journal article·2017-12

Microstructure characterization and nano & micro hardness of tri-modal microstructure of titanium alloy under different hot working conditions

Zhenni Lei, Pengfei Gao, Hongwei Li, Xiaoguang Fan, Yang Cai, Mei Zhan

Publisher page

Abstract

Abstract In this work, the dependences of tri-modal microstructure parameters and corresponding nano & micro hardness on through-process processing parameters were quantitatively studied during the three-step thermo-mechanical processing of TA15 titanium alloy. It is found that the processing parameters of first step, especially for the deformation temperature and strain rate, mainly affect primary equiaxed α (αp) through the α → β phase transformation and the competition between dynamic recovery and dynamic recrystallization. The second processing step primarily affects the content and thickness of lamellar α (αl). In the third processing step, compared with low-temperature aging, normal annealing provides sufficient driving force for αl and secondary lamellar α (αs) growing, which leads to thicker αl and αs. As for the nano & micro hardness, in one sample undergoing different process, transformed β matrix (βt) is always harder than αl and αs due to the interfacial-strengthening effect. In addition, with increasing strain rate of the first step, αp becomes harder due to the constantly enhanced work hardening effect while the hardness of βt varies little because of the competition between interfacial strengthening and distribution disorder degree. However, the nano hardness of αl decreases firstly and then increases with strain rate, which presents the same trend with the micro hardness of integrated hardness at different processing conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Springback evaluation in hot v-bending of Ti-6Al-4V alloy sheets10.1007/s00170-014-6190-z ↗
2. Titanium alloys for aerospace applications10.1002/adem.200310095 ↗
3. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. Strengthening versus softening mechanisms by hydrogen addition in β-Ti40 alloy10.1016/j.ijhydene.2013.12.058 ↗
5. Hot compressive deformation behavior and microstructure evolution of Ti–6Al–2Zr–1Mo–1V alloy at 1073K10.1016/j.msea.2008.02.047 ↗
6. Plastic flow and microstructural evolution in Ti–6Al–2Zr–1Mo–1V alloys during hot deformation10.1179/174328409X439097 ↗
7. Microstructure evolution of TA15 titanium alloy subjected to equal channel angular pressing and subsequent annealing at various temperatures10.1016/j.jmatprotec.2011.03.004 ↗
8. Microstructural evolution of a Ti-4.5Al-3Mo-1V alloy during hot working10.1007/s10853-006-2658-z ↗
9. Alpha/beta heat treatment of a titanium alloy with a nonuniform microstructure10.1007/s11661-007-9088-7 ↗
10. Flow softening and microstructural evolution of TC11 titanium alloy during hot deformation10.1016/j.jmatprotec.2008.04.063 ↗
11. Importance of twinning in static and dynamic compression of a Ti–6Al–4V titanium alloy with an equiaxed microstructure10.1016/j.msea.2011.12.047 ↗
12. Tensile behavior at 700°C in Ti–Al–Sn–Zr–Mo–Nb–W–Si alloy with a bi-modal microstructure10.1016/j.msea.2013.11.096 ↗
13. Dynamic deformation behavior and ballistic impact properties of Ti-6Al-4V alloy having equiaxed and bimodal microstructures10.1007/s11661-004-0055-2 ↗
14. An investigation of a new near-beta forging process for titanium alloys and its application in aviation components10.1016/j.msea.2004.10.016 ↗
15. Microstructural features of TA15 titanium alloy under different temperature routes in isothermal local loading forming10.1016/j.msea.2012.02.006 ↗
16. Dependence of microstructure morphology on processing in subtransus isothermal local loading forming of TA15 titanium alloy10.1016/j.msea.2012.03.021 ↗
17. Tri-modal microstructure and performance of TA15 Ti-alloy under near-β forging and given subsequent solution and aging treatment10.1016/j.msea.2015.12.031 ↗
18. Tri-modal microstructure evolution of TA15 Ti-alloy under conventional forging combined with given subsequent heat treatment10.1016/j.jmatprotec.2015.09.011 ↗
19. Prediction and control of equiaxed α in near-β forging of TA15 Ti-alloy based on BP neural network: for purpose of tri-modal microstructure10.1016/j.msea.2013.10.080 ↗
20. Quantitative analysis of the microstructure of transitional region under multi-heat isothermal local loading forming of TA15 titanium alloy10.1016/j.matdes.2010.11.058 ↗
21. A study of the microstructure and hardness of two titanium alloys: commercially pure and Ti–6Al–4V10.1016/j.jallcom.2009.06.172 ↗
22. Determination of hardness and elastic modulus inverse pole figures of a polycrystalline commercially pure titanium by coupling nanoindentation and EBSD techniques10.1016/j.msea.2014.06.098 ↗
23. Development of strength-hardness relationships in additively manufactured titanium alloys10.1016/j.msea.2017.03.102 ↗
24. Development of a trimodal microstructure with superior combined strength, ductility and creep-rupture properties in a near alpha titanium alloy10.1016/j.msea.2017.04.068 ↗
25. Microindentation on W and Mo oriented single crystals: an STM study10.1016/0956-7151(93)90100-7 ↗
26. The deformation of plastically non-homogeneous materials10.1080/14786437008238426 ↗
27. A phenomenological theory for strain gradient effects in plasticity10.1016/0022-5096(93)90072-N ↗
28. Direct observations and analyses of dislocation substructures in the α phase of an α/β Ti-alloy formed by nanoindentation10.1016/j.actamat.2005.07.030 ↗
29. Material-length-scale-controlled nanoindentation size effects due to strain-gradient plasticity10.1016/S1359-6454(03)00281-7 ↗
30. Investigations on indentation size effects using a pile-up corrected hardness10.1088/0022-3727/41/7/074027 ↗
31. Size effects in micro- and nanoscale indentation10.1016/j.actamat.2005.12.031 ↗
32. Complete mechanical characterization of nanocrystalline Al-Mg alloy using nanoindentation10.1016/j.mechmat.2012.04.005 ↗
33. Indentation size effects in crystalline materials: a law for strain gradient plasticity10.1016/S0022-5096(97)00086-0 ↗
34. Indentation size effect in metallic materials: correcting for the size of the plastic zone10.1016/j.scriptamat.2005.02.009 ↗
35. Taylor factors in materials with many deformation modes10.1016/1359-6462(96)00137-6 ↗
36. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
37. Temperature dependence of the elastic constants10.1103/PhysRevB.2.3952 ↗
38. Mechanical behavior of Ti cold spray coatings determined by a multi-scale indentation method10.1016/j.msea.2011.09.083 ↗
39. Quantitative analysis of the microstructure of near β titanium alloy during compression tests10.1016/j.jmatprotec.2006.04.022 ↗
40. Determination of plastic properties of metals by instrumented indentation using different sharp indenters10.1016/S1359-6454(02)00568-2 ↗
41. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
42. Micromechanical behavior study of forged 7050 aluminum alloy by microindentation10.1016/j.matdes.2012.01.036 ↗
43. Orowan strengthening effect on the nanoindentation hardness of the ferrite matrix in microalloyed steels