The microstructure and formation mechanism of face-centered cubic Ti in commercial pure Ti foils during tensile deformation at room temperature
Source abstract
Abstract
Abstract Two variants of face-centered cubic (fcc) Ti phase appear in ultra-thin commercial pure Ti foils with hexagonal closed packed (hcp) structure during tensile deformation at room temperature. The orientation relationship between fcc-Ti phase and hcp-Ti matrix is determined as 〈0001〉HCP // 〈001〉FCC, 〈11 2 ¯ 0 〉HCP // 〈1 1 ¯ 0 〉FCC and 〈01 1 ¯ 0〉HCP // 〈110〉 FCC. The fcc-Ti phase with a habit plane of {01 1 ¯ 0}HCP usually nucleates at grain boundary and grows along the direction of 〈11 2 ¯ 0 〉HCP. The thickness of fcc-Ti phase with a shape of thin plate ranges from 10 nm to 200 nm. Dislocations, steps and stacking faults with a space of 0.58 nm can be seen in fcc-Ti. The formation of a five-layer fcc-Ti can be accomplished by the formation of stacking faults and gliding of 1/6[11 2 ¯ 0 ] Shockley partial dislocations on the prismatic plane of hcp-Ti. The 1/3[11 2 ¯ 0 ] dislocations in hcp-matrix can cross the fcc-Ti phase because the Burgers vector of these dislocations is coincidence with 1/2[110] dislocations in the fcc-Ti.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Microstructure and mechanical properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Characterization and analysis of deformation heterogeneities in commercial purity titanium10.1016/j.matchar.2015.09.001 ↗
2. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
3. Dynamic mechanical behavior of pure titanium10.1016/j.jmatprotec.2004.04.327 ↗
4. Mechanical properties and deformation mechanisms of a commercially pure titanium10.1016/S1359-6454(99)00203-7 ↗
5. Stress-induced hexagonal close-packed to face-centered cubic phase transformation in commercial-purity titanium under cryogenic plane-strain compression10.1016/j.scriptamat.2013.05.038 ↗
6. Study of interface and base metal microstructures in explosive clad joint of Ti-5Ta-1.8Nb and 304L stainless steel10.1179/1362171810Y.0000000001 ↗
7. Saroja, formation and reversion of metastable fcc phase in a Ti–5Ta–2Nb explosive clad10.1016/j.matchar.2016.03.022 ↗
8. The formation of f.c.c. titanium in titanium-aluminum multilayers10.1016/1359-6454(95)00159-5 ↗
9. Formation of face-centered-cubic titanium by mechanical attrition10.1063/1.1530718 ↗
10. Microstructural evolution and formation mechanism of FCC titanium during heat treatment processing10.1016/j.jallcom.2012.10.083 ↗
11. Phase transformation behavior in titanium single-crystal nanopillars under [0001] orientation tension: a molecular dynamics simulation10.1016/j.commatsci.2014.05.018 ↗
12. Rolling-induced face centered cubic titanium in hexagonal close packed titanium at room temperature10.1038/srep24370 ↗
13. Effect of twinning on microstructure and texture evolutions of pure Ti during dynamic plastic deformation10.1016/j.msea.2012.11.097 ↗
14. In situ TEM observation of FCC Ti formation at elevated temperatures10.1016/j.scriptamat.2017.06.033 ↗
15. A comparative study on the microstructure and mechanical behavior of titanium: ultrafine grain vs. coarse grain10.1016/j.msea.2016.05.093 ↗
16. Ultrafine-grained pure Ti recycled by equal channel angular pressing with high strength and good ductility10.1016/j.jmatprotec.2012.10.016 ↗
17. Effects of strain rates on deformation twinning behavior in α-titanium10.1016/j.matchar.2015.05.016 ↗
18. Effect of deformation twinning on microstructure and texture evolution during cold rolling of CP-titanium10.1016/j.msea.2005.03.019 ↗
19. Analysis of twinning behavior of pure Ti compressed at different strain rates by Schmid factor10.1016/j.msea.2013.03.031 ↗
20. Jenkins · 1996
21. Thickness-dependent fcc-hcp phase transformation in polycrystalline titanium thin films10.1016/j.actamat.2010.12.046 ↗
22. Size-dependent deformation mechanism transition in titanium nanowires under high strain rate tension10.1016/j.matdes.2017.08.058 ↗