Dynamic recrystallization mechanism and near-isotropic mechanical properties of WE43 magnesium alloy sheets rolled at different temperatures
Source abstract
Abstract
The dynamic recrystallization (DRX) behavior and mechanical properties of WE43 magnesium alloy during hot rolling rather than hot compression at 400–500 °C were systematically investigated by electron backscattering diffraction (EBSD) analysis. At relatively low temperatures, such as 400 °C, the rolled sheets cracked, and no DRX grains were found, and twinning contributed more to the plastic deformation . However, when the rolling temperature was above 450 °C, the alloy exhibited an excellent rolling ability, and slip dominated the plastic deformation. In parallel, the recrystallization mechanism involved continuous dynamic recrystallization (CDRX), where grains nucleated along the original grain boundaries and geometrically necessary dislocations (GNDs) occurred within the parent grains. In addition, a few twin-induced recrystallization grains were observed in the early stage of the rolling process at 500 °C. Rolled sheets at suitable temperatures have similar strength and fracture elongation and do not exhibit obvious anisotropy. This can be attributable to the random orientation of the DRX grains and similar Schmid factor (SF) values of different loading directions at different rolling temperatures.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Effects of minor Nd and Er additions on the precipitation evolution and dynamic recrystallization behavior of Mg-6.0Zn-0.5Mn alloy10.1016/j.jma.2020.06.018 ↗
2. Evading strength-corrosion tradeoff in Mg alloys via dense ultrafine twins10.1038/s41467-021-24939-3 ↗
3. Enhanced strength and corrosion resistance of Mg-Gd-Y-Zr alloy with ultrafine grains10.1016/j.matlet.2017.11.096 ↗
4. Microstructure and superior mechanical properties of a multi-axially forged WE magnesium alloy10.1016/j.jallcom.2016.09.198 ↗
5. Comparisons of microstructure homogeneity, texture and mechanical properties of AZ80 magnesium alloy fabricated by annular channel angular extrusion and backward extrusion10.1016/j.jma.2020.05.010 ↗
6. Texture tailoring and bendability improvement of rolled AZ31 alloy using {10–12} twinning: The effect of precompression levels10.1016/j.jma.2019.09.002 ↗
7. Comparison of static recrystallization behavior in hot rolled Mg-3Al-1Zn and Mg-3Zn-0.5Ca sheets10.1016/j.jallcom.2013.11.210 ↗
8. Twinning-induced dynamic recrystallization and micro-plastic mechanism during hot-rolling process of a magnesium alloy10.1016/j.msea.2017.05.037 ↗
9. Enhanced strength and ductility AZ91 alloy with heterogeneous lamella structure prepared by pre-aging and low-temperature extrusion10.1016/j.msea.2021.141094 ↗
10. The origin of “rare earth” texture development in extruded mg-based alloys and its effect on tensile ductility10.1016/j.msea.2008.05.045 ↗
11. Individual effect of recrystallisation nucleation sites on texture weakening in a magnesium alloy: part 1-double twins10.1016/j.actamat.2017.06.015 ↗
12. Current issues in magnesium sheet alloys: where do we go from here?10.1016/j.scriptamat.2014.04.017 ↗
13. Bettles · 2012
14. Evolution of microstructure and microtexture during the hot deformation of Mg–3% Al10.1016/j.actamat.2010.04.017 ↗
15. Recrystallization mechanism of as-cast AZ91 magnesium alloy during hot compressive deformation10.1016/j.msea.2009.08.062 ↗
16. Twins, shear bands and recrystallization of a Mg–2.0%Zn–0.8%Gd alloy during rolling10.1016/j.scriptamat.2010.09.029 ↗
17. Influence of deformation twinning on static annealing of AZ31 Mg alloy10.1016/j.actamat.2013.06.037 ↗
18. Twin recrystallization mechanisms and exceptional contribution to texture evolution during annealing in a magnesium alloy10.1016/j.actamat.2016.12.058 ↗
19. Dynamic recrystallization behaviors of a Mg-4Y-2Nd-0.2Zn-0.5Zr alloy and the resultant mechanical properties after hot compression10.1016/j.matdes.2016.02.072 ↗
20. Effect of microalloying with rare-earth elements on the texture of extruded magnesium-based alloys10.1016/j.scriptamat.2008.06.008 ↗
21. Explaining texture weakening and improved formability in magnesium rare earth alloys10.1179/1743284714Y.0000000632 ↗
22. Mechanical anisotropy and deep drawing behaviour of AZ31 and ZE10 magnesium alloy sheets10.1016/j.actamat.2009.09.038 ↗
23. Effect of strain path on the evolution of microstructure, texture and tensile properties of WE43 alloy10.1016/j.msea.2018.01.018 ↗
24. Effect of solution treatment on the microstructure and mechanical properties of sand-cast Mg–9Gd–4Y–0.5Zr alloy10.1007/s40195-017-0591-6 ↗
25. Dynamic precipitation and dynamic recrystallization during hot deformation of a solutionized WE43 magnesium alloy10.1016/j.msea.2019.138076 ↗
26. Micro and macro texture evolution during multiaxial forging of a WE43 magnesium alloy10.1016/j.jallcom.2017.12.181 ↗
27. Characterization of continuous dynamic recrystallization in WE43 magnesium alloy10.1016/j.matchemphys.2020.123726 ↗
28. Role of RE in the deformation and recrystallization of Mg alloy and a new alloy design concept for Mg-RE alloys10.1016/j.scriptamat.2014.12.010 ↗
29. Direct observation of precipitation along twin boundaries and dissolution in a magnesium alloy annealing at high temperature10.1016/j.scriptamat.2017.05.015 ↗
30. Managing strength and ductility in AZ91 magnesium alloy through ECAP combined with prior and post aging treatment10.1016/j.matchar.2019.04.022 ↗
31. The role of double twinning on transgranular fracture in magnesium AZ61 in a localized stress field10.1016/j.actamat.2015.09.026 ↗
32. A near-isotropic ultrafine-grained Mg-Gd-Ag alloy with high strength-ductility synergy10.1016/j.jmrt.2020.09.115 ↗
33. Deformation and fracture mechanisms in WE43 magnesium-rare earth alloy fabricated by direct-chill casting and rolling10.1016/j.msea.2018.04.090 ↗
34. Y. Wang, F. Li, N. Bian, H.Q. Du, P. Da Huo, Mechanism of plasticity enhancement of AZ31B magnesium alloy sheet by accumulative alternating back extrusion, J. Magnes. Alloy, doi:10.1016/j.jma.2021.08.035, (In press).10.1016/j.jma.2021.08.035 ↗
35. Grain size effect on tensile properties and slip systems of pure magnesium10.1016/j.actamat.2020.116604 ↗
36. Microstructural development during hot working of Mg-3Al-1Zn10.1007/s11661-007-9207-5 ↗
37. Triggering rare earth texture modification in magnesium alloys by addition of zinc and zirconium10.1016/j.actamat.2013.12.015 ↗
38. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
39. Effect of magnesium carbonate on microstructure and rolling behaviors of AZ31 alloy10.1016/j.msea.2010.10.053 ↗
40. Evading strength-corrosion tradeoff in Mg alloys via dense ultrafine twins10.1038/s41467-021-24939-3 ↗
41. Exceptional mechanical properties of ultra-fine grain Mg-4Y-3RE alloy processed by ECAP10.1016/j.msea.2017.09.106 ↗
42. Mechanical properties of Mg–Al–Zn alloy with a tilted basal texture obtained by differential speed rolling10.1016/j.msea.2007.11.029 ↗
43. Reducing the yield asymmetry in Mg-5Li-3Al-2Zn alloy by hot-extrusion and multi-pass rolling10.1016/j.jma.2020.06.015 ↗