Crack is a serious defect limiting the additive manufacturing of metal materials. The morphologies and crystallographic orientation of cracks for Al-Zn-Mg-Cu alloy prepared by laser powder bed fusion (LPBF) were clarified. The mechanisms of crack initiation and propagation were expounded. Results show that the cracks were crisscrossed horizontally and propagated through multilayers along the building direction in the as-printed specimens. The cracks were classified as solidification cracks, which occurred in the final stage during solidification when the liquid fraction was <20%. Al-Zn-Mg-Cu alloy has a wide temperature range between the liquidus and solidus, leading to high cracking susceptibility. Solidification cracks were prone to initiate at high-angle grain boundaries (HAGBs) and terminate at low-angle grain boundaries (LAGBs) or within grains. LPBF process could affect crack initiation and propagation by refining the grain size and inhibiting the growth orientation. Solidification and thermal shrinkage of adjacent grains during solidification provided subjective factors for cracking initiation. Directional preferential growth of dendrites along the 〈001〉 crystal orientation and the untimely filling of the liquid phase provided secondary factors. This study can provide theoretical guidance for crack suppression in additive manufacturing of 7075 aluminum alloy and other metals with high cracking susceptibility.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Selective laser melting additive manufacturing of 7xxx series Al-Zn-mg-cu alloy: cracking elimination by co-incorporation of Si and TiB2
2. Fast aging strengthening by hybrid precipitates in high pressure die-cast Al-Si-cu-mg-Zn alloy10.1016/j.matchar.2021.111312 ↗
3. Wire arc additive manufacturing of Al-Zn-mg-cu alloy: microstructures and mechanical properties
4. Wire-arc additive manufacturing of a novel high-performance Al-Zn-mg-cu alloy: processing, characterization and feasibility demonstration
5. A novel hierarchical manufacturing method of the selective laser melted Al 7075 alloy
6. Strength and microstructure of laser fusion-welded Ti-SS dissimilar material pair10.1007/s00170-012-4342-6 ↗
7. Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by selective laser melting (SLM)10.1016/j.matchar.2017.06.029 ↗
8. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
9. Material-structure-performance integrated laser-metal additive manufacturing
10. Effects of Cu addition on the precipitation hardening response and intergranular corrosion of Al-5.2Mg-2.0Zn (wt.%) alloy10.1016/j.matchar.2016.11.004 ↗
11. Effects of Cu content on microstructure and properties of super-high-strength Al-9.3Zn-2.4Mg-xCu-Zr alloy10.1016/j.jallcom.2019.02.228 ↗
12. The mechanism of grain refinement and plasticity enhancement by an improved thermomechanical treatment of 7055 Al alloy10.1016/j.msea.2017.06.106 ↗
13. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
14. Change of hot cracking susceptibility in welding of high strength aluminum alloy AA 707510.1016/j.phpro.2016.08.048 ↗
15. Research trends in laser powder bed fusion of Al alloys within the last decade
16. Development of a high strength Al–Zn–Si–mg–cu alloy for selective laser melting10.1016/j.jallcom.2019.06.123 ↗
17. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
18. Microstructure and mechanical properties of A7075 alloy with additional Si objects fabricated by selective laser melting10.2320/matertrans.Y-M2019837 ↗
19. Investigation into the effect of energy density on densification, surface roughness and loss of alloying elements of 7075 aluminium alloy processed by laser powder bed fusion10.1016/j.optlastec.2021.107621 ↗
20. A novel strategy to additively manufacture 7075 aluminium alloy with selective laser melting10.1016/j.msea.2021.141638 ↗
21. Towards understanding metallurgical defect formation of selective laser melted wrought aluminum alloys
22. Microstructure evolution and properties of nanoparticulate SiC modified AlSi10Mg alloys10.1016/j.msea.2021.140864 ↗
23. High power laser powder bed fusion of AlSi10Mg alloy: effect of layer thickness on defect, microstructure and mechanical property10.1016/j.msea.2022.143107 ↗
24. Hot cracking in ZK60 magnesium alloy produced by laser powder bed fusion process10.1016/j.matlet.2021.130283 ↗
25. On the solidification behaviour and cracking origin of a nickel-based superalloy during selective laser melting10.1016/j.matchar.2018.12.032 ↗
26. A generalised hot cracking criterion for nickel-based superalloys additively manufactured by electron beam melting
27. Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling10.1016/j.jallcom.2016.01.250 ↗
28. Atomic-scale grain boundary engineering to overcome hot-cracking in additively-manufactured superalloys10.1016/j.actamat.2019.07.041 ↗
29. Revealing hot tearing mechanism for an additively manufactured high-entropy alloy via selective laser melting10.1016/j.scriptamat.2019.04.036 ↗
30. The effect of layer thickness at selective laser melting10.1016/j.proeng.2017.01.179 ↗
31. Effect of high layer thickness on surface quality and defect behavior of Ti-6Al-4V fabricated by selective laser melting10.1016/j.optlastec.2020.106471 ↗
32. Orientation selection process during the early stage of cubic dendrite growth: a phase-field crystal study10.1016/j.actamat.2012.07.012 ↗
33. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗
34. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
35. Strength and strain hardening of a selective laser melted AlSi10Mg alloy10.1016/j.scriptamat.2017.07.025 ↗
36. Niobium nanoparticle-enabled grain refinement of a crack-free high strength Al-Zn-mg-cu alloy manufactured by selective laser melting10.1016/j.jallcom.2021.163427 ↗
37. A Scheil–Gulliver model dedicated to the solidification of steel10.1016/j.calphad.2015.01.002 ↗
38. Fluidity test of Al-Si alloy using by computer simulation