Heat treatment of Al-Cu-Li-Sc-Zr alloy produced by laser powder bed fusion
Source abstract
Abstract
Developing effective heat treatments to enhance the property of LPBF-produced aluminum alloys has received strong attention in recent years. In this paper, we present a systematic study on the effect of heat treatment on the LPBF-fabricated Al-Cu-Li-Sc-Zr alloy. The heat treatment temperatures were designed according to the phase transformation and precipitation kinetic analyses. Based on precipitation kinetic analysis, the heat treatment durations of LPBF-fabricated Al-Cu-Li-Sc-Zr alloy were designed shorter than those of conventional manufacturing. Aging at 170 °C caused a small amount of T 1 phases to precipitate, and thus slightly increased the yield strength (YS) of the samples. Aging at 300 °C caused plenty of Al 3 (Sc, Zr) phases to precipitate, and thus significantly raised the YS of the samples. Solid solution treatment at 520 °C caused grain coarsening and coarse AlCuSc phases precipitated, and thus decreased the tensile properties. The solid solution treatment is not suitable for LPBF-fabricated Al-Cu-Li-Sc-Zr alloy. This study provides a systematic understanding of post heat treatment on microstructure and mechanical properties of LPBF-fabricated Al-Cu-Li-Sc-Zr alloy, contributing to heat-treatable Al Li alloys design for LPBF.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Towards high-temperature applications of aluminium alloys enabled by additive manufacturing10.1080/09506608.2021.1951580 ↗
2. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
3. Alloy design via additive manufacturing: advantages, challenges, applications and perspectives10.1016/j.mattod.2021.11.026 ↗
4. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
5. Design approaches for printability-performance synergy in Al alloys for laser-powder bed additive manufacturing10.1016/j.matdes.2021.109640 ↗
6. 3D printing of Aluminium alloys: additive manufacturing of Aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
7. Heat treatment of aluminium alloys produced by laser powder bed fusion: a review10.1016/j.matdes.2021.109651 ↗
8. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
9. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
10. Low temperature annealing dedicated to AlSi10Mg selective laser melting products10.1016/j.jallcom.2016.12.019 ↗
11. Microstructures and mechanical properties of A356 (AlSi7Mg0.3) aluminum alloy fabricated by selective laser melting10.1016/j.matdes.2015.10.065 ↗
12. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
13. Effect of heat treatments on fatigue property of selective laser melting AlSi10Mg10.1016/j.ijfatigue.2018.07.016 ↗
14. Abnormal corrosion behavior of selective laser melted AlSi10Mg alloy induced by heat treatment at 300 °C10.1016/j.jallcom.2019.06.274 ↗
15. Effect of T6 heat treatment on the surface tribological and corrosion properties of AlSi10Mg samples produced by selective laser melting10.1016/j.matchar.2020.110769 ↗
16. A comparative study of the effects of thermal treatments on AlSi10Mg produced by laser powder bed fusion10.1016/j.jallcom.2020.154822 ↗
17. Study of heat treatment parameters for additively manufactured AlSi10Mg in comparison with corresponding cast alloy10.1016/j.msea.2018.10.026 ↗
18. Evolution of the microstructure and mechanical properties of additively manufactured AlSi10Mg during room temperature holds and low temperature aging
19. Effect of heat treatment on the microstructure and anisotropy in mechanical properties of A357 alloy produced by selective laser melting10.1016/j.matdes.2018.05.026 ↗
20. The effect of annealing on microstructure and mechanical properties of selective laser melting AlSi10Mg10.1088/1757-899X/538/1/012023 ↗
21. Stress relaxation and the cellular structure-dependence of plastic deformation in additively manufactured AlSi10Mg alloys10.1016/j.ijplas.2019.12.003 ↗
22. A high strength Al–Li alloy produced by laser powder bed fusion: densification, microstructure, and mechanical properties
23. Mechanical behavior and microstructure evolution of Al-cu-mg alloy produced by laser powder bed fusion: effect of heat treatment10.1016/j.matchar.2020.110364 ↗
24. Aging responses of an Al-cu alloy fabricated by selective laser melting
25. Effects of process conditions on the mechanical behavior of Aluminium wrought alloy EN AW-2219 (AlCu6Mn) additively manufactured by laser beam melting in powder bed10.3390/mi8010023 ↗
26. Towards a high strength aluminium alloy development methodology for selective laser melting10.1016/j.matdes.2019.107775 ↗
27. Selective laser melting of a high strength Al Mn Sc alloy: alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
28. Microstructural features of Sc- and Zr-modified Al-mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
29. SLM-processed Sc- and Zr- modified Al-mg alloy: mechanical properties and microstructural effects of heat treatment10.1016/j.msea.2017.06.089 ↗
30. A heat treatable TiB2/Al-3.5Cu-1.5Mg-1Si composite fabricated by selective laser melting: microstructure, heat treatment and mechanical properties10.1016/j.compositesb.2018.04.026 ↗
31. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
32. Changing the alloy composition of Al7075 for better processability by selective laser melting10.1016/j.jmatprotec.2016.08.003 ↗
33. Investigation of solidification and precipitation behavior of Si-modified 7075 aluminum alloy fabricated by laser-based powder bed fusion10.1007/s11661-020-06073-9 ↗
34. Development of a high strength Al–Zn–Si–mg–cu alloy for selective laser melting10.1016/j.jallcom.2019.06.123 ↗
35. High strength Al–Li alloy development for laser powder bed fusion
36. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
37. The evolution and characterizations of Al3(ScxZr1-x) phase in Al–mg-based alloys proceeded by SLM10.1016/j.msea.2021.141863 ↗
38. Quantification and modelling of the microstructure/strength relationship by tailoring the morphological parameters of the T1 phase in an Al–cu–Li alloy10.1016/j.actamat.2014.04.046 ↗
39. Influence of the degree of scandium supersaturation on the precipitation kinetics of rapidly solidified Al-mg-Sc-Zr alloys10.1016/j.actamat.2016.07.001 ↗
40. Calculation of the Avrami parameters for heterogeneous solid state reactions using a modification of the Kissinger method10.1007/BF01912301 ↗
41. Hot deformation behavior and microstructure characteristic of 2055 Al-Li alloy during uniaxial compression10.1088/2053-1591/aba29b ↗
42. Precipitation kinetics, microstructure evolution and mechanical behavior of a developed Al-Mn-Sc alloy fabricated by selective laser melting10.1016/j.actamat.2020.04.015 ↗
43. Effect of precipitates on mechanical properties of AA219510.1016/j.jallcom.2016.01.229 ↗
44. Mechanical properties of aluminium–copper–lithium alloy AA2195 at cryogenic temperatures10.1016/j.matdes.2014.02.024 ↗
45. Microstructures and mechanical properties of spray deposited 2195 Al-cu-Li alloy through thermo-mechanical processing10.1016/j.msea.2018.04.116 ↗
46. Role of Zr and Sc addition in controlling the microstructure and tensile properties of aluminum–copper based alloys10.1016/j.matdes.2015.09.090 ↗
47. Alloys: scandium overtakes zirconium10.1038/nmat1663 ↗
48. Complex precipitation pathways in multicomponent alloys10.1038/nmat1652 ↗
49. Understanding grain refinement of Sc addition in a Zr containing Al-Zn-mg-cu aluminum alloy from experiments and first-principles10.1016/j.intermet.2020.106823 ↗
50. A general mechanism of grain growth I10.1016/j.jmat.2021.02.007 ↗
51. Scandium in aluminium alloys10.1179/174328005X14311 ↗
52. Influence of mg and Li content on the microstructure evolution of Al cu Li alloys during long-term ageing10.1016/j.actamat.2016.09.036 ↗