journal article·2020-10

Effect of adding Ce on the hot-tearing susceptibility of the 5TiB2/Al-5Cu composite

Xiaobo Zhang, Peng Zhu, Long Zeng, Baigang Feng, Xiongbin Wan, Junqiang Ren

Publisher page

Abstract

Abstract Hot tearing is a severe solidification defect that occurs during the metal solidification process. To reduce the hot-tearing susceptibility (HTS) of a 5TiB2/Al-5Cu composite, rare-earth Ce with mass fractions of 0.2%, 0.5%, and 1% was added to the composite in this study. The results indicated that the HTS of the composite decreased with the increase of Ce from 0.2% to 1%. The HTS value of the 5TiB2/Al-5Cu composite decreased from 15.61 to 5.60, and the solidification-temperature range of the composites gradually narrowed after the Ce addition. In addition, the grain size of the composite was refined, and the average grain diameter decreased from 26.29 μm to 18.97 μm. With the increase in Ce content, the composite microstructure was refined and the TiB2 particle agglomeration dissolved. As the Ce increased, the finer lamellar Al8Cu4Ce phase promoted a more uniform microstructure and a more fluid liquid metal. Therefore, the residual liquid metal better fed the cracks, and the grain-boundary phases formed more bridges to improve the high HTS of 5TiB2/Al-5Cu composites.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Hot deformation flow behavior of powder metallurgy based Al-SiC and Al-Al2O3 composite in a single step and two-step uni-axial compression10.1016/j.matchar.2019.03.047 ↗
2. Simultaneously increasing the elevated-temperature tensile strength and plasticity of in situ nano-sized TiCx/Al-Cu-Mg composites10.1016/j.matchar.2017.01.013 ↗
3. In-situ investigation of deformation behavior and fracture mechanism of laminated Al/Ti composites fabricated by hot rolling10.1016/j.jallcom.2018.12.272 ↗
4. Influence of a new kind of Al–Ti–C master alloy on the microstructure and mechanical properties of Al–5Cu alloy10.1016/j.jallcom.2013.11.187 ↗
5. Novel preparation of Al-5%Cu/BN and Si3N4 composites with analyzing microstructure, thermal and mechanical properties10.1016/j.matchar.2017.12.015 ↗
6. Double-peak age strengthening of cold-worked 2024 aluminum alloy10.1016/j.actamat.2012.11.039 ↗
7. Influence of Al addition on solidification path and hot tearing susceptibility of Mg–2Zn–(3 + 0.5x)Y–xAl alloys10.1016/j.jma.2019.04.001 ↗
8. Quality index and hot tearing susceptibility of Al–7Si–0.35Mg–xCu alloys10.1016/S1003-6326(18)64783-1 ↗
9. Effect of TiBor on the grain refinement and hot tearing susceptibility of AZ91D magnesium alloy10.1016/j.jallcom.2018.05.129 ↗
10. Preparation of in-situ 5 vol% TiB 2 particulate reinforced Al–4.5Cu alloy matrix composites assisted by improved mechanical stirring process10.1016/j.matdes.2016.01.023 ↗
11. Tuning the microstructure features of in-situ nano TiB2/Al-Cu-Mg composites to enhance mechanical properties10.1016/j.jallcom.2018.10.078 ↗
12. Improvement of yttrium on the hot tearing susceptibility of 6TiB2/Al-5Cu composite10.1016/S1002-0721(14)60566-4 ↗
13. Microstructure and mechanical properties at both room and high temperature of in-situ TiC reinforced Al–4.5Cu matrix nanocomposite10.1016/j.jallcom.2018.07.045 ↗
14. Eutectic microstructures in dilute Al-Ce and Al-Co alloys10.1016/j.matchar.2019.06.010 ↗
15. The ternary Al–Ce–Cu phase diagram in the aluminum-rich corner10.1016/j.actamat.2007.06.009 ↗
16. Effects of TiB2 particle size on the microstructure and mechanical properties of TiB2-based composites10.1016/j.ceramint.2018.08.270 ↗
17. Quantitative analysis of TiB2 particles and properties of Cu-TiB2 composite prepared by in situ reaction10.1016/S1875-5372(18)30039-0 ↗
18. Hot tearing of ternary Mg-Al-Ca alloy castings10.1007/s11661-006-1059-x ↗
19. A review on hot tearing of magnesium alloys10.1016/j.jma.2016.08.003 ↗
20. G. Cao, I. Haygood, S. Kou, Onset of Hot Tearing in Ternary Mg-Al-Sr Alloy Castings, Metall. Trans. A 41(8) 2139–2150.10.1007/s11661-010-0248-9 ↗
21. Thermodynamic assessment of Al–Ce–Cu system10.1016/j.jallcom.2009.04.083 ↗
22. Effect of homogeneity of particle distribution on tensile crack propagation in mushy state rolled in situ Al–4.5Cu–5TiB2 particulate composite10.1016/j.msea.2013.03.049 ↗
23. Crack-healing behavior of Al2O3-TiB2-TiSi2 ceramic material10.1016/j.ceramint.2017.10.164 ↗
24. Improving the mechanical properties of Fe – TiB2 high modulus steels through controlled solidification processes10.1016/j.actamat.2016.07.056 ↗
25. A novel two-step processing method for fabrication of in situ Al2O3np/Al-Al11Ce3 nanocomposite10.1016/S1002-0721(14)60403-8 ↗
26. Effects of cerium addition on solidification behaviour and intermetallic structure of novel Al–Cu–Li alloys10.1016/S1875-5372(16)30125-4 ↗
27. Effect of RE addition on solidification process and high-temperature strength of Al−12%Si−4%Cu−1.6%Mn heat-resistant alloy10.1016/S1003-6326(19)65020-X ↗
28. Evaluation of effects of crack deflection and grain bridging on toughening of nanocrystalline SiO2 stishovite10.1016/j.jeurceramsoc.2017.06.047 ↗
29. Investigation of rare earth particulate on tribological and mechanical properties of Al-6061 alloy composites for aerospace application10.1016/j.jmrt.2019.06.025 ↗
30. The contribution of constitutional supercooling to nucleation and grain formation10.1007/s11661-015-2960-y ↗
31. Thermodynamic aspects of grain growth restriction in multicomponent alloy solidification10.1016/j.actamat.2011.06.026 ↗
32. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles10.1007/s11661-005-0054-y ↗
33. Mechanical properties in the semi-solid state and hot tearing of aluminium alloys10.1016/S0079-6425(03)00037-9 ↗
34. Hot-tear susceptibility of aluminum wrought alloys and the effect of grain refining10.1007/s11661-007-9132-7 ↗
35. A criterion for cracking during solidification10.1016/j.actamat.2015.01.034 ↗