Interfacial characteristics of austenitic 316 L and martensitic 15–5PH stainless steels joined by laser powder bed fusion
Source abstract
Abstract
Laser powder bed fusion (LPBF) is an additive manufacturing (AM) technology capable of producing complex geometry components from a range of metals and alloys. The static mechanical strength of LPBF manufactured materials can rival that of the equivalent cast and wrought materials, but are more susceptible to fatigue failures due to stress concentrating roughness and porosity defects. The ability to process and join multiple powder materials within a single LPBF build process is an emerging capability that is now becoming commercially available. This new capability offers the possibility of compositional complexity, in addition to the geometric complexity offered by AM, and can help to eliminate the need for additional processing to join different materials. This study focuses on the combination of 316 L austenitic stainless steel (SS) and precipitation hardening 15–5PH martensitic SS by LPBF. The interfacial characteristics and microhardness variation at the interface were investigated by optical microscopy, scanning electron microscopy, energy dispersive spectroscopy, electron backscatter diffraction, and microhardness testing. Good apparent bonding was observed at the interface without any visible cracks or defects. A finer-grain region was observed at a distance of 115 μm below the interface with a grain size of about 25% of that in the surrounding 15–5PH SS. A narrow compositional transition distance of 7 μm along the building direction (less than the 30 μm LPBF layer thickness) and a wavey-morphology interface with an amplitude of about 66 μm (about twice the LPBF layer thickness) were found. A sharp change of hardness was measured within ±200 μm from the interface. Regions far from the interface exhibited similar microstructure and hardness as the corresponding single material components. The results suggest that LPBF joining between 316 L SS and 15–5PH SS can achieve each material's distinct microstructure and properties at far-interface regions, with a narrow wavey region (∼115 μm) at the interface that exhibits high densification and a sharp transition in microstructure and properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. Laser melting functionally graded composition of Waspaloy® and zirconia powders10.1007/s10853-007-1661-3 ↗
2. Göbel · 2010
3. Customized smartness: a survey on links between additive manufacturing and sensor integration10.1016/j.protcy.2016.08.038 ↗
4. Laser welding of dissimilar metal combinations10.1007/BF00361499 ↗
5. Layer architecture and fatigue life of ultrafine-grained laminated metal composites consisting of different aluminum alloys10.1016/j.msea.2017.06.105 ↗
6. Effect of rotation speed on the microstructure and mechanical properties of dissimilar friction stir-welded copper/brass metals
7. Recent progress and scientific challenges in multi-material additive manufacturing via laser-based powder bed fusion10.1080/17452759.2021.1928520 ↗
8. Zhong · 2017
9. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
10. Precipitation hardening stainless steel produced by powder bed fusion: influence of positioning and heat treatment
11. A comparative study of microstructure and high-temperature mechanical properties of 15-5 PH stainless steel processed via additive manufacturing and traditional manufacturing10.1007/s40964-018-0051-5 ↗
12. Influence mechanism of process parameters on the interfacial characterization of selective laser melting 316L/CuSn1010.1016/j.msea.2020.139316 ↗
13. Dual interfacial characterization and property in multi-material selective laser melting of 316L stainless steel and C52400 copper alloy10.1016/j.matchar.2020.110489 ↗
14. Interfacial characterization and mechanical properties of 316L stainless steel/inconel 718 manufactured by selective laser melting10.1016/j.msea.2019.05.011 ↗
15. Multi-material selective laser melting of Fe/Al-12Si components10.1016/j.mfglet.2017.01.002 ↗
16. The application of electron beam welding for the joining of dissimilar metals: an overview10.1016/0924-0136(95)02150-7 ↗
17. The effect of intermetallics on the strength properties of diffusion bonds formed between Ti–5.5 Al–2.4 V and 304 stainless steel10.1016/S0921-5093(03)00649-X ↗
18. Laser cladding of martensitic stainless steels on armor steels
19. Van Rooyen · 2006
20. Dissimilar welding of austenitic and martensitic stainless steel joints for nuclear applications: A review
21. Fatigue performance of additive manufactured metallic parts10.1108/13552541311302932 ↗
22. Fatigue crack propagation behavior in the vicinity of an interface between materials with different yield stresses10.1016/S0921-5093(00)00703-6 ↗
23. Brothers
24. Additive · 2020 · 316L
25. Additive
26. ASTM B962-17 · 2017
27. NIH image to ImageJ: 25 years of image analysis10.1038/nmeth.2089 ↗
28. Suwas · 2014
29. BS EN ISO 6507-1 · 2018
30. BS EN ISO 6892-1 · 2016
31. ASTM E8/E8M-13a · 2013
32. Microstructural characterization of 15-5PH stainless steel processed by laser powder-bed fusion
33. High-throughput experimentation for microstructural design in additively manufactured 316L stainless steel10.1016/j.msea.2020.139841 ↗
34. Mechanical behavior of selective laser melted 316L stainless steel10.1016/j.msea.2017.04.058 ↗
35. Scaling laws for the additive manufacturing10.1016/j.jmatprotec.2018.02.034 ↗
36. A comparative analysis of laser additive manufacturing of high layer thickness pure Ti and Inconel 718 alloy materials using finite element method10.3390/ma14040876 ↗
37. Influence of warm oxide layer on wettability and contact angle for heat transport devices
38. Optimization of process parameter and Additive simulation for fatigue strength development by selective laser melting of AlSi10Mg alloy
39. Defect formation mechanisms in selective laser melting: a review10.1007/s10033-017-0121-5 ↗
40. AZoM
41. Intragranular cellular segregation network structure strengthening 316L stainless steel prepared by selective laser melting10.1016/j.jnucmat.2015.12.034 ↗
42. A comparison of the tensile, fatigue, and fracture behavior of Ti–6Al–4V and 15-5 PH stainless steel parts made by selective laser melting10.1007/s00170-013-5106-7 ↗
43. Selective laser melting and heat treatment of precipitation hardening stainless steel with a refined microstructure and excellent mechanical properties10.1016/j.scriptamat.2019.10.040 ↗
44. Texture evolution in selective laser melted maraging stainless steel CX with martensitic transformation10.1007/s10853-020-05290-2 ↗
45. Microstructure and mechanical properties of stainless steel 316L vertical struts manufactured by laser powder bed fusion process10.1016/j.msea.2018.08.069 ↗
46. The orientation relationship between lath martensite and austenite in low carbon, low alloy steels10.1016/0956-7151(90)90180-O ↗
47. The effect of grain boundary structure on sensitization behavior in a nickel-based superalloy10.1007/s10853-018-2919-7 ↗
48. Role of dendrite branching and growth kinetics in the formation of low angle boundaries in Ni–base superalloys10.1016/j.msea.2005.09.030 ↗
49. Effects of heat treatment on microstructure, mechanical and corrosion properties of 15-5 PH stainless steel parts built by selective laser melting process10.1016/j.jmapro.2019.12.048 ↗
50. Effects of heat treatment and build orientations on the fatigue life of selective laser melted 15-5 PH stainless steel10.1016/j.msea.2019.04.003 ↗
51. Effects of process time interval and heat treatment on the mechanical and microstructural properties of direct laser deposited 316L stainless steel10.1016/j.msea.2015.07.056 ↗
52. Effect of scanning strategy on the microstructure, texture, and mechanical properties of 15-5PH stainless steel processed by selective laser melting10.1016/j.matchar.2021.111012 ↗
53. Fatigue crack growth in IN718/316L multi-materials layered structures fabricated by laser powder bed fusion10.1016/j.ijfatigue.2021.106454 ↗
54. Interfacial characterization of SLM parts in multi-material processing: metallurgical diffusion between 316L stainless steel and C18400 copper alloy10.1016/j.matchar.2014.05.001 ↗
55. Inline additively manufactured functionally graded multi-materials: microstructural and mechanical characterization of 316L parts with H13 layers10.1007/s40964-018-0044-4 ↗
56. Additive manufacturing of maraging steel-H13 bimetals using laser powder bed fusion technique
57. Studies on energy penetration and Marangoni effect during laser melting process
58. Marangoni flow at the gas/melt interface of steel10.1007/s11663-003-0015-z ↗
59. Molten pool behaviour and its physical mechanism during selective laser melting of TiC/AlSi10Mg nanocomposites: simulation and experiments10.1088/0022-3727/48/3/035303 ↗
60. Enhancing the corrosion resistance of selective laser melted 15-5PH martensite stainless steel via heat treatment10.1016/j.corsci.2019.108427 ↗
61. In situ tempering of Martensite during laser powder bed fusion of Fe-0.45 C steel10.1016/j.mtla.2022.101459 ↗
62. Outstanding improvement in the CSL distribution in interstitial free (IF) steel via strain annealing route10.1016/j.matchar.2022.111817 ↗
63. Nitrogen effects in additively manufactured martensitic stainless steels: conventional thermal processing and comparison with wrought10.1007/s11661-020-05703-6 ↗
64. Grain refinement in laser powder bed fusion: the influence of dynamic recrystallization and recovery10.1016/j.matdes.2020.109181 ↗
65. Effect of homogenization on precipitation behavior and strengthening of 17-4PH stainless steel fabricated using laser powder bed fusion
66. Evolution of microstructure and impact-strength energy in thermally and thermomechanically aged 15-5 PH