Selective laser melting of Ti6Al4V alloy: Effect of post-processing on fatigue life, residual stress, microstructure, microhardness and surface roughness
Source abstract
Abstract
In this study; turning, milling, heat treatment and shot peening (SP) post-process operations alone or in different combinations were performed on Ti6Al4V specimens which were produced by selective laser melting (SLM); then the effects of these operations on the fatigue life, residual stress, microstructure, microhardness and surface roughness were investigated. SP processes were carried out in two different types, traditional and multiple, and it was observed that the multiple SP process, which was carried out with the same almen intensity as traditional, with a smaller ball diameter, was effective in reducing the surface roughness. As a result of the heat treatment, α + β transformation was observed in the microstructure. α phase was seen in both lamellar and globular forms. Traditional SP and multiple SP processes provided a significant increase in microhardness values in the 0–250 μm depth range. A significant decrease in the microhardness values of the heat-treated specimens was observed due to the α + β transformation in the microstructure. Traditional SP and multiple SP processes enabled the residual stress type to become compressive type in both the x-axis and the y-axis in the 0–150 μm depth which is a very critical region for fatigue cracks despite the x-axis direction surface unmachined. Fatigue test were performed on machined, multiple shot-peened and machined after heat-treated specimens. The best results in terms of fatigue strength were obtained in the specimens that were heat-treated. It was observed that the most important cause of fatigue crack initiation in multiple shot-peened specimens was an internal defect located deeper than 250 μm. Fisheye formation was observed on fracture surfaces of some multiple shot-peened fatigue specimens.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Surface Treatment and Residual Stress · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (81)
Show source-provided references
1. Donachie · 2000
2. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
3. An investigation of ductile fracture behavior of Ti6Al4V alloy fabricated by selective laser melting10.1016/j.jallcom.2021.161926 ↗
4. Microstructure and anisotropic mechanical properties of selective laser melted Ti6Al4V alloy under different scanning strategies10.1016/j.msea.2021.142236 ↗
5. Microstructure and property evaluation of TA15 titanium alloy fabricated by selective laser melting after heat treatment10.1016/j.optlastec.2021.107422 ↗
6. Additive manufactured Ti-6A1-4V using welding wire: comparison of laser and arc beam deposition and evaluation with respect to aerospace material specifications10.1016/j.phpro.2010.08.087 ↗
7. Wire based additive layer manufacturing: comparison of microstructure and mechanical properties of Ti-6Al-4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
8. Abe, residual stress within metallic model made by selective laser melting process10.1016/S0007-8506(07)60677-5 ↗
9. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: atigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
10. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
11. Lutjering · 2003
12. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
13. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
14. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
15. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
16. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
17. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
18. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
19. The effect of SLM process parameters on density, hardness, tensile strength and surface quality of Ti-6Al-4V
20. The effect of post-sintering treatments on the fatigue and biological behavior of Ti-6Al-4V ELI parts made by selective laser melting10.1016/j.jmbbm.2017.03.024 ↗
21. Effect of ultrasonic shot peening on microstructure evolution and corrosion resistance of selective laser melted Ti-6Al-4V alloy10.1016/j.jmrt.2021.01.091 ↗
22. Characterization on surface properties of Ti-6Al-4V after multiple shot peening treatments10.1115/1.4033577 ↗
23. 2020
24. ISO 26910-1:2009 · 2009
25. ASTM E384-17 · 2019
26. The anisotropy of high cycle fatigue property and fatigue crack growth behavior of Ti–6Al–4V alloy fabricated by high-power laser metal deposition10.1016/j.msea.2022.143745 ↗
27. Anisotropy in the impact toughness of selective laser melted Ti-6Al-4V alloy10.1016/j.msea.2015.10.045 ↗
28. Roughness of shot-peened surfaces - definition and measurement
29. A three-dimensional measure of surface roughness based on mathematical morphology10.1016/j.ijmachtools.2005.12.003 ↗
30. Numerical and experimental analysis of surface roughness generated by shot peening10.1016/j.apsusc.2012.03.111 ↗
31. JIS B 0601 · 2001
32. JIS B 0031 · 2003
33. Predictions of decreased surface roughness after shot peening using controlled media dimensions10.1016/j.jmst.2020.03.075 ↗
34. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti–6Al–4V and TiB/Ti–6Al–4V composite: A comparative study10.1016/j.msea.2020.140415 ↗
35. Effect of heat treatment on the phase transformation and mechanical properties of Ti6Al4V fabricated by selective laser melting10.1016/j.jallcom.2018.06.076 ↗
36. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
37. The kinetics of phase transformations during continuous cooling of the Ti6Al4V alloy from the single-phase β range10.2478/v10172-011-0077-x ↗
38. Finite element modeling of the morphology of β to α phase transformation in Ti-6Al-4V alloy10.1007/s11661-002-0204-4 ↗
39. Use of high temperature X-ray diffractometry to study phase transitions and thermal expansion properties in Ti-6Al-4V10.1179/026708303225008013 ↗
40. The kinetics of static globularization of Ti-6Al-4V10.1007/s11661-002-0340-x ↗
41. Surface severe plastic deformation of AISI 304 via conventional shot peening, severe shot peening and repeening10.1016/j.apsusc.2015.05.093 ↗
42. Effect of shot peening on the oxidation behavior of thermal barrier coatings10.1016/j.apsusc.2015.06.113 ↗
43. Surface nanocrystallization of 316L stainless steel induced by ultrasonic shot peening10.1016/S0921-5093(00)00686-9 ↗
44. Effects of laser shock processing on mechanical properties and micro-structure of ANSI 304 austenitic stainless steel10.1016/j.msea.2011.03.041 ↗
45. Almen intensity effect on microstructure and mechanical properties of low carbon steel subjected to severe shot peening10.1016/j.apsusc.2013.10.184 ↗
46. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
47. The cleavage strength of polycrystals
48. Laser peening process and its impact on materials properties in comparison with shot peening and ultrasonic impact peening10.3390/ma7127925 ↗
49. Fretting wear behavior of fine grain structured aluminium alloy formed by oil jet peening process under dry sliding condition10.1016/j.wear.2012.07.026 ↗
50. Microstructural evolution and microhardness of a selective-laser-melted Ti-6Al-4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
51. Evaluation of heat treatment parameters on microstructure and hardness properties of high-speed selective laser melted Ti6Al4V10.3390/met11020255 ↗
52. The heat treatment influence on the microstructure and hardness of TC4 titanium alloy manufactured via selective laser melting
53. An assessment of subsurface residual stress analysis in SLM Ti-6Al-4V10.3390/ma10040348 ↗
54. Study of residual stress in selective laser melting of Ti6Al4V10.1016/j.matdes.2020.108846 ↗
55. A study of the relationship between thermal expansion and residual stresses in selective laser melting of Ti-6Al-4V10.1016/j.jmapro.2020.01.039 ↗
56. Effect of rescanning cycles on the characteristics of selective laser melting of Ti6Al4V10.1016/j.optlastec.2019.105890 ↗
57. An Experimental Investigation into Additive Manufacturing-Induced Residual Stresses in 316L Stainless Steel10.1007/s11661-014-2549-x ↗
58. On the simulation scalability of predicting residual stress and distortion in selective laser melting10.1115/1.4038893 ↗
59. Effect of machining parameters and heat treatment on the residual stress distribution in titanium alloy IMI-83410.1016/S0924-0136(03)00612-5 ↗
60. Surface integrity of selective-laser-melted components10.1016/j.cirp.2010.03.131 ↗
61. Machining distortion of titanium alloys aero engine case based on the energy principles
62. The effect of machining on the surface integrity and fatigue life10.1016/j.ijfatigue.2008.01.005 ↗
63. Analysis of machining-induced residual stresses of milled aluminum workpieces, their repeatability, and their resulting distortion10.1007/s00170-021-07171-7 ↗
64. Effect of machining-induced residual stress on the distortion of thin-walled parts10.1007/s00170-014-6281-x ↗
65. Methods of measuring residual stresses in components10.1016/j.matdes.2011.08.022 ↗
66. Review of shot peening processes to obtain nanocrystalline surfaces in metal alloys10.1179/026708408X334087 ↗
67. Murakami · 2002
68. Microstructural analysis of selective laser melted Ti6Al4V modified by laser peening and shot peening for enhanced fatigue characteristics10.1016/j.matchar.2021.110935 ↗
69. Microstructural characterisation of metallic shot peened and laser shock peened Ti–6Al–4V10.1016/j.actamat.2016.10.044 ↗
70. Numerical analysis and experimental validation on residual stress distribution of titanium matrix composite after shot peening treatment10.1016/j.mechmat.2016.05.005 ↗
71. Post-processing of the Inconel 718 alloy parts fabricated by selective laser melting: effects of mechanical surface treatments on surface topography, porosity, hardness and residual stress10.1016/j.surfcoat.2019.125136 ↗
72. Enhanced fatigue behavior of powder metallurgy Ti-6Al-4V alloy by applying ultrasonic impact treatment10.1016/j.msea.2015.06.072 ↗
73. Four-dimensional annihilation behaviors of micro pores during surface cold working10.2320/matertrans.M2010069 ↗
74. Microstructure and mechanical properties of laser shock peened 38CrSi steel10.1016/j.msea.2020.139486 ↗
75. Microstructural evolution, mechanical behaviors and strengthening mechanism of 300 M steel subjected to multi-pass laser shock peening10.1016/j.optlastec.2021.107726 ↗
76. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
77. Selective laser melting of Ti6Al4V alloy: Process parameters, defects and post-treatments10.1016/j.jmapro.2021.01.009 ↗
78. Fatigue performances of selective laser melted Ti-6Al-4V alloy: influence of surface finishing, hot isostatic pressing and heat treatments10.1016/j.ijfatigue.2018.11.019 ↗
79. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
80. XCT analysis of the influence of melt strategies on defect population in Ti-6Al-4V components manufactured by Selective Electron Beam Melting10.1016/j.matchar.2015.02.008 ↗
81. Very high cycle fatigue of high-strength steels: Crack initiation by FGA formation investigated at artificial defects10.1016/j.prostr.2016.06.141 ↗