The effect of major constituents on microstructure and mechanical properties of cast Al-Li-Cu-Zr alloy
Source abstract
Abstract
Abstract The effect of major constituents (the Li content increases from 0.5 to 3 wt% and the Cu content decreases from 4.5 to 2 wt%) on microstructure and mechanical properties of cast Al-Li-Cu-Zr alloy were studied to understand a qualitative assessment of sequence and kinetics of multiple precipitations. Increasing the Li content progressively raises the melting temperature from 520 °C in 1# alloy (Al-0.5Li-4.5Cu, wt%) and 2# alloy (Al-1Li-4.5Cu) to 560 °C in 6# alloy (Al-3Li-2Cu). In addition, the variations of the major constituents result in the changes of the type and volume fraction of the inter- and intra-granular intermetallic phases. TEM results indicate that minor modifications to alloy composition greatly alter precipitation behavior during isothermal aging. The Li-poor alloy (2# alloy) presents a much shorter incubation time of T1-Al2CuLi precipitate than the Li-rich alloy (Al-1.5Li-4.5Cu, 3# alloy), while the nucleation of θ'-Al2Cu precipitate is promoted in Li-rich alloy. No typical spherical δ'-Al3Li precipitate is observed in 2# and 3# alloys during isothermal aging, except for the as-quenched 3# alloy. The preferential nucleation of δ' precipitate on the coherent and broad face of θ' precipitate is observed in 2# and 3# alloys, leading to the formation of “sandwich-like” δ'/θ'/δ' phases. Further decreasing Cu content to 2 wt% and increasing Li content to 3 wt% (6# alloy), the predominant phase in the matrix is δ' precipitate, accompanied by a small amount of unevenly distributed θ' and T1 precipitates. The best balance between ductility and strength is obtained by 2# alloy aged for 32 h, but 6# alloy has significant advantages in terms of density (2.437 g/cm3) and elastic modulus (82.65 GPa) over 2# alloy (density: 2.675 g/cm3; elastic modulus: 75.45 GPa).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Progress in structural materials for aerospace systems10.1016/j.actamat.2003.08.023 ↗
2. Experimental and modelling assessment of precipitation kinetics in an Al–Li–Mg alloy10.1016/j.actamat.2012.01.010 ↗
3. Atomic structure and growth mechanism of T1 precipitate in Al–Cu–Li–Mg–Ag alloy10.1016/j.scriptamat.2015.07.020 ↗
4. Strength, deformation, fracture behaviour and ductility of aluminium-lithium alloys10.1007/BF00585420 ↗
5. Microstructural evolution during ageing of Al–Cu–Li–x alloys10.1016/j.actamat.2013.12.001 ↗
6. Precipitation behavior of the high-Li-content in-situ TiB2/Al-Li-Cu composite10.1016/j.matchar.2017.08.015 ↗
7. Atom probe microscopy investigation of Mg site occupancy within δ’ precipitates in an Al–Mg–Li alloy10.1016/j.scriptamat.2012.02.021 ↗
8. The influence of precipitation on plastic deformation of Al–Cu–Li alloys10.1016/j.actamat.2013.03.015 ↗
9. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al–Li–Cu–X alloy10.1016/S1471-5317(00)00002-X ↗
10. Transmission electron microscopy study of the early stage of precipitates in aged Al–Li–Cu alloys10.1016/S1359-6454(03)00104-6 ↗
11. Transmission electron microscopy study of the evolution of precipitates in aged Al–Li–Cu alloys: the θ’ and T1 phases10.1016/S1359-6454(03)00253-2 ↗
12. Atomic structure of T1 precipitates in Al–Li–Cu alloys revisited with HAADF-STEM imaging and small-angle X-ray scattering10.1016/j.actamat.2010.09.044 ↗
13. Precipitates and intermetallic phases in precipitation hardening Al–Cu–Mg–(Li) based alloys10.1179/174328005X14357 ↗
14. The influence of Cu/Li ratio on precipitation in Al–Cu–Li–x alloys10.1016/j.actamat.2012.12.041 ↗
15. The evolution of Al-Li base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
16. Influence of Mg, Ag and Zn minor solute additions on the precipitation kinetics and strengthening of an Al-Cu-Li alloy10.1016/j.actamat.2017.05.029 ↗
17. Microstructural evolution and mechanical properties of cast high-Li-content TiB2/Al-Li-Cu composite during heat treatment10.1016/j.jallcom.2017.12.126 ↗
18. Heterogeneous Zr solute segregation and Al3Zr dispersoid distributions in Al–Cu–Li alloys10.1016/j.actamat.2015.03.057 ↗
19. Dynamic method of measuring Young's modulus of elasticity10.1088/0950-7671/41/11/302 ↗
20. Atom probe study of early stage phase decomposition in an Al-7.8 at.% Li alloy10.1016/0956-7151(92)90466-R ↗
21. Effects of TiB2 particles on artificial aging response of high-Li-content TiB2/Al-Li-Cu composite10.1016/j.jallcom.2018.03.299 ↗
22. Revisiting the role of peritectics in grain refinement of Al alloys10.1016/j.actamat.2012.09.075 ↗
23. Diffusion coefficients of some solutes in fcc and liquid Al: critical evaluation and correlation10.1016/S0921-5093(03)00624-5 ↗
24. Microstructural characteristics and mechanical properties of cast Al-3Li-xCu-0.2Zr alloy10.1016/j.msea.2016.09.040 ↗
25. The effect of Li content on the natural aging response of Al-Cu-Li-Mg-Ag-Zr alloys10.1016/S1359-6454(96)00360-6 ↗
26. Spinodal decomposition of Al-rich Al-Li alloys10.1016/0001-6160(89)90036-9 ↗
27. “Composite” precipitates in an Al-Li-Zr alloy10.1016/0036-9748(84)90424-1 ↗
28. Solid state phase transformations in aluminium alloys containing lithium10.1179/mst.1987.3.2.81 ↗
29. Interactions between cadmium and multiple precipitates in an Al-Li-Cu alloy: Improving aging kinetics and precipitation hardening10.1016/j.jmst.2019.11.032 ↗
30. Interfacial structure evolution of the growing composite precipitates in Al-Cu-Li alloys10.1016/j.actamat.2017.03.018 ↗
31. The influence of Sc solute partitioning on the microalloying effect and mechanical properties of Al-Cu alloys with minor Sc addition10.1016/j.actamat.2016.08.013 ↗
32. The aging characteristics of an AI-2 Pct Li-3 Pct Cu-0.12 Pct Zr alloy at 190° C10.1007/BF02669814 ↗
33. Effect of stretching on the precipitation kinetics of an Al-2.0 Li-2.8 Cu-0.5 Mg (−0.13 Zr) alloy10.1007/BF02659485 ↗
34. The effect of plastic deformation on Al2CuLi (T1) precipitation10.1007/BF02656799 ↗
35. Experimental, computational and theoretical studies of δ’ phase coarsening in Al–Li alloys10.1016/j.actamat.2012.07.021 ↗