Heterogeneous deformation-induced strengthening of extruded Tip/WE43 composites
Source abstract
Abstract
Titanium (Ti) particles reinforced WE43 (Mg-4Y-2Nd-1Gd-0.5Zr) matrix composites (Ti p /WE43) were prepared via ultrasonic-assisted stirring casting and following hot extrusion. Ti particles can refine the grains and promote the precipitation of the second phases in magnesium (Mg) matrix. Meanwhile, bimodal structures combining coarse deformed grains and recrystallization equiaxed grains were formed. The generation of heterogeneous interfaces promotes heterogeneous deformation-induced (HDI) strengthening. Extruded 3Ti p /WE43 with a yield strength (YS) of 241 MPa, an ultimate tensile strength (UTS) of 283 MPa, and an elongation (EL) of 17.3%, respectively, possesses an excellent strength–ductility combination. The interfacial product of Ti/Mg was mainly composed Ti 3 Al layer with about 200 nm, which was conducive to interfacial bonding and stress transfer. The dislocation entanglements and stacking faults inside the Ti particles can promote the coordinated deformation between the Mg matrix and Ti particles. The rare-earth rich phases Ti 2ZrAl, Mg 41Nd 5, and Mg 24Y 5 precipitated in the matrix can hinder dislocation movement by activating Orowan strengthening. The key factors of YS increment of the composites were considered to be HDI strengthening, fine grain strengthening, and thermal mismatch strengthening.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Research advances of magnesium and magnesium alloys worldwide in 202110.1016/j.jma.2022.04.001 ↗
2. Mechanical and biocorrosive properties of magnesium-aluminum alloy scaffold for biomedical applications10.1016/j.jmbbm.2019.06.022 ↗
3. Towards magnesium alloys for high-volume automotive applications10.1016/j.scriptamat.2016.07.035 ↗
4. Influence of Ti particle sizes on microstructure and mechanical behaviors of AZ91-Ti composites under different loading paths10.1016/j.msea.2023.145723 ↗
5. A review on ignition mechanisms and characteristics of magnesium alloys10.1016/j.jma.2019.11.014 ↗
6. Recent development in the fabrication of metal matrix-particulate composites using powder-metallurgy techniques10.1007/BF01154673 ↗
7. Hot extrusion of SiCp/AZ91 Mg matrix composites10.1016/S1003-6326(11)61407-6 ↗
8. Development of high performance magnesium nano-composites using nano-Al2O3 as reinforcement10.1016/j.msea.2004.09.047 ↗
9. Influence of micron-Ti and Nano-cu additions on the microstructure and mechanical properties of pure magnesium10.3390/met2030274 ↗
10. Microstructures and mechanical properties of titanium-reinforced magnesium matrix composites: review and perspective10.1016/j.jma.2022.07.008 ↗
11. Characterization of accumulative fold-forged magnesium-nickel multilayered composite structures10.1016/j.matchar.2020.110478 ↗
12. Improved mechanical proprieties of “magnesium based composites” with titanium–aluminum hybrids10.1016/j.jma.2014.12.010 ↗
13. Work hardening and softening behavior of Mg-Zn-Ca alloy influenced by deformable Ti particles10.1016/j.msea.2021.142336 ↗
14. Towards refining microstructures of biodegradable magnesium alloy WE43 by spark plasma sintering10.1016/j.actbio.2019.06.045 ↗
15. Effect of strain path on the evolution of microstructure, texture and tensile properties of WE43 alloy10.1016/j.msea.2018.01.018 ↗
16. Thermal stability of bimodal microstructure in magnesium alloy AZ91 processed by ECAP10.1016/j.matchar.2015.07.009 ↗
17. Effect of Y and Gd content on the microstructure and mechanical properties of Mg-Y-RE alloys10.1016/j.jma.2019.03.002 ↗
18. Titanium particulate reinforced AZ31 magnesium matrix composites with improved ductility prepared using friction stir processing10.1016/j.msea.2019.138793 ↗
19. Nanocrystalline Ti/AZ61 magnesium matrix composite: evolution of microstructure and mechanical property during annealing treatment10.1016/j.jallcom.2018.01.136 ↗
20. Effect of micron-Ti particles on microstructure and mechanical properties of Mg-3Al-1Zn based composites10.1016/j.msea.2021.142526 ↗
21. Mechanical properties and microstructural characteristics of Ti/ WE43 composites10.1016/j.vacuum.2022.111534 ↗
22. Strengthening mechanism and microstructure of deformable Ti particles reinforced AZ91 composite10.1007/s40195-022-01428-0 ↗
23. Preparation of NiTip/WE43 magnesium matrix composites by friction stir processing
24. Effect of particle size ratio and particle clustering on sintering and stiffness of aluminium matrix composite10.1179/174329006X113463 ↗
25. Mechanical behavior of particle reinforced metal matrix composites10.1002/1527-2648(200106)3:6<357::AID-ADEM357>3.0.CO;2-I ↗
26. An alternating ageing-annealing process for enhancing strength and ductility of a Mg-Gd-Y-Zn-Zr alloy10.1016/j.msea.2021.142103 ↗
27. Enhanced overall strength and ductility of magnesium matrix composites by low content of graphene nanoplatelets10.1016/j.compositesa.2017.05.011 ↗
28. Exploring mechanical behavior of Mg-6Zn alloy reinforced with graphene nanoplatelets10.1016/j.msea.2015.10.009 ↗
29. Effect of rotary swaging on the microstructure and mechanical properties of high-strength Mg-Mn-Al-Ca-Zn alloys10.1016/j.matchar.2022.112575 ↗
30. High strength and deformation stability achieved in CrCoNi alloy containing deformable oxides10.1016/j.jmst.2022.06.026 ↗
31. Deformation and fracture behavior of Mg alloy, WE43, after various aging heat treatments10.1016/j.msea.2017.08.067 ↗
32. Effect of Ti-6Al-4V particle reinforcements on mechanical properties of Mg-9Al-1Zn alloy10.1016/S1003-6326(22)66016-3 ↗
33. Additive manufactured WE43 magnesium: a comparative study of the microstructure and mechanical properties with those of powder extruded and as-cast WE4310.1016/j.matchar.2018.11.011 ↗
34. In-vitro characterization of stress corrosion cracking of aluminium-free magnesium alloys for temporary bio-implant applications10.1016/j.msec.2014.06.018 ↗
35. Superior properties of Mg-4Y-3RE-Zr alloy prepared by powder metallurgy10.1016/j.jmst.2016.09.019 ↗
36. Biocorrosion properties of as-extruded Mg-Nd-Zn-Zr alloy compared with commercial AZ31 and WE43 alloys10.1016/j.matlet.2011.08.079 ↗
37. Enhancing the strength and ductility in accumulative back extruded WE43 magnesium alloy through achieving bimodal grain size distribution and texture weakening10.1016/j.msea.2017.04.098 ↗
38. Combining gradient structure and supersaturated solid solution to achieve superior mechanical properties in WE43 magnesium alloy10.1016/j.jmst.2021.04.074 ↗
39. The influence of extrusion process on the microstructure and mechanical properties of magnesium alloys10.1515/amm-2017-0080 ↗
40. Effect of aggressive ions on degradation of WE43 magnesium alloy in physiological environment10.1016/S1452-3981(23)07718-0 ↗
41. Development and characteristics of a low rare-earth containing magnesium alloy with high strength-ductility synergy10.1016/j.jma.2022.01.005 ↗
42. Microstructure and mechanical properties of equal channel angular pressed Mg-Y-RE-Zr alloy10.1080/02670836.2015.1104021 ↗
43. Microstructure, mechanical properties and fracture behavior of a new WE43 alloy10.1007/s12598-020-01423-3 ↗
44. Microstructures and mechanical properties of the age hardened Mg–4.2Y–2.5Nd–1Gd–0.6Zr (WE43) microalloyed with Zn10.1016/j.jma.2014.01.010 ↗
45. Effect of pre-deformation on microstructure and mechanical properties of WE43 magnesium alloy II: aging at 250 and 300 degrees C10.1016/j.jma.2019.11.012 ↗
46. Microstructure, mechanical properties and fracture behaviors of large-scale sand-cast Mg-3Y-2Gd-1Nd-0.4Zr alloy10.1016/j.jma.2021.08.010 ↗
47. Effect of microstructure on tensile and compressive behavior of WE43 alloy in as cast and heat treated conditions10.1016/j.msea.2017.10.084 ↗
48. Additive manufacturing of dense WE43 Mg alloy by laser powder bed fusion
49. Applying multi-pass friction stir processing to refine the microstructure and enhance the strength, ductility and corrosion resistance of WE43 magnesium alloy10.1016/j.jmrt.2021.03.021 ↗
50. Increasing strength and ductility of magnesium alloy WE43 by equal-channel angular pressing10.1016/j.msea.2017.12.026 ↗
51. Optimising the torsional properties and corrosion resistance of biodegradable WE43 Mg alloy by ECAP and subsequent ageing10.1080/10667857.2019.1688539 ↗
52. Mechanical properties of a Mg-10 (vol.%)Ti composite10.1016/S0266-3538(03)00215-X ↗
53. Fabrication, microstructure and mechanical properties of Mg matrix composites reinforced by high volume fraction of sphere TC4 particles10.1016/j.jma.2016.10.003 ↗
54. Dynamic precipitation and deformation behaviors of a bimodal-grained WE43 alloy with enhanced mechanical properties10.1016/j.ijplas.2023.103682 ↗
55. Architecture design strategies and strengthening-toughening mechanisms of metal matrix composites
56. Heterostructured materials: superior properties from hetero-zone interaction10.1080/21663831.2020.1796836 ↗
57. Heterostructured metallic materials: plastic deformation and strain hardening
58. Microstructure and mechanical properties in Al-Mg-Sc alloy induced by hetero-deformation10.1016/j.matchar.2021.111622 ↗
59. Bulk nanocrystalline high-strength magnesium alloys prepared via rotary swaging10.1016/j.actamat.2020.09.024 ↗
60. Synergistic effects of hybrid (SiC+TiC) nanoparticles and dynamic precipitates in the design of a high-strength magnesium matrix nanocomposite10.1016/j.matchemphys.2020.124048 ↗
61. A TEM quantitative evaluation of strengthening in an Mg–RE alloy reinforced with SiC10.1016/j.matchar.2011.04.011 ↗
62. Development of ductile magnesium composite materials using titanium as reinforcement10.1016/S0925-8388(02)00413-9 ↗
63. Back stress strengthening and strain hardening in gradient structure10.1080/21663831.2016.1153004 ↗
64. Strengthening-toughening mechanism and mechanical properties of span-scale Heterostructure high-entropy alloy