Abstract

Strength-ductility trade-off is an enduring problem in a wide range of metals and alloys including the advanced high-strength steels. In this work, we propose a novel non-isothermal low-temperature warm rolling (WR) treatment which was applied after the conventional intercritical annealing (IA) in order to overcome the strength-ductility compromise in a medium manganese steel, Fe-5.1Mn-0.22C-0.85Si-0.42Al (composition in wt%). IA + WR treatment yielded a simultaneous improvement in tensile properties, wherein yield strength (YS), ultimate tensile strength (UTS), and ductility improved by 32%, 12%, and 6% respectively, compared to the conventional IA treatment. Despite an increase in the yield point elongation (2%) and Lüders strain (3%) in the IA + WR specimen, the ductility of the same improved as compared to the IA specimen. Microstructure of the IA + WR specimen was tailored by introducing a significantly higher dislocation density in the constituent ferrite and retained austenite (RA) phases along with a relatively higher density of planar defects (stacking faults and nano-twins) in the RA phase. X-ray line profile analysis quantified the increased dislocation density (order ∼10 15 vs 10 14 m −2) and twin fault probability (∼1.35% vs ∼0.12%) in the RA phase of the IA + WR compared to the IA specimen. The improvement in YS was primarily due to the increase in the dislocation density of the constituent phases in the IA + WR specimen. Introduction of a high density of lattice defects in the RA phase during the WR treatment above the M d 30 temperature enhanced the mechanical stability of the RA phase, leading to a decreased rate of TRIP effect and formation of hierarchical twins during tensile deformation. The near-ubiquitous strength-ductility trade-off was overcome via a tailored microstructure consisting of regulated austenite stability leading to discontinuous TRIP effect, hierarchical twinning in RA phase, and favorable texture in the constituent phases. The present study provides a pathway to tailor the microstructure for escaping the strength-ductility paradox in different metastable FCC alloys such as stainless steel, HEAs, TWIP steels etc.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
2. Materials, design and manufacturing for lightweight vehicles
3. Recent progress in medium-Mn steels made with new designing strategies, a review10.1016/j.jmst.2017.06.017 ↗
4. 112: the cyclic properties of engineering materials10.1016/0956-7151(94)90493-6 ↗
5. Retaining ductility10.1038/nmat1141 ↗
6. The conflicts between strength and toughness10.1038/nmat3115 ↗
7. Stacking fault energy of austenite phase in medium manganese steel10.1007/s11661-019-05367-x ↗
8. High strength Fe–Mn–(Al, Si) TRIP/TWIP steels development — properties — application10.1016/S0749-6419(00)00015-2 ↗
9. Effect of the strain rate on the TRIP–TWIP transition in austenitic Fe-12 pct Mn-0.6 pct C TWIP steel10.1007/s11661-013-2028-9 ↗
10. Observation of the TWIP + TRIP plasticity-enhancement mechanism in Al-added 6 Wt Pct medium Mn steel10.1007/s11661-015-2854-z ↗
11. Critical assessment of the strain-rate dependent work hardening behaviour of AISI 304 stainless steel10.1016/j.msea.2020.140675 ↗
12. Austenite stability effects on tensile behavior of manganese-enriched-austenite transformation-induced plasticity steel10.1007/s11661-011-0687-y ↗
13. Austenite stability and its effect on the ductility of the cold-rolled medium-Mn steel10.2355/isijinternational.54.1952 ↗
14. Design of a novel Mn-based 1 GPa duplex stainless TRIP steel with 60% ductility by a reduction of austenite stability10.1016/j.actamat.2011.04.011 ↗
15. On the intercritical annealing parameters and ensuing mechanical properties of low-carbon medium-Mn steel10.1016/j.msea.2018.07.055 ↗
16. Hot rolled and cold rolled medium manganese steel: mechanical properties and microstructure10.1016/j.msea.2017.06.088 ↗
17. Deformation mechanisms for a new medium-Mn steel with 1.1 GPa yield strength and 50% uniform elongation10.1016/j.jmst.2022.05.048 ↗
18. Effect of pre-existed austenite on austenite reversion and mechanical behavior of an Fe-0.2C-8Mn-2Al medium Mn steel10.1016/j.actamat.2018.01.009 ↗
19. Evolution of microstructure and deformation behavior in Al–Ni added medium-Mn steel processed through intercritical / cold rolling and annealing10.1016/j.msea.2021.141852 ↗
20. Microstructure-mechanical property evaluation and deformation mechanism in Al added medium Mn steel processed through intercritical rolling and annealing10.1016/j.msea.2020.140100 ↗
21. Effect of prior austenite grain size on the evolution of microstructure and mechanical properties of an intercritically annealed medium manganese steel10.1016/j.msea.2019.138458 ↗
22. The size effect of initial martensite constituents on the microstructure and tensile properties of intercritically annealed Fe–9Mn–0.05C steel10.1016/j.msea.2015.02.075 ↗
23. Adjusting the microstructure evolution, mechanical properties and deformation behaviors of Fe-5.95Mn-1.55Si-1.03Al-0.055C medium Mn steel by cold-rolling reduction ratio10.1016/j.jmrt.2019.11.058 ↗
24. Effect of cold deformation extent and ART annealing duration on the microstructure and mechanical properties of a medium manganese steel10.1016/j.matchemphys.2021.124940 ↗
25. Tailoring hetero-grained austenite via a cyclic thermomechanical process for achieving ultrahigh strength-ductility in medium-Mn steel10.1016/j.scriptamat.2022.114767 ↗
26. Enhancing strength–ductility synergy in medium Mn steel with hetero-structured austenite developed by two-stage cyclic thermomechanical treatment and flash annealing10.1016/j.scriptamat.2022.115196 ↗
27. Resetting the austenite stability in a medium Mn steel via dislocation engineering10.1007/s11661-019-05222-z ↗
28. Analysis of medium manganese steel through cold-rolling and intercritical annealing or warm-rolling10.1080/02670836.2018.1463613 ↗
29. Super-high-strength and formable medium Mn steel manufactured by warm rolling process10.1016/j.actamat.2019.05.043 ↗
30. Effect of warm rolling process on microstructures and tensile properties of 10 Mn steel10.1016/j.jmst.2019.12.026 ↗
31. Microstructural evolution and strain hardening behavior of a novel two-stage warm rolled ultra-high strength medium Mn steel with heterogeneous structures10.1016/j.ijplas.2022.103212 ↗
32. High strength-toughness combination of a low-carbon medium-manganese steel plate with laminated microstructure and retained austenite10.1016/j.msea.2017.09.059 ↗
33. Thermo-Calc and DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
34. BL-02: a versatile X-ray scattering and diffraction beamline for engineering applications at Indus-2 synchrotron source10.1107/S1600577521004690 ↗
35. Texture analysis with MTEX- free and open source software toolbox
36. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
37. Correlation between strength and microstructure of ball-milled Al–mg alloys determined by X-ray diffraction10.1016/j.msea.2004.01.089 ↗
38. Cullity · 1956
39. Austenite stabilization through manganese enrichment10.1016/j.scriptamat.2010.09.040 ↗
40. Empirical formulae for the calculation of some transformation temperatures
41. A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels10.1016/0001-6160(59)90170-1 ↗
42. The relative contributions of TWIP and TRIP to strength in fine grained medium-Mn steels10.1016/j.msea.2022.143864 ↗
43. Intercritical tempering enables nanoscale austenite/ε-martensite formation in low-C medium-Mn steel: a pathway to control mechanical properties10.1016/j.msea.2018.08.082 ↗
44. Microstructure and mechanical properties of Fe–0.2C–5Mn steel processed by ART-annealing10.1016/j.msea.2011.05.039 ↗
45. Time-evolution of microstructure and mechanical behaviour of double annealed medium Mn steel10.1080/02670836.2019.1585031 ↗
46. Deformation microstructures and strengthening mechanisms of an ultrafine grained duplex medium-Mn steel10.1016/j.msea.2012.11.044 ↗
47. Enhanced work-hardening behavior and mechanical properties in ultrafine-grained steels with large-fractioned metastable austenite10.1016/j.scriptamat.2010.06.023 ↗
48. Excellent Total mechanical-properties-balance of 5% Mn, 30000 MPa% steel10.2355/isijinternational.51.685 ↗
49. Localized deformation in multiphase, ultra-fine-grained 6 Pct Mn transformation-induced plasticity steel10.1007/s11661-011-0636-9 ↗
50. Experimental and numerical analysis on formation of stable austenite during the intercritical annealing of 5Mn steel10.1016/j.actamat.2011.03.025 ↗
51. Austenite transformation and work hardening of medium manganese steel10.1007/s42243-018-0176-2 ↗
52. Intercritical annealing response of medium manganese steels having different carbon concentrations10.1002/srin.201800069 ↗
53. Interplay between reversed austenite and plastic deformation in a directly quenched and intercritically annealed 0.04C-5Mn low-Al steel10.1016/j.jallcom.2016.11.046 ↗
54. Austenite stability and its effect on the toughness of a high strength ultra-low carbon medium manganese steel plate10.1016/j.msea.2016.07.104 ↗
55. Microstructures and mechanical properties of the third generation automobile steels fabricated by ART-annealing10.1007/s11431-012-4877-7 ↗
56. Heat treatment effects on the microstructure and mechanical properties of a medium manganese steel (0.2C–5Mn)10.1016/j.msea.2011.11.009 ↗
57. Microstructure and mechanical properties of Fe–0.2C–5Mn steel processed by ART-annealing10.1016/j.msea.2011.05.039 ↗
58. Flash annealing yields a strong and ductile medium Mn steel with heterogeneous microstructure10.1016/j.scriptamat.2021.113819 ↗
59. Gubicza · 2014
60. An experimental investigation of extrapolation methods in the derivation of accurate unit-cell dimensions of crystals10.1088/0959-5309/57/3/302 ↗
61. Texture formation in metal alloys with cubic crystal structures10.1080/02670836.2016.1231746 ↗
62. Novel observation of dominant role of strain rate over stain during pre-straining on corrosion behaviour of 304L austenitic stainless steel10.1016/j.matchemphys.2021.125522 ↗
63. Effect of texture on corrosion behavior of AISI 304L stainless steel10.1016/j.matchar.2004.11.004 ↗
64. Effect of microstructure on corrosion behavior of medium manganese steel10.1016/j.matlet.2022.133344 ↗
65. Transformation textures in steels10.1179/095066090790324046 ↗
66. Recrystallization behaviour and tensile properties of Al-added medium-Mn-steel at different deformation-annealing conditions10.1080/02670836.2018.1560987 ↗
67. Effect of MnS inclusion and crystallographic texture on anisotropy in charpy impact toughness of low carbon ferritic steel10.1016/j.msea.2015.12.047 ↗
68. On prominent TRIP effect and non-basal slip in a TWIP high entropy alloy during high-pressure torsion processing10.1016/j.matchar.2021.111284 ↗
69. Simultaneous occurrence of twinning and phase transformation during yield point elongation in medium manganese steels10.1007/s11661-022-06879-9 ↗
70. Dependence of tensile deformation behavior of TWIP steels on stacking fault energy, temperature and strain rate10.1016/j.actamat.2010.05.049 ↗
71. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe–Mn–C alloys10.1016/j.msea.2004.01.059 ↗
72. The influence of alloying, temperature, and related effects on the stacking fault energy10.1007/BF03038370 ↗
73. Revisiting stacking fault energy of steels10.1007/s11661-015-3266-9 ↗
74. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
75. On the mechanical stability of austenite matrix after Martensite formation in a medium Mn steel10.1007/s11661-016-3502-y ↗
76. Dieter · 1988
77. Tensile behavior of Intercritically annealed 10 pct Mn multi-phase steel10.1007/s11661-013-2047-6 ↗
78. Multiple deformation mechanisms induced by pre-twinning in CoCrFeNi high entropy alloy10.1016/j.scriptamat.2021.114266 ↗
79. The effect of grain size and grain orientation on deformation twinning in a Fe–22 wt.% Mn–0.6 wt.% C TWIP steel10.1016/j.msea.2010.02.041 ↗
80. Development and control of annealing textures in low-carbon steels10.1179/imtr.1984.29.1.25 ↗