Single and multiple track formation mechanism of laser powder bed fusion 316L/CuSn10 multi-material
Source abstract
Abstract
This paper focuses on the influence mechanism of process parameters on the geometry morphology and microstructure characteristic of single-track and multi-track 316L/CuSn10 multiple materials manufactured by laser powder bed fusion (LPBF). The width of single-track increases with the increase of laser power and layer thickness, and decreases with the increase of scanning speed. Both variations in the copper content and wetting angle of the molten pool were investigated. In addition, the comparison of defect characteristics shows that the scanning speed and layer thickness have a greater influence on the formation of single cracks. The traces of Marangoni convection are observed directly in the centre of the molten pool due to the difference in microstructure between 316L and CuSn10 alloys. It is found that the copper penetration cracks appear on the steel side at the molten pool bottom. Moreover, fine grains appear in the copper-rich region, and the large-angle grain boundary distribution seems to be the reason for the concentration of dislocations. Four types of crack formation mechanisms are found in the cross section of the multi-track: crack formation inside the molten pool, passing through the track boundary, extending to the steel substrate, and copper penetration cracks.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Recent developments in metal additive manufacturing10.1016/j.coche.2020.03.001 ↗
2. The metallurgy and processing science of metal additive manufacturing10.1080/09506608.2015.1116649 ↗
3. Additive manufacturing of metallic components–process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
4. Scientific, technological and economic issues in metal printing and their solutions10.1038/s41563-019-0408-2 ↗
5. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
6. Remanufacturing of turbine blades by laser direct deposition with its energy and environmental impact analysis10.1016/j.jclepro.2014.05.084 ↗
7. Clinical, industrial, and research perspectives on powder bed fusion additively manufactured metal implants
8. Microstructural evolution, nanoprecipitation behavior and mechanical properties of selective laser melted high-performance grade 300 maraging steel10.1016/j.matdes.2017.08.026 ↗
9. Additive manufacturing of Inconel 718—copper alloy bimetallic structure using laser engineered net shaping (LENSTM)
10. Multi-material selective laser melting of Fe/Al-12Si components10.1016/j.mfglet.2017.01.002 ↗
11. 3D printing of multiple metallic materials via modified selective laser melting10.1016/j.cirp.2018.04.096 ↗
12. New approach to multi-material processing in selective laser melting10.1016/j.phpro.2016.08.093 ↗
13. Additive manufacturing of a steel–ceramic multi-material by selective laser melting10.1007/s11663-019-01523-1 ↗
14. Interfacial characterization and mechanical properties of 316L stainless steel/inconel 718 manufactured by selective laser melting10.1016/j.msea.2019.05.011 ↗
15. Hybrid additive manufacturing of Al-Ti6Al4V functionally graded materials with selective laser melting and cold spraying10.1016/j.jmatprotec.2018.01.015 ↗
16. Opportunities and challenges in additive manufacturing of functionally graded metallic materials via powder-fed laser directed energy deposition: a review
17. Machining of functionally graded Ti6Al4V/WC produced by directed energy deposition
18. Gradient transition zone structure in “steel–copper” sample produced by double wire-feed electron beam additive manufacturing
19. Stainless steel to titanium bimetallic structure using LENS™
20. Multiscale study of different types of interface of a buffer material in powder-based directed energy deposition: example of Ti6Al4V/Ti6Al4V-Mo/Mo-Inconel 718
21. Processing optimisation, mechanical properties and microstructural evolution during selective laser melting of Cu-15Sn high-tin bronze10.1016/j.msea.2018.02.051 ↗
22. Mechanical behavior of selective laser melted 316L stainless steel10.1016/j.msea.2017.04.058 ↗
23. Towards bi-metallic injection molds by directed energy deposition10.1016/j.mfglet.2021.01.001 ↗
24. Copper/stainless steel conductor for high field pulsed magnets10.1016/0921-4526(95)00478-5 ↗
25. Cu-Nb and Cu/stainless steel winding materials for high field pulsed magnets10.1109/77.828465 ↗
26. Influence of the feed rate and the lateral beam displacement on the joining quality of laser-welded copper-stainless steel connections10.1016/j.phpro.2010.08.029 ↗
27. Additive manufacturing of copper-stainless steel hybrid components using laser-aided directed energy deposition10.1016/j.jmst.2020.11.048 ↗
28. Additive manufacturing of steel–copper functionally graded material with ultrahigh bonding strength10.1016/j.jmst.2020.07.044 ↗
29. Dual interfacial characterization and property in multi-material selective laser melting of 316L stainless steel and C52400 copper alloy10.1016/j.matchar.2020.110489 ↗
30. Interfacial characteristic and mechanical performance of maraging steel-copper functional bimetal produced by selective laser melting based hybrid manufacture10.1016/j.matdes.2018.05.064 ↗
31. Interfacial microstructure and mechanical properties of 316L/CuSn10 multi-material bimetallic structure fabricated by selective laser melting10.1016/j.msea.2019.02.097 ↗
32. Interfacial characterization of SLM parts in multi-material processing: metallurgical diffusion between 316L stainless steel and C18400 copper alloy10.1016/j.matchar.2014.05.001 ↗
33. Additive manufacturing of horizontal and 3D functionally graded 316L/Cu10Sn components via multiple material selective laser melting10.1115/1.4043983 ↗
34. On the formation of AlSi10Mg single tracks and layers in selective laser melting: microstructure and nano-mechanical properties10.1016/j.jmatprotec.2015.11.016 ↗
35. Formation mechanisms of TiB2 tracks on Ti6Al4V alloy during selective laser melting of ceramic-metal multi-material10.1016/j.powtec.2020.04.027 ↗
36. Preparation method and underlying mechanism of MWCNTs/Ti6Al4V nanocomposite powder for selective laser melting additive manufacturing10.1016/j.powtec.2020.04.041 ↗
37. Quantitative characterization of porosity in laser welds of stainless steel10.1016/j.scriptamat.2012.06.015 ↗
38. III. An essay on the cohesion of fluids
39. Observation of keyhole-mode laser melting in laser powder-bed fusion additive manufacturing10.1016/j.jmatprotec.2014.06.005 ↗
40. Intergranular attack of steel by molten copper
41. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
42. Parametric analysis of the selective laser melting process10.1016/j.apsusc.2007.02.088 ↗
43. Direct laser sintering of metal powders: mechanism, kinetics and microstructural features10.1016/j.msea.2006.04.117 ↗