journal article·2022-12

Effect of microstructure on corrosion behaviour of Al-Cu-Li alloys

J.Y. Huang, W.Q. Ming, C.L. Wu

Publisher page

Abstract

The corrosion behaviour and its relationship with microstructure, especially the distribution of precipitates at grain boundaries and within grains, of two Al-Cu-Li alloys with different Cu/Li ratio were investigated using accelerated immersion testing, advanced microscopy characterization and quasi-in-situ corrosion observation. The Al-2.23Cu-0.96Li alloy with low Cu/Li ratio exhibited excellent intergranular corrosion resistance and its corrosion modes unusually remained consistent intragranular corrosion regardless of the ageing stage. The corrosion behaviour of the counterpart Al-4.03Cu-0.91Li alloy with high Cu/Li ratio was found to follow the general evolution regulation, from intergranular corrosion to intragranular corrosion with the ageing time. Microstructure characterizations demonstrated that the coarsening and discontinuous distribution of grain-boundary precipitates played the key role in lowering the intergranular corrosion susceptibility of the two Al-Cu-Li alloys. Further quasi-in-situ corrosion observation of the Al-2.23Cu-0.96Li alloy showed that the dealloying process of the grain-boundary precipitates led to the dissolution of the precipitate-free zone, which meant that the broadening of the precipitate-free zone along the grain boundary could reduce the intergranular corrosion resistance of the alloy. Besides, the thin T 1 precipitates that were uniformly distributed within the grains did not suffer preferential dissolution, but they still affected the intragranular corrosion propagation at the nanoscale. Specifically, the corroded T 1 precipitates could become {111} Al-oriented sidewalls of the intragranular corrosion channel.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Fabrication methods to manufacture isotropic Al-Li alloys and products for space and aerospace applications10.1016/S0921-5093(98)00827-2 ↗
2. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
3. Development and characterization of Al–Li alloys10.1016/j.msea.2006.01.045 ↗
4. The evolution of Al-Li Base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
5. Recent developments in advanced aircraft aluminium alloys
6. Microstructure characteristics and constitutive modeling for elevated temperature flow behavior of Al–Cu–Li X2A66 alloy10.1557/jmr.2017.466 ↗
7. Hot deformation characterization of as-homogenized Al-cu-Li X2A66 alloy through processing maps and microstructural evolution10.1016/j.jmst.2019.06.001 ↗
8. Formation mechanism of precipitate T1 in AlCuLi alloys10.1016/j.jallcom.2014.10.208 ↗
9. Atomic structure of T1 precipitates in Al–Li–Cu alloys revisited with HAADF-STEM imaging and small-angle X-ray scattering10.1016/j.actamat.2010.09.044 ↗
10. A closer look at the role of Zn in the microstructure and corrosion of an Al-Cu-Li alloy10.1016/j.corsci.2018.10.003 ↗
11. Localized dissolution of grain boundary T1 precipitates in Al-3Cu-2Li10.1515/corrrev-2015-0032 ↗
12. Effects of aging time on corrosion behavior of an Al-Cu-Li alloy10.1016/j.corsci.2020.108759 ↗
13. The crystallographic corrosion and its microstructure in an Al-Cu-Li alloy10.1016/j.jallcom.2020.158588 ↗
14. The effect of thermo-mechanical treatment on the formation of T1 phase and δ′/θ’/δ′ composite precipitate in an Al-Cu-Li-Mg alloy10.1016/j.matchar.2021.111123 ↗
15. The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys10.1016/j.actamat.2012.12.041 ↗
16. Interfacial structure evolution of the growing composite precipitates in Al-Cu-Li alloys10.1016/j.actamat.2017.03.018 ↗
17. Li-atoms-induced structure changes of Guinier–Preston–Bagaryatsky zones in AlCuLiMg alloys10.1016/j.matchar.2016.09.037 ↗
18. Genetic structural phase evolution from Li-containing S-like phase precipitates towards S-phase in AlCuLiMg alloys10.1016/j.actamat.2022.117997 ↗
19. Simulation study on function mechanism of some precipitates in localized corrosion of Al alloys10.1016/j.corsci.2006.12.002 ↗
20. In-situ nanoscopic observations of dealloying-driven local corrosion from surface initiation to in-depth propagation10.1016/j.corsci.2020.108912 ↗
21. Correlation of intergranular corrosion behaviour with microstructure in Al-Cu-Li alloy10.1016/j.corsci.2018.05.011 ↗
22. Correlation between artificial aging and intergranular corrosion sensitivity of a new Al-Cu-Li alloy sheet10.1002/maco.201609090 ↗
23. Intergranular corrosion of Zn-free and Zn-microalloyed Al–xCu–yLi alloys10.1016/j.corsci.2016.01.001 ↗
24. Corrosion mechanism associated with T1 and T2 precipitates of Al–Cu–Li alloys in NaCl solution10.1016/j.jallcom.2007.06.072 ↗
25. Localized corrosion at nm-scale hardening precipitates in Al-Cu-Li alloys10.1016/j.actamat.2020.03.006 ↗
26. Corrosion behaviour of 2A97-T6 Al-Cu-Li alloy: the influence of non-uniform precipitation10.1016/j.corsci.2017.12.010 ↗
27. Investigation on formation mechanism of T1 precipitate in an Al-Cu-Li alloy10.1016/j.jallcom.2017.06.198 ↗
28. National standard of the People’’s Republic of China · 2005
29. Effect of aging on the mechanical properties and corrosion susceptibility of an Al-Cu-Li-Zr alloy containing Sc10.1016/S1001-0521(08)60105-9 ↗
30. Study of aging and electrochemical behaviour of Al-Li-Cu-Mg alloys10.1002/maco.201106409 ↗
31. Effect of aging treatment on microstructures, tensile properties and intergranular corrosion behavior of Al–Cu–Li alloy10.1016/j.matchar.2018.04.043 ↗
32. The influence of artificial ageing on the corrosion behaviour of a 2050 aluminium–copper–lithium alloy10.1016/j.corsci.2013.11.060 ↗
33. Effects of aging treatment on the intergranular corrosion behavior of Al–Cu–Mg–Ag alloy10.1016/j.jallcom.2015.03.174 ↗
34. Electrochemical studies on single-crystal aluminium surfaces10.1016/S0013-4686(97)00305-8 ↗
35. Pitting corrosion of Al and Al-Cu single crystals10.1149/1.2086291 ↗
36. Size-dependent role of S phase in pitting initiation of 2024Al alloy10.1016/j.corsci.2016.01.016 ↗
37. Unraveling the precipitate-induced discontinuity of the surface oxide film on Al alloy10.1016/j.apsusc.2022.153108 ↗