Microstructural characterization of unidirectional solidified eutectic Al–Si–Ni alloy
Source abstract
Abstract
Abstract Al–11.1wt.%Si–4.2wt.%Ni eutectic alloy was directionally solidified upward at a constant temperature gradient (G = 5.82 K/mm) in a wide range of growth rates (V = 4.60–243.33 μm/s) and a constant growth rate (V = 11.63 μm/s) with different temperature gradients (G = 2.11–5.82 K/mm) by using a Bridgman type directional solidification furnace. The microstructure of directionally solidified Al–11.1wt.%Si–4.2wt.%Ni alloy was observed to be irregular plates of Al3Ni and Si within an α–Al matrix from quenched samples. The values of eutectic spacings (λSi and λAl3Ni) were measured from transverse sections of the samples. The dependency of λSi and λAl3Ni on the values of V and G was found to be λSi = 12.58V− 0.50, λAl3Ni = 7.94V− 0.47, λSi = 5.57G− 0.42 and λAl3Ni = 4.31G− 0.45, respectively by using linear regression analysis. The values of bulk growth were also determined to be λSi2V= 170.52 and λAl3Ni2V= 82.01 μm3/s by using the measured values of λSi, λAl3Ni and V. The values of λSi and λAl3Ni obtained in present work were compared with the values of λSi and λAl3Ni obtained in previous works for Al–Si and Al–Ni eutectic alloys. From the comparison, it can be seen that the values of λSi and λAl3Ni for A1–Si–Ni eutectic alloy are smaller than the values of λSi and λAl3Ni for A1–Si and A–Ni eutectic alloys under similar growth conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Porter · 1992
2. The order–disorder transformation in Ni3Al and Ni3Al -Fe alloys. 1. Determination of the transition-temperatures and their relation to ductility10.1016/0001-6160(87)90273-2 ↗
3. Multiphase solidification in multicomponent alloys10.1016/j.mser.2004.07.002 ↗
4. Coupled two-phase [alpha(Al)+theta(Al2Cu)] planar growth and destabilisation along the univariant eutectic reaction in Al–Cu–Ag alloys10.1016/j.scriptamat.2004.05.040 ↗
5. Experimental study of Bi–Cd–In phase diagram using conventional methods plus quenching and ‘solidification path’ techniques10.1179/026708300101508919 ↗
6. Unconstrained growth along a ternary eutectic solidification path in Al–Cu–Ag: preparation of a MAXUS sounding rocket experiment10.1016/j.msea.2005.08.171 ↗
7. Directional solidification studies in complex ternary alloy systems10.1016/j.jcrysgro.2004.11.268 ↗
8. Jones · Aluminum Alloys · 1978 · 54 · 274
9. Characterisation of intermetallic phases in multicomponent Al–Si casting alloys for engineering applications10.4028/www.scientific.net/MSF.519-521.359 ↗
10. The effect of heat-treatment on aluminum-based piston alloys10.1016/j.matdes.2006.09.010 ↗
11. Nanocrystalline Ni3Al alloy produced by mechanical alloying of nickel aluminides and hot-pressing consolidation10.1016/j.jallcom.2006.08.209 ↗
12. Tensile strength and ductility of Al–MT (MT=Fe, Ni) intermetallic alloys10.1080/10426910701190204 ↗
13. Constituent phase diagrams of the Al–Cu–Fe–Mg–Ni–Si system and their application to the analysis of aluminium piston alloys10.1016/j.actamat.2005.07.003 ↗
14. The dependence of lamellar spacing on growth rate and temperature gradient in the lead–tin eutectic alloy10.1016/S0924-0136(99)00344-1 ↗
15. The effect of growth rate on microstructure and microindentation hardness in the In–Bi–Sn ternary alloy at low melting point10.1016/j.jallcom.2008.02.056 ↗
16. Directional solidification of Al–Cu–Ag alloy10.1007/s00339-009-5130-5 ↗
17. The Al–Ni–Si phase diagram between 0 and 3 3.3at.% Ni10.1016/S0966-9795(02)00184-X ↗
18. Aluminum–Nickel–Silicon Ternary Alloy Phase Diagram
19. Jackson · 1958 · 174
20. Interflake spacings and undercoolings in Al–Si irregular eutectic alloy10.1016/j.msea.2003.11.020 ↗
21. Unidirectional solidification of aluminium–nickel eutectic alloy10.4149/km_2010_5_291 ↗
22. Lamellar and eutectic growth
23. Microstructure and mechanical properties of unidirectionally solidified Al–Si–Ni ternary eutectic10.1007/BF02658416 ↗
24. Eutectic spacing selection in Al–Cu system10.1179/mst.1994.10.4.312 ↗
25. The microstructure parameters and microhardness of directionally solidified Sn–Ag–Cu eutectic alloy10.1016/j.jallcom.2009.06.067 ↗
26. In situ observation of microstructure evolution in low-melting Bi–In–Sn alloys by light microscopy10.1016/j.actamat.2005.04.015 ↗
27. Effect of solidification parameters on the microstructure of Sn–3.7Ag–0.9Zn solder10.1016/j.matchar.2010.08.007 ↗
28. Dependency of microstructural parameters and microindentation hardness on the temperature gradient in the In–Bi–Sn ternary alloy with a low melting point10.3365/met.mat.2008.10.575 ↗
29. Dependency of eutectic spacings and microhardness on the temperature gradient for directionally solidified Sn–Ag–Cu lead free solder10.1016/j.matchemphys.2009.09.022 ↗
30. Phase separation and undercooling in Al–Si eutectic alloy—the influence of freezing rate and temperature gradient10.1016/0001-6160(76)90102-4 ↗