journal article·2022-12

Effect of direct aging treatment on microstructure, mechanical and corrosion properties of a Si-Zr-Er modified Al-Zn-Mg-Cu alloy prepared by selective laser melting technology

Zhiqian Zhang, Dehua Li, Shengci Li, Hongling Deng, Siyu Zhang, Jin Fang, Hao Yuan, Bo Deng, Liang Qi

Publisher page

Abstract

In this paper, a novel Al-Zn-Mg-Cu alloy with Si-Zr-Er addition was prepared by selective laser melting (SLM) technology. Effects of aging temperature and aging time on the microstructure, mechanical properties and corrosion resistance of the alloy were systematically studied. Results show that unique bimodal grain structure is formed in the as-printed and direct aging treated alloys, which is composed of fine equiaxed grains at the molten pool boundary and coarse columnar grains in the molten pool. Mechanical properties of the alloy can be improved by direct aging treatment, and the highest tensile strength reached 465 MPa. The precipitated Mg 2Si and Al 3(Er,Zr) with L1 2 structure play an important role in improving the mechanical properties. The precipitates and fraction of high-angle grain boundaries are important to evaluate the corrosion resistance of the investigated alloy. Considering the mechanical properties and corrosion resistance, the optimal aging process of the alloy studied in this paper is 150 °C × 4 h.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Investigation on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys with various Zn/Mg ratios [J]10.1016/j.jmst.2020.12.045 ↗
2. Effects of critical defects on stress corrosion cracking of Al–Zn–Mg–Cu–Zr alloy [J]10.1016/j.jmrt.2021.03.070 ↗
3. Ultra-high strength Al-Zn-Mg-Cu alloys with high zinc content prepared via powder hot extrusion [J]10.1016/j.micron.2021.103015 ↗
4. Discovery of aluminum alloys with ultra-strength and high-toughness via a property-oriented design strategy [J]10.1016/j.jmst.2021.05.011 ↗
5. A review of selective laser melting of aluminum alloys: processing, microstructure, property and developing trends [J]10.1016/j.jmst.2018.09.004 ↗
6. Selective laser melting of a novel Sc and Zr modified Al-6.2Mg alloy: processing, microstructure, and properties [J]10.1016/j.powtec.2017.06.050 ↗
7. Additive manufacturing of metals [J]10.1016/j.actamat.2016.07.019 ↗
8. Effect of temperature on the microstructure and tensile properties of micro-crack free hastelloy X produced by selective laser melting [J]
9. Additive manufacturing of metallic components–process, structure and properties [J]10.1016/j.pmatsci.2017.10.001 ↗
10. Early-stage precipitation in Al–Zn–Mg–Cu alloy (7050) [J]10.1016/j.actamat.2004.06.025 ↗
11. Additive manufacturing: scientific and technological challenges, market uptake and opportunities [J]10.1016/j.mattod.2017.07.001 ↗
12. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties [J]10.1016/j.pmatsci.2015.03.002 ↗
13. Influence of process parameters on the quality of aluminium alloy EN AW 7075 using selective laser melting (SLM) [J]10.1016/j.phpro.2016.08.096 ↗
14. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy [J]10.1016/j.scriptamat.2017.02.036 ↗
15. Microstructures and tensile properties of a selective laser melted Al–Zn–Mg–Cu (Al7075) alloy by Si and Zr microalloying [J]10.1016/j.msea.2020.139492 ↗
16. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2 [J]
17. SLM-processed Sc- and Zr- modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment [J]10.1016/j.msea.2017.06.089 ↗
18. Effect of Er and Zr additions and aging treatment on grain refinement of aluminum alloy fabricated by laser powder bed fusion [J]10.1016/j.jallcom.2022.165237 ↗
19. Effect of aging treatment on the microstructure and mechanical properties of Al-3.02Mg-0.2Sc-0.1Zr alloy printed by selective laser melting [J]10.1016/j.matdes.2019.107668 ↗
20. On the corrosion of a high solute Al-Zn-Mg alloy produced by laser powder bed fusion [J]10.1016/j.corsci.2021.109626 ↗
21. Microstructure and corrosion evolution of additively manufactured aluminium alloy AA7075 as a function of ageing [J]
22. Influence of scanning strategy and parameter on microstructural feature, residual stress and performance of Sc and Zr modified Al–Mg alloy produced by selective laser melting [J]10.1016/j.msea.2020.139593 ↗
23. Effect of heat treatment on microstructure, hardness and corrosion resistance of 7075 Al alloys fabricated by SLM [J]10.1016/j.jmapro.2020.10.071 ↗
24. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms [J]10.1016/j.actamat.2020.03.060 ↗
25. Laser-based directed energy deposition of novel Sc/Zr-modified Al-Mg alloys: columnar-to-equiaxed transition and aging hardening behavior [J]10.1016/j.jmst.2020.08.003 ↗
26. Thermal behavior during selective laser melting of commercially pure titanium powder: numerical simulation and experimental study [J]
27. Comparative study of performance comparison of AlSi10Mg alloy prepared by selective laser melting and casting [J]10.1016/j.jmst.2019.08.049 ↗
28. An additively manufactured Al-14.1Mg-0.47Si-0.31Sc-0.17Zr alloy with high specific strength, good thermal stability and excellent corrosion resistance [J]10.1016/j.jmst.2020.06.036 ↗
29. Densification, microstructure and mechanical properties of an Al-14.1Mg-0.47Si-0.31Sc-0.17Zr alloy printed by selective laser melting [J]10.1016/j.msea.2020.138931 ↗
30. Superior mechanical properties of a selective-laser-melted AlZnMgCuScZr alloy enabled by a tunable hierarchical microstructure and dual-nanoprecipitation [J]10.1016/j.mattod.2021.11.019 ↗
31. A solution to the hot cracking problem for aluminium alloys manufactured by laser beam melting [J]10.1016/j.actamat.2020.07.015 ↗
32. Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting [J]10.1016/j.actamat.2018.04.053 ↗
33. Effects of the addition of silicon to 7075 aluminum alloy on microstructure, mechanical properties, and selective laser melting processability [J]10.1016/j.msea.2020.139079 ↗
34. Role of Er on the densification, microstructure and mechanical properties of 7075 aluminium alloys manufactured by laser powder bed fusion [J]10.1016/j.jmrt.2022.08.004 ↗
35. 3D printing of high-strength aluminium alloys [J]10.1038/nature23894 ↗
36. Precipitation of Al3(Sc,Zr) particles in an Al-Zn-Mg-Cu-Sc-Zr alloy during conventional solution heat treatment and its effect on tensile properties [J]10.1016/j.actamat.2008.04.005 ↗
37. Effects of heat treatment on the microstructure, residual stress, and mechanical properties of Co–Cr alloy fabricated by selective laser melting [J]10.1016/j.jmbbm.2021.105051 ↗
38. Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM) [J]10.1016/j.msea.2020.139533 ↗
39. Effect of Zr content on the precipitation and dynamic softening behavior in Al–Fe–Zr alloys [J]10.1016/j.matchar.2020.110181 ↗
40. Laws for work-hardening and low-temperature creep [J]10.1115/1.3443340 ↗
41. Effects of direct aging treatment on microstructure, mechanical properties and residual stress of selective laser melted AlSi10Mg alloy [J]10.1016/j.jmst.2022.08.032 ↗
42. Grain-boundary diffusion coefficient in α-Al2O3 from spark plasma sintering tests: evidence of collective motion of charge disconnections [J]10.1016/j.ceramint.2018.07.073 ↗
43. Effect of aging treatment on microstructures, tensile properties and intergranular corrosion behavior of Al–Cu–Li alloy [J]10.1016/j.matchar.2018.04.043 ↗
44. Corrosion behaviors of selective laser melted aluminum alloys: a review [J]10.3390/met10010102 ↗
45. Effects of retrogression and re-aging treatment on precipitation behavior, mechanical and corrosion properties of a Zr+Er modified Al-Zn-Mg-Cu alloy [J]10.1016/j.matchar.2021.111617 ↗
46. Optimization of heat treatment for an Al–Mg–Sc–Mn–Zr alloy with ultrafine grains manufactured by laser powder bed fusion [J]10.1016/j.matchar.2022.111977 ↗
47. Influence of heat treatment on corrosion behavior of rare earth element Sc modified Al-Mg alloy processed by selective laser melting [J]10.1016/j.apsusc.2020.145330 ↗