Combined factors for enhanced high-temperature strength of Al-Mn-Cr heat-resistant alloy fabricated using laser-based powder bed fusion
Source abstract
Abstract
A newly designed heat-resistant Al-8mass%Mn-2mass%Cr alloy (Al-8Mn-2Cr) was fabricated using a laser-based powder bed fusion (PBF-LB). The Vickers hardness of the Al-8Mn-2Cr PBF-LB samples drastically increased after aging heat treatments, and the aged samples exhibited excellent high-temperature strengths at ≥250 °C. Both the as-built and aged samples possessed coarse columnar crystal grains with a strong texture of 〈001〉 parallel to the stacking direction. The manganese and chromium solutes in the as-built samples were supersaturated in an α-Al phase owing to the rapid solidification by laser melting. Most manganese and chromium supersaturated in the α-Al solid solution remained even after aging, although they were precipitated partially into the Al 6Mn and Al 7Cr phases at cell boundaries. The quantitative analysis of the strengths based on the microstructural observation demonstrated that the dominant reinforcement factors for both the as-built and aged Al-8Mn-2Cr PBF-LB samples were solid-solution strengthening by supersaturated manganese and chromium and grain boundary strengthening. Dispersion strengthening by the Al 6Mn and Al 7Cr precipitations through the Orowan mechanism was additionally effective in the aged samples. Moreover, the coarse columnar crystal grains with a strong texture might suppress creep-like grain boundary sliding at ≥250 °C, thus preventing deterioration in the high-temperature strengths.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Milewski · 2017 · 7
2. Aluminum alloy for additive manufacturing in automotive production10.1007/s38311-020-0285-y ↗
3. Additive manufacturing of aluminum alloys: augmenting or competing with traditional manufacturing?
4. Sun · 2017 · 55
5. Compressive properties of Al-Si alloy lattice structures with three different unit cells fabricated via laser powder bed fusion10.3390/ma13132902 ↗
6. Achieving superior mechanical properties of selective laser melted AlSi10Mg via direct aging treatment10.1016/j.jmst.2021.07.059 ↗
7. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
8. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: comparison between virgin and recycled powders10.1016/j.addma.2018.07.014 ↗
9. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: the effect of a conventional T6-like heat treatment10.1016/j.msea.2016.04.092 ↗
10. Selective laser melting of AlSi10Mg alloy: process optimization and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
11. Control of microstructural characteristics and mechanical properties of AlSi12 alloy by processing conditions of laser powder bed fusion
12. Effect of energy per layer on the anisotropy of selective laser melted AlSi12 aluminium alloy10.1016/j.addma.2018.05.040 ↗
13. Defining the tensile properties of AlSi12 parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
14. Comparative thermal fatigue behavior of AlSi7Mg alloy produced by L-PBF and sand casting10.1016/j.ijfatigue.2021.106424 ↗
15. Effects of annealing on the microstructure and mechanical properties of selective laser melted AlSi7Mg alloy10.1016/j.msea.2018.10.047 ↗
16. The influence of processing parameters on aluminium alloy A357 manufactured by selective laser melting10.1016/j.matdes.2016.07.009 ↗
17. Rapid solidification: selective laser melting of AlSi10Mg
18. Parametric analysis of thermal behavior during selective laser melting additive manufacturing of aluminum alloy powder10.1016/j.matdes.2014.07.006 ↗
19. Microstructures and mechanical properties of aluminum-transition metal binary alloys (Al-Fe, Al-Mn, and Al-Cr) processed by laser powder bed fusion10.1016/j.jallcom.2021.159680 ↗
20. Microstructures and mechanical properties of A356 (AlSi7Mg0.3) aluminum alloy fabricated by selective laser melting10.1016/j.matdes.2015.10.065 ↗
21. Microstructural development and aging behavior of Al-Cr-Zr heat-resistant alloy fabricated using laser powder bed fusion10.1016/j.jmrt.2021.10.027 ↗
22. Thermal and mechanical properties of commercial-purity aluminum fabricated using selective laser melting10.2320/matertrans.L-M2017809 ↗
23. Phase diagrams (Al-Mn-Cr, Al-Si-Mg)
24. Effects of manganese contents in solid solution and microstructures on creep behavior of 3003 aluminum alloy extrusions10.2464/jilm.52.417 ↗
25. Formation of a quasicrystalline phase in Al–Mn base alloys cast at intermediate cooling rates10.1007/s10853-017-1011-z ↗
26. Mondolfo · 1976 · 483
27. The structure of the intermetallic phase θ(Cr-Al)10.1107/S0365110X60000571 ↗
28. The interface response-functions in multi-componental alloy solidification10.1016/S0167-2789(98)00202-4 ↗
29. Microstructure of selective laser melted AlSi10Mg alloy10.1016/j.matdes.2019.107677 ↗
30. Texture of metals
31. Columnar to equiaxed transition in solidification processing10.1016/S1468-6996(01)00047-X ↗
32. Grain refinement of aluminum casting alloy by heterogeneous nucleation sites with smaller lattice disregistry10.2464/jilm.64.157 ↗
33. A review on additive manufacturing of Al–cu (2xxx) aluminium alloys, processes and defects10.1080/02670836.2021.1958487 ↗
34. Effect of silicon content on densification, mechanical and thermal properties of Al-xSi binary alloys fabricated using selective laser melting10.1016/j.msea.2016.11.059 ↗
35. Hot shortness of the aluminum-silicon alloys of commercial purity
36. Methods for estimation of solute concentration in aluminum alloys10.2464/jilm.50.518 ↗
37. The effect of microstructure and composition on the properties of vapour quenched Al-Cr alloys – II. Tensile properties10.1016/0001-6160(87)90027-7 ↗
38. Structural evolution of rapidly solidified Al–Mn and Al–Mn–Sr alloys10.1016/j.msea.2006.05.017 ↗
39. Selective laser melting of a high strength Al-Mn-Sc alloy: alloy design and strengthening mechanism10.1016/j.actamat.2019.04.014 ↗
40. Quantitative size-factors for metallic solid solutions10.1007/BF00549722 ↗
41. Microstructure and properties of a high temperature Al-Ce-Mn alloy produced by laser additive manufacturing10.1016/j.actamat.2020.07.014 ↗
42. Microstructure and mechanical properties of Al-mg-Zr alloys processed by selective laser melting10.1016/j.actamat.2018.04.053 ↗
43. Strengthening of an Al–Cu–Sn alloy by deformation-resistant precipitate plates10.1016/j.actamat.2008.03.028 ↗
44. The effect of microstructure and composition on the properties of vapour quenched Al-Cr alloys II. Tensile properties10.1016/0001-6160(87)90027-7 ↗
45. On the strength of discontinuous silicon carbide reinforced aluminum composites10.1016/0036-9748(86)90210-3 ↗
46. R. A. Michi, A. Plotkowski, A. Shyam, R. R. Dehoff, S. S. Babu, Towards high-temperature applications of aluminium alloys enabled by additive manufacturing. Int. Mater. Rev., DOI: https://doi.org/10.1080/09506608.2021.1951580.10.1080/09506608.2021.1951580 ↗
47. Constitution in the solid state of aluminum rich alloys in the Al-Mn-Cr ternary system10.2464/jilm.22.8_504 ↗
48. Some observations of grain boundary sliding in the presence of second phase particles10.1016/0001-6160(72)90002-8 ↗
49. Effect of grain size on creep properties of type 316LN stainless steel10.1007/BF03026948 ↗
50. Heat resisting steels and superalloys10.2464/jilm.36.851 ↗
51. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
52. High temperature cleavage fracture in 5383 aluminum alloy10.1016/S0921-5093(01)01091-7 ↗
53. Intergranular fracture caused by trace impurities in an Al–5.5 Mol% mg alloy10.1016/S1359-6454(01)00291-9 ↗
54. Intergranular fracture at elevated temperature10.1016/0001-6160(75)90047-4 ↗
55. Three dimensional constitutive relations and ductile fracture