titanium alloys of the pseudo-β class10.1134/S2075113317040141 ↗
53. Characterization of the outer layer nanostructure in the electrochemical response of stainless steel in aqueous sodium hydroxide10.1080/00032719.2017.1378228 ↗
54. A comparative study of primary and secondary passive films formed on AM355 stainless steel in 0.1M NaOH10.1016/j.apsusc.2017.08.151 ↗
55. Passive film-induced stress and mechanical properties of α-Ti in methanol solution10.1016/j.corsci.2013.10.011 ↗
56. Effect of rolling-induced microstructure on corrosion behaviour of an as-extruded Mg-5Li-1Al alloy sheet10.1016/j.corsci.2017.02.009 ↗
57. Effect of crystallographic texture and microstructure on pitting corrosion behavior of low carbon steels: a Monte Carlo model10.1016/j.commatsci.2019.02.016 ↗
58. Electrochemical and surface analyses of nanostructured Ti–24Nb–4Zr–8Sn alloys in simulated body solution10.1016/j.actbio.2014.02.032 ↗
59. Effect of surface nanocrystallization on the corrosion behavior of Ti–6Al–4V titanium alloy10.1016/j.surfcoat.2013.02.052 ↗
60. Effect of crystal orientation and {101¯2} twins on the corrosion behaviour of AZ31 magnesium alloy10.1016/j.jallcom.2020.154096 ↗
61. Corrosion behavior of electrodeposited Ni with normal and bimodal grain size distribution10.1016/S1003-6326(19)64952-6 ↗
62. Effect of crystal orientation on corrosion behavior of directionally solidified Mg-4 wt%Zn alloy10.1016/j.jmst.2017.06.009 ↗