Mechanism of corrosion protection in reinforced Ti-6Al-4 V alloy by wire arc additive manufacturing using magnetic arc oscillation
Source abstract
Abstract
Large titanium component fabricated using Wire Arc Additive Manufacturing (WAAM) remains a challenge as it is difficult to obtain uniform material properties, such as corrosion resistance, for industrial applications. In this study, corrosion performance of Ti-6Al-4 V alloy that have been fabricated using WAAM with magnetic arc oscillations were fully explored by means of material characterization and electrochemical corrosion testing. Compared to stable arc, oscillated arc specimens impart superior corrosion resistance owing to refined α grains that bring substantial grain boundaries to produce copious ion position or reactive site, allowing for rapid formation of passive film which is insusceptible to chloride-induced localized attack. For typical α + β structure, lamellar α size plays a critical role in passive film generation, growth and dissolution in corrosive media. The research outcomes provide a better understanding of corrosion behavior for Ti-6Al-4 V alloy fabricated by WAAM, which will benefit further process design and improvement.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. A review on wire and arc additive manufacturing of titanium alloy10.1016/j.jmapro.2021.08.018 ↗
2. A practical path planning methodology for wire and arc additive manufacturing of thin-walled structures10.1016/j.rcim.2015.01.003 ↗
3. Low cost integration of additive and subtractive processes for hybrid layered manufacturing10.1016/j.rcim.2010.03.008 ↗
4. Enhanced corrosion performance in Ti-6Al-4V alloy produced via wire-arc directed energy deposition with magnetic arc oscillation
5. Effect of magnetic arc oscillation on the geometry of single-pass multi-layer walls and the process stability in wire and arc additive manufacturing10.1016/j.jmatprotec.2020.116723 ↗
6. Tailoring the surface finish, dendritic microstructure and mechanical properties of wire arc additively manufactured Hastelloy C276 alloy by magnetic arc oscillation
7. Electrochemical dissolution behavior of Ti6Al4V alloy: effect of microstructure and processing method10.1016/j.jmatprotec.2022.117646 ↗
8. Effect of zirconium content on the microstructure and corrosion behavior of Ti-6Al-4V-xZr alloys10.1016/j.corsci.2016.09.012 ↗
9. Distinction in corrosion resistance of selective laser melted Ti-6Al-4V alloy on different planes10.1016/j.corsci.2016.06.009 ↗
10. Improved corrosion behaviour of electron beam melted Ti-6Al–4V alloy in phosphate buffered saline10.1016/j.corsci.2017.05.003 ↗
11. Corrosion behavior of dual-phase Ti–6Al–4V alloys: a discussion on the impact of Fe content10.1016/j.jallcom.2020.157708 ↗
12. Effects of synchronized magnetic arc oscillation on microstructure, texture, grain boundary and mechanical properties of wire arc additively manufactured Ti6Al4V alloy
13. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
14. Corrosion behavior of selective laser melted Ti-6Al-4V alloy in NaCl solution10.1016/j.corsci.2015.10.041 ↗
15. Synergistic effect of chloride ion and Shewanella algae accelerates the corrosion of Ti-6Al-4V alloy10.1016/j.jmst.2020.07.022 ↗
16. Electrochemical behavior of open-cellular structured Ti-6Al-4V alloy fabricated by electron beam melting in simulated physiological fluid: the significance of pore characteristics10.1016/j.jmst.2021.05.024 ↗
17. Effect of stress-relief annealing on anodic dissolution behaviour of additive manufactured Ti-6Al-4V via laser solid forming10.1016/j.corsci.2019.04.002 ↗
18. Effect of surface treatment on electrochemical behavior of CP Ti, Ti–6Al–4V and Ti–13Nb–13Zr alloys in simulated human body fluid10.1016/j.corsci.2005.06.003 ↗
19. Phase angle analysis for stress corrosion cracking of carbon steel in fuel-grade ethanol: experiments and simulation10.1016/j.electacta.2010.07.024 ↗
20. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗
21. Corrosion resistance of Ti and Ti–Pd alloy in phosphate buffered saline solutions with and without H2O2 addition10.1016/S1003-6326(13)62541-8 ↗
22. Distinction in electrochemical behaviour of Ti6Al4V alloy produced by direct energy deposition and forging10.1016/j.jallcom.2020.157912 ↗
23. Effect of Nb addition on the stability and biological corrosion resistance of Ti-Zr alloy passivation films10.1016/j.corsci.2020.108696 ↗
24. In situ corrosion monitoring of Ti–6Al–4V alloy in H2SO4/HCl mixed solution using electrochemical AFM10.1016/j.electacta.2010.10.024 ↗
25. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
26. Distinction in anodic dissolution behavior on different planes of laser solid formed Ti-6Al-4V alloy10.1016/j.electacta.2018.07.112 ↗
27. Electrochemical behaviour of passive film formed on the surface of Ti-6Al-4V alloys fabricated by electron beam melting10.1016/j.corsci.2018.09.010 ↗
28. Electrochemical studies of the pitting corrosion of tin in citric acid solution containing Cl−10.1016/j.electacta.2008.01.051 ↗
29. Passivation characteristics of ultra-thin 316L foil in NaCl solutions10.1016/j.jmst.2022.01.043 ↗
30. The semiconducting properties of passive films formed on AISI 316 L and AISI 321 stainless steels: a test of the point defect model (PDM)10.1016/j.corsci.2011.05.063 ↗
31. Effects of competitive anion adsorption (Br− or Cl−) and semiconducting properties of the passive films on the corrosion behavior of the additively manufactured Ti–6Al–4V alloys10.1016/j.corsci.2020.108789 ↗
32. Performance of different microstructure on electrochemical behaviors of laser solid formed Ti–6Al–4V alloy in NaCl solution10.1016/j.corsci.2021.109392 ↗