journal article·2023-03

Formation mechanisms and three-dimensional characterization of composite inclusion of MnS-Al2O3 in high speed wheel steel

Xiaopei Guo, Min Tan, Tao Li, Liying Ju, Jie Dang, Han Guo, Yi Zhao

Publisher page

Abstract

Inclusions have a significant impact on the properties of steel. The composite inclusions of MnS-Al 2O 3 in high speed wheel steel largely reduce the stress concentration around the inclusion and enhance the toughness of the steel. In this paper, high speed wheel steel was prepared in the laboratory. The inclusions in steel mainly include MnS, Al 2O 3 and composite inclusions of MnS-Al 2O 3. The orientation of the interface of MnS and Al 2O 3 in composite inclusion was Al 2O 3 (1 0–1 4) // MnS (211), which was analyzed by TEM. It is indicated that Al 2O 3 inclusions provide effective nucleation conditions for the precipitation of MnS due to the calculation of the mismatch between Al 2O 3 and MnS. The composite inclusions in steel were reconstructed by Micro-CT and the three-dimensional (3D) morphologies were analyzed in detail. This method avoids artifacts and misleading of the two-dimensional observation of the cross sections of the steel samples. Meanwhile, the 3D observation by Micro-CT is an innovative method to characterize the different phases of the inclusion simultaneously, which paved a way for the analysis of the composite inclusions in the steel. The formation of Al 2O 3 , MnS and composite inclusion was discussed based on the thermodynamic calculations. It was clarified that the Al 2O 3 precipitated in liquid steel, while MnS precipitated after the steel completely solidified.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgical Processes and Thermodynamics · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. The railway accident of Eschede – technical background[J]10.1016/j.engfailanal.2003.11.001 ↗
2. Characterization of segregation degree for large size metal component and application on high-speed train wheel[J]10.1016/j.aca.2022.339719 ↗
3. Effect of carbon contents on dry sliding wear behavior of high vanadium high speed steel[J]10.1016/j.wear.2012.07.003 ↗
4. Mechanisms and new parameter attribute reduction of high-speed railway wheel rim steel subjected to low temperature fatigue[J]10.1016/j.msea.2016.07.055 ↗
5. Study on fatigue failure mechanism at various temperatures of a high-speed railway wheel steel[J]10.1016/j.msea.2017.04.042 ↗
6. Temperature-dependent crack induced by microstructure evolution in 20Mn2SiMoCuV bainite wheel steel[J]10.1016/j.engfailanal.2022.106593 ↗
7. Properties and microstructure of high performance wheels[J]10.1016/j.wear.2010.10.017 ↗
8. Influence of non-uniform microstructure on rolling contact fatigue behavior of high-speed wheel steels[J]10.1016/j.engfailanal.2019.03.002 ↗
9. Investigations of fatigue crack propagation in ER8 railway wheel steel with varying microstructures[J]10.1016/j.msea.2022.142980 ↗
10. Frictional heat-induced phase transformation on train wheel surface[J]10.1016/S1006-706X(08)60248-4 ↗
11. Study on Wear and fatigue performance of two types of high-speed railway wheel materials at different ambient temperatures[J]10.3390/ma13051152 ↗
12. Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength[J]10.1016/S0142-1123(02)00037-3 ↗
13. The effect of inclusions on the fatigue behavior of fine-grained high strength 42CrMoVNb steel[J]10.1016/j.ijfatigue.2004.01.009 ↗
14. Effect of inclusion density on ductile fracture toughness and roughness[J]10.1016/j.jmps.2013.10.003 ↗
15. The effect of non-metallic inclusions on the mechanical properties of 32 CDV 13 steel and their mechanical stress analysis by numerical simulation[J]10.1016/j.tafmec.2018.01.013 ↗
16. The effect of different non-metallic inclusions on the machinability of steels[J]10.3390/ma8020751 ↗
17. The influence of nonmetallic inclusions on the mechanical properties of steel: A review[J]10.1007/PL00020378 ↗
18. The effect of inclusion type on the toughness of 4340 steel[J]10.1080/10426910903221138 ↗
19. Effect of MnS inclusion and crystallographic texture on anisotropy in Charpy impact toughness of low carbon ferritic steel[J]10.1016/j.msea.2015.12.047 ↗
20. Mechanical anisotropy and local ductility in transverse tensile deformation in hot rolled steels: the role of MnS inclusions[J]10.1016/j.msea.2018.12.026 ↗
21. Effect of shape of sulfide inclusions on anisotropy of inclusion spacings and on directionality of ductility in hot-rolled C-Mn steels[J]10.1007/BF02644720 ↗
22. Characterization of the morphological evolution of MnS inclusions in free-cutting steel during heating[J]10.1016/j.jmrt.2022.01.095 ↗
23. Morphological transformation of elongated MnS inclusions in non-quenched and tempered steel during isothermal heating[J]
24. Behavior of MnS inclusions during homogenization process in low-alloyed steel FAS3420H[J]10.1515/htmp-2021-0014 ↗
25. Effect of heat treatment conditions on shape control of large-sized elongated MnS inclusions in Resulfurized free-cutting steels[J]10.2355/isijinternational.51.1995 ↗
26. Relationship between repeatedly quenching and fisheye cracks around TiN and Al2O3 inclusions in high carbon bearing steel[J]10.1179/1432891713Z.000000000355 ↗
27. Quantitative investigation of influence of Al2O3 non-metallic inclusions on bending strength of powder metallurgy highspeed steel[J]10.1088/1742-6596/2200/1/012025 ↗
28. Prediction of fatigue life of steels in consideration of defect-induced crack initiation and propagation[J]10.2355/isijinternational.ISIJINT-2019-573 ↗
29. The effect of inclusions on internal cracks for 20Mn5N steel ingot after forging[J]10.4028/www.scientific.net/AMR.834-836.829 ↗
30. Fracture behaviors at inclusions of very-high-cycle fatigue in newly developed clean bearing steel[J]10.1142/S0217979221502684 ↗
31. Fracture evolution in ferrite/martensite dual-phase flange steel[J]10.1080/03019233.2020.1733779 ↗
32. Influence of inclusion on crack initiation in wheel rim[J]10.1016/S1006-706X(11)60010-1 ↗
33. Effect of sulfur contents on properties and inclusions in high speed wheel steels[J]
34. Study of the effect of sulfur contents on fracture toughness of railway wheel steels for high speed train[J]
35. Assessment of inclusion analysis via manual and automated SEM and total oxygen content of steel[J]10.1016/j.jmrt.2015.01.008 ↗
36. Qualitative and quantitative determination of micro-inclusions by automated SEM/EDX analysis[J]10.1007/s00216-004-2528-y ↗
37. Automated SEM-EDS pottery classification based on minero-chemical quantitative parameters: an application on ancient Greek pottery from Adrano (NE Sicily, Italy)[J]10.1002/xrs.3118 ↗
38. TEM characterization of a titanium nitride (TiN) inclusion in a Fe-Ni-co Maraging steel[J]10.1007/s11661-015-2896-2 ↗
39. TEM study of PM 2000 steel[J]10.1179/174329005X64171 ↗
40. Analysis of oxide inclusions in steel by fast laser-induced breakdown spectroscopy scanning: an approach to quantification[J]10.1366/000370207780220895 ↗
41. Distinguishing MgO·Al2O3 spinel inclusions from alumina or magnesia inclusions in aluminum-killed stainless steel using Cathodoluminescence imaging[J]10.2355/isijinternational.ISIJINT-2021-152 ↗
42. Non-metallic inclusion density in bearing steel characterized by ultrasonic testing[M]
43. Detection of non-metallic inclusions in steel continuous casting billets[J]10.1007/s11663-014-0042-y ↗
44. Calcium modification of spinel inclusions in aluminum-killed steel: reaction steps[J]10.1007/s11663-012-9660-4 ↗
45. Atomic-scale analysis of oxide inclusion in weld metal using atom probe tomography[J]10.1007/s11661-022-06623-3 ↗
46. Continuum plasticity modelling of work hardening for precipitation-hardened martensitic steel guided by atom probe tomography[J]10.1016/j.matdes.2022.110463 ↗
47. Mechanical and macrostructural properties of 3D printed concrete dosed with steel fibers under different loading direction[J]10.1016/j.conbuildmat.2022.126616 ↗
48. Spatial distribution of steel fibers and air bubbles in UHPC cylinder determined by X-ray CT method[J]10.1016/j.conbuildmat.2017.11.030 ↗
49. Three-dimensional observation of nonmetallic inclusion clusters in solid metal by X-ray Micro-CT[J]10.2355/isijinternational.ISIJINT-2016-218 ↗
50. Three-dimensional characterization of MnS inclusions in steel during rolling process[J]10.1016/j.matchar.2019.109944 ↗
51. Three-dimensional characterization of typical inclusions in steel by X-ray Micro-CT[J]10.1016/j.jmrt.2020.01.106 ↗
52. Three-dimensional characterization of typical inclusions in steel by X-ray Micro-CT[J]
53. Nucleation catalysis.[J]10.1021/ie50510a031 ↗
54. The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron[J]10.1007/BF02642799 ↗
55. PITRE: software for phase-sensitive X-ray image processing and tomography reconstruction[J]10.1107/S0909049512029731 ↗
56. Mathematical model of the thermal processing of steel ingots: part I. heat flow model[J]10.1007/BF02658437 ↗
57. Huang · 2017 · 181
58. Thermodynamics on control of inclusions composition in ultraclean steels[J]10.2355/isijinternational.36.528 ↗
59. Extraction, thermodynamic analysis, and precipitation mechanism of MnS-TiN complex inclusions in low-sulfur steels[J]10.1007/s11661-016-3463-1 ↗
60. Dispersion Behavior of MgO, ZrO2, Al2O3,CaO-Al2O3 and MnO-SiO2 deoxidation particles during solidification of Fe-10mass%Ni alloy[J]10.2355/isijinternational.46.22 ↗