Abstract
Abstract Characteristics of the oxide film formed on stainless steel weld overlay cladding aged at 400 °C for different times in high temperature water were studied. The results showed that thermal aging showed no obvious effect on the volume fraction of ferrite phase but resulted in high corrosion susceptibility of the aged ferrite phase mainly. The oxide film formed on the unaged cladding material consisted of 100-nm-thick inner oxide layer (FeCr2O4 and Cr2O3) and Fe-rich outer oxide particles (Fe3O4) with a size of
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Sensitization behavior of type 308 stainless steel weld metals after postweld heat treatment and low-temperature aging and its relation to microstructure10.1007/s11661-002-0183-5 ↗
2. Intergranular stress corrosion cracking behavior of niobium-added Type 308 stainless steel weld overlay metal in a simulated BWR environment10.1016/S0029-5493(02)00002-X ↗
3. The aging behavior of homogenized type 308 and 308CRE stainless steel10.1007/BF02647189 ↗
4. Microscopical evaluation of low temperature aging of type 308 stainless steel weldments10.1179/mst.1990.6.3.314 ↗
5. Low temperature aging behavior of type 308 stainless steel weld metal10.1016/0956-7151(91)90118-K ↗
6. Effects of thermal aging on microstructure and hardness of stainless steel weld-overlay claddings of nuclear reactor pressure vessels10.1016/j.jnucmat.2014.04.003 ↗
7. Microstructural changes of a thermally aged stainless steel submerged arc weld overlay cladding of nuclear reactor pressure vessels10.1016/j.jnucmat.2011.12.004 ↗
8. Study on microstructural changes in thermally-aged stainless steel weld-overlay cladding of nuclear reactor pressure vessels by atom probe tomography10.1016/j.jnucmat.2011.06.004 ↗
9. Microstructure evolution and impact fracture behaviors of Z3CN20-09M stainless steels after long-term thermal aging10.1016/j.msea.2013.05.009 ↗
10. Microstructures and mechanical properties of cast austenite stainless steels after long-term thermal aging at low temperature10.1016/j.matdes.2013.02.061 ↗
11. Low temperature thermal aging of austenitic stainless steel welds: kinetics and effects on mechanical properties10.1016/j.msea.2011.11.055 ↗
12. Effects of ferrite content on the mechanical properties of thermal aged duplex stainless steels10.1016/j.msea.2014.11.065 ↗
13. Evaluation of thermal aging embrittlement of duplex stainless steels by electrochemical method10.1016/0956-716X(95)00119-G ↗
14. Detection and evaluation of material degradation of thermally aged duplex stainless steels: electrochemical polarization test and AFM surface analysis10.1016/0022-3115(96)00361-3 ↗
15. Low temperature thermal ageing embrittlement of austenitic stainless steel welds and its electrochemical assessment10.1016/j.corsci.2011.09.031 ↗
16. Thermal aging at 475 °C of newly developed lean duplex stainless steel 2404: mechanical properties and corrosion behavior10.1016/j.corsci.2016.12.014 ↗
17. Influence of long-term low-temperature aging on the microhardness and corrosion properties of duplex stainless steel10.1016/j.corsci.2012.10.038 ↗
18. Effects of aging at 475 °C on corrosion properties of tungsten-containing duplex stainless steels10.1016/S0010-938X(02)00079-3 ↗
19. Effect of thermal aging at 475 °C on the properties of lean duplex stainless steel 210110.1016/j.matchar.2016.03.002 ↗
20. Effects of low temperature aging on the mechanical properties and corrosion resistance of duplex and lean duplex stainless steels UNS S32205 and UNS S32304
21. In situ Raman spectroscopic analysis of surface oxide films on Ni-base alloy/low alloy steel dissimilar metal weld interfaces in high-temperature water10.1016/j.jnucmat.2014.03.038 ↗
22. In-situ investigation of thermal aging effect on oxide formation in Ni-base alloy/low alloy steel dissimilar metal weld interfaces10.1016/j.corsci.2014.06.006 ↗
23. Effect of thermal aging on corrosion fatigue of Z3CN20.09M duplex stainless steel in high temperature water10.1016/j.msea.2015.12.080 ↗
24. Microstructure and electrochemical behavior of stainless steel weld overlay cladding exposed to post weld heat treatment10.1557/jmr.2016.526 ↗
25. Research status and outlook on thermal aging of cast austenitic stainless steels used in primary coolant pipes of nuclear power plant
26. Effects of temperature on the oxide film properties of 304 stainless steel in high temperature lithium borate buffer solution10.1016/j.corsci.2009.08.006 ↗
27. Process in study on corrosion scale formed in high-temperature and high-pressure water
28. Effect of nickel ion from autoclave material on oxidation behaviour of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.12.008 ↗
29. The evolution of electrochemical behaviour and oxide film properties of 304 stainless steel in high temperature aqueous environment10.1016/j.electacta.2012.03.148 ↗
30. Influence of later-dissolved oxygen on microstructural changes in oxide films formed on alloy 690TT in hydrogenated primary water10.1016/j.corsci.2015.02.003 ↗
31. Effect of electropolishing on corrosion of nuclear grade 316L stainless steel in deaerated high temperature water10.1016/j.corsci.2016.09.002 ↗
32. Corrosion of nickel-base alloys in primary medium of pressurized water reactors: new insights on the oxide growth mechanisms and kinetic modelling10.1016/j.corsci.2015.09.001 ↗
33. G-phase formation in aged type 308 stainless steel10.1007/BF02646233 ↗
34. Effect of surface state on the oxidation behavior of welded 308L in simulated nominal primary water of PWR10.1016/j.apsusc.2015.02.066 ↗
35. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
36. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
37. Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments10.1016/j.corsci.2010.06.016 ↗
38. Properties of oxide films formed on 316L SS and model alloys with modified Ni, Cr and Si contents in high temperature water10.1016/j.corsci.2016.02.001 ↗
39. Corrosion of engineering materials in a supercritical water cooled reactor: characterization of oxide scales on Alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
40. Interpretation of the relation between ferrite fraction and pitting corrosion resistance of commercial 2205 duplex stainless steel10.1016/j.corsci.2014.08.021 ↗
41. Effects of Mn on the mechanical properties and high temperature oxidation of 9Cr2WVTa steel10.1016/j.jnucmat.2017.07.024 ↗
42. Effect of Mn addition on corrosion properties of biodegradable Mg-4Zn-0.5Ca-xMn alloys10.1016/j.jallcom.2016.10.244 ↗