Influence of heat treatment, microstructure evolution, and damage mechanism on high cycle fatigue behaviour of additively manufactured Ti-modified Al 2024 alloy
Source abstract
Abstract
The high cycle fatigue behaviour of titanium modified Al 2024 alloy produced by laser powder bed fusion (LPBF) is investigated to elucidate the effect of the microstructural features, residual stress, and defects (such as porosity and lack of fusion) on dynamic behaviour. The titanium acts as a grain refining agent; it can reduce the solidification cracking and produce the ultrafine-grained (UFG) microstructure in aluminium alloys. The 2% titanium addition resulted in the UFG microstructure with an average size of 0.52 μm in as-built samples. The microstructural features were examined through scanning electron microscopy (SEM), transmission electron microscopy (TEM), and electron back-scattered diffraction (EBSD) analysis. The influence of the microstructural features, such as grain size, dislocation density, precipitate-dislocation interaction, etc., on the fatigue life of as built and T6 heat treated samples was analysed in detail. The effect of varying stress amplitude at a stress ratio of 0.1 and a frequency of 30 Hz was investigated for the as-built and heat-treated sample. The T6 heat-treated sample showed 21.9% higher fatigue strength compared to the as-built samples (87.8 MPa in the heat-treated sample compared to 72 MPa in the as-built sample). The corresponding damage mechanisms are thoroughly explored through scanning electron fractography, TEM, and EBSD. The defects like porosity and lack of fusion defects in the surface or sub-surface level were observed to be critical regions as crack initiation sites.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles10.1016/j.actamat.2020.06.026 ↗
2. Laser powder bed fusion of nano-CaB6 decorated 2024 aluminum alloy10.1016/j.jallcom.2021.158714 ↗
3. Anisotropic high cycle fatigue property of Sc and Zr-modified Al-Mg alloy fabricated by laser powder bed fusion
4. Processing and characterization of crack-free aluminum 6061 using high-temperature heating in laser powder bed fusion additive manufacturing
5. A novel crack-free Ti-modified Al-Cu-Mg alloy designed for selective laser melting
6. Selective laser melting additive manufacturing of 7xxx series Al-Zn-Mg-Cu alloy: cracking elimination by co-incorporation of Si and TiB2
7. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
8. Microstructure and mechanical properties of a TiB2-modified Al–cu alloy processed by laser powder-bed fusion10.1016/j.msea.2020.140209 ↗
9. Effect of processing parameters on the densification of an additively manufactured 2024 Al alloy10.1016/j.jmst.2020.03.070 ↗
10. Effect of Zr content on formability, microstructure and mechanical properties of selective laser melted Zr modified Al-4.24Cu-1.97Mg-0.56Mn alloys10.1016/j.jallcom.2018.06.032 ↗
11. Effect of Zirconium addition on crack, microstructure and mechanical behavior of selective laser melted Al-Cu-Mg alloy10.1016/j.scriptamat.2017.02.036 ↗
13. The effect of defect population on the anisotropic fatigue resistance of AlSi10Mg alloy fabricated by laser powder bed fusion10.1016/j.ijfatigue.2021.106317 ↗
14. Effect of surface and subsurface defects on fatigue behavior of AlSi10Mg alloy processed by laser powder bed fusion (L-PBF)10.3390/met9101063 ↗
15. Study on the fatigue behaviour of selective laser melted AlSi10Mg alloy10.1016/j.msea.2020.139180 ↗
16. Davis · 1993
17. Properties and selection: nonferrous alloys and special-purpose materials was
18. Kaufman · 2008
19. Fatigue of 2024-T351 aluminium alloy at different load ratios up to 10 10 cycles10.1016/j.ijfatigue.2012.07.013 ↗
20. Level set simulations of dislocation-particle bypass mechanisms10.1016/j.actamat.2003.12.016 ↗
21. Homogenization timing effect on microstructure and precipitation strengthening of 17–4PH stainless steel fabricated by laser powder bed fusion
22. High cycle fatigue performance of AlSi10mg alloy produced by selective laser melting10.1016/j.mechmat.2020.103499 ↗
23. Fundamentals of solidification in aluminum castings
24. Novel approach to additively manufacture high-strength Al alloys by laser powder bed fusion through addition of hybrid grain refiners
25. A statistically significant experimental technique for investigating microsegregation in cast alloys10.1007/BF02666687 ↗
26. Microstructural features of Sc- and Zr-modified Al-Mg alloys processed by selective laser melting10.1016/j.matdes.2016.11.040 ↗
27. Rollett · 2004
28. Exceptional high fatigue strength in Cu-15at.%Al alloy with moderate grain size
29. On the Hall-Petch relationship in a nanostructured Al-Cu alloy10.1016/j.msea.2010.08.070 ↗
30. Prediction of non propagating cracks10.1016/0013-7944(79)90081-X ↗