Effects of Sc microalloying on mechanical properties and corrosion resistance of FSW joints of spray formed 7055 aluminum alloy
Source abstract
Abstract
The joint strength and corrosion resistance of spray formed Al-Zn-Mg-Cu alloy usually decrease after friction stir welding (FSW). In this study, a small amount of Sc (0.2 wt%) was added to improve the yield strength of the spray formed Al-8.02Zn-2.05 Mg-2.4Cu-0.12Zr (wt%) FSW joint while reducing the corrosion sensitivity. After adding Sc, the tensile strength of the joint increased by 38 MPa, the yield strength increased by 32 MPa and the elongation increased by 0.9 % under the fine grain strengthening effect of Al 3(Sc,Zr) phase and Orowan strengthening effect. Sc refines the grains in the heat-affected zone (HAZ), reduces the precipitation of intergranular phases, reduces the width of precipitate-free zone (PFZ), and retains more low-angle grain boundaries (LAGB) in the alloy. Therefore, the corrosion potential increased from −0.97 V SCE to −0.87 V SCE, the corrosion current density decreased from 2.82 μA·cm −2 to 2.29 μA·cm −2, and the intergranular corrosion depth decreased from 31.39 μm to 18.81 μm.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. The effect of minor scandium addition on microstructure evolution and mechanical properties of spray formed Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2023.169710 ↗
2. Influence of secondary thermal cycle on softening behavior and mechanism of heat affected zone in TIG-welded spray formed 7055 aluminum alloy10.1016/j.jmrt.2022.10.062 ↗
3. Studies on softening behavior and mechanism of heat-affected zone of spray formed 7055 aluminum alloy under TIG welding10.1016/j.jmrt.2022.03.074 ↗
4. Changing the solidification sequence and the morphology of iron-containing intermetallic phases in AA6061 aluminum alloy processed by spray forming10.1016/j.matchar.2018.09.006 ↗
5. Microstructure analysis and low-cycle fatigue behavior of spray-formed Al–Li alloy 2195 extruded plate10.1016/j.msea.2018.11.053 ↗
6. Friction stir welding: An alternative to fusion welding for better stress corrosion cracking resistance of maraging steel10.1016/j.jmapro.2016.11.005 ↗
7. Microstructure and residual stress distributions in friction stir welding of dissimilar aluminium alloys10.1016/j.matdes.2015.08.050 ↗
8. Weld temperature effects during friction stir welding of dissimilar aluminum alloys 6061-t6 and 7075-t610.1007/s00170-013-5485-9 ↗
9. Effect of weld thermal cycle on metallurgical and corrosion behavior of friction stir weld joint of AA2014 aluminium alloy10.1016/j.jmapro.2018.12.001 ↗
10. Corrosion behavior and mechanical properties of Al-Zn-Mg aluminum alloy weld10.1016/j.corsci.2017.05.007 ↗
11. Effect of welding parameters on microstructure and mechanical properties of friction stir welded joints of a super high strength Al–Zn–Mg–Cu aluminum alloy10.1016/j.matdes.2014.10.055 ↗
12. Local melting mechanism and its effects on mechanical properties of friction spot welded joint for Al-Zn-Mg-Cu alloy10.1016/j.jmst.2017.11.014 ↗
13. Enhancing the mechanical performances of friction stir lap welded Al-Zn-Mg-Cu alloy joint by promoting diffusion of alloying element Zn toward the pre-positioned Cu interlayer10.1016/j.msea.2021.142467 ↗
14. Stress corrosion behavior and microstructure analysis of Al-Zn-Mg-Cu alloys friction stir welded joints under different aging conditions10.1016/j.corsci.2022.110821 ↗
15. A look in the corrosion of aluminum alloy friction stir welds10.1016/j.scriptamat.2007.10.043 ↗
16. Microstructure evolution and stress corrosion cracking sensitivity of friction stir welded high strength AA7085 joint10.1016/j.matdes.2021.110297 ↗
17. Relationship between microstructure, microhardness and corrosion sensitivity of an AA 2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
18. Microstructure evolution and its effect on the corrosion of dissimilar aluminum alloys friction stir welding joint10.1016/j.corsci.2023.111249 ↗
19. Effect of microstructure inhomogeneity on creep behavior of friction stir welding 7B50-T7451 aluminum alloy thick plate joint10.1016/j.matchar.2022.112292 ↗
20. Corrosion protection of AA7449-T7951 friction stir welds by laser surface melting with an Excimer laser10.1016/j.corsci.2011.07.043 ↗
21. Corrosion susceptibility of peened friction stir welded 7075 aluminum alloy joints10.1016/j.corsci.2008.09.031 ↗
22. Macro-galvanic effect and its influence on corrosion behaviors of friction stir welding joint of 7050-T76 Al alloy- ScienceDirect
23. Microstructure and Corrosion Behavior of Friction Stir Welded Al Alloy Coated by In Situ Shot-Peening-Assisted Cold Spray10.1007/s40195-019-00966-4 ↗
24. Stress corrosion cracking and hydrogen embrittlement of an Al-Zn-Mg-Cu alloy10.1016/j.actamat.2004.06.023 ↗
25. Hydrogen trapping and embrittlement in high-strength Al-alloys
26. Segregation assisted grain boundary precipitation in a model Al-Zn-Mg-Cu alloy10.1016/j.actamat.2018.07.003 ↗
27. Mechanisms of hydrogen embrittlement in high-strength aluminum alloys containing coherent or incoherent dispersoids, Corrosion Science: The Journal on Environmental Degradation of Materials and Its
28. Effect of Cr, Yb and Zr additions on localized corrosion of Al–Zn–Mg–Cu alloy10.1016/j.corsci.2009.08.001 ↗
29. Effect of Zn content and Sc、Zr addition on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys10.1016/j.jallcom.2023.169246 ↗
30. Effect of Sc microalloying on microstructure evolution and mechanical properties of extruded Al–Zn–Mg–Cu alloys10.1016/j.msea.2021.142197 ↗
31. Effect of recrystallization on intergranular fracture and corrosion of Al–Zn–Mg–Cu–Zr alloy10.1016/j.jallcom.2014.10.044 ↗
32. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
33. Effect of grain size on corrosion of high purity aluminium10.1016/j.electacta.2010.09.023 ↗
34. Effects of Sc and Zr microalloying additions on the microstructure and mechanical properties of new Al–Zn–Mg alloys10.1016/j.jallcom.2012.03.108 ↗
35. Microstructure, mechanical properties and corrosion behavior of commercial 7N01 alloys10.1016/S1003-6326(22)65832-1 ↗
36. Influence of scandium on the pitting behaviour of Al–Zn–Mg–Cu alloys10.1016/j.actamat.2007.08.021 ↗
37. Effect of Scandium Addition on Mechanical Properties and Corrosion Resistance of Medium Strength (Al-Zn-Mg-Cu) Alloy10.4028/www.scientific.net/MSF.794-796.241 ↗
38. Influence of Heat Treatment and Scandium Addition on the Electrochemical Polarization Behavior of Al-Zn-Mg-Cu-Zr Alloy10.1007/s11661-007-9303-6 ↗
39. The influence of Sc and Zr additions on microstructure and corrosion behavior of AA5182 alloy sheet10.1016/j.corsci.2022.110181 ↗
40. The time–temperature–corrosion susceptibility in a 7050-T7451 friction stir weld10.1016/j.msea.2008.03.039 ↗
41. Influence of Processing Parameters on Induced Energy, Mechanical and Corrosion Properties of FSW Butt Joint of 7475 AA10.1007/s11665-011-0074-2 ↗
42. Improvement of weld temperature distribution and mechanical properties of 7050 aluminum alloy butt joints by submerged friction stir welding10.1016/j.matdes.2011.06.021 ↗
43. Microstructural investigation of friction stir welded 7050-T651 aluminium10.1016/S1359-6454(02)00449-4 ↗
44. Avoiding abnormal grain growth in thick 7XXX aluminium alloy friction stir welds during T6 post heat treatments10.1016/j.msea.2021.140901 ↗
45. In-situ investigation on the pitting corrosion behavior of friction stir welded joint of AA2024-T3 aluminium alloy10.1016/j.corsci.2009.10.027 ↗
46. Microstructure and pitting corrosion of friction stir welded joints in 2219-O aluminum alloy thick plate10.1016/j.corsci.2009.07.004 ↗
47. Stress corrosion cracking susceptibility of friction stir welded AA7075–AA6056 dissimilar joint10.1016/j.msea.2004.09.065 ↗
48. Corrosion behaviour of friction stir welded AA7108 T79 aluminium alloy10.1016/j.corsci.2005.02.020 ↗
49. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
50. High-energy and durable aqueous magnesium batteries: Recent advances and perspectives10.1016/j.ensm.2021.09.008 ↗
51. Enhancing the stress corrosion cracking resistance of a low-Cu containing Al-Zn-Mg-Cu aluminum alloy by step-quench and aging heat treatment10.1016/j.corsci.2019.108184 ↗
52. Dislocation-aided electrochemical behavior of precipitates in stress corrosion cracking of Al–Zn–Mg–Cu alloys
53. Friction stir welding/processing of metals and alloys: A comprehensive review on microstructural evolution
54. Microstructure evolution and strengthening mechanisms in friction-stir welded Al–Mg–Sc alloy10.1016/j.msea.2019.138540 ↗
55. Enhanced mechanical property and corrosion resistance of alloy 5182 FSW joints by Sc and Zr alloying10.1016/j.matchar.2022.112412 ↗
56. Microstructure evolution during FSW/FSP of high strength aluminum alloys10.1016/j.msea.2005.06.009 ↗
57. Two-stage annealing of a cold-rolled Al–Mn–Fe–Si alloy with different microchemistry states10.1016/j.jmatprotec.2015.02.016 ↗
58. Microstructural origins of mechanical and electrochemical heterogeneities of friction stir welded heat-treatable aluminum alloy
59. Experimental study on temperature distributions within the workpiece during friction stir welding of aluminum alloys10.1016/j.ijmachtools.2007.12.003 ↗
60. Solution hardening by tetragonal dist ortions: Application to irradiation hardening in F.C.C. crystals10.1016/0001-6160(62)90098-6 ↗
61. Substitutional solution hardening10.1016/0001-6160(63)90213-X ↗
62. The dislocation distribution, flow stress, and stored energy in cold-worked polycrystalline silver10.1080/14786436008238300 ↗
63. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
64. Achieving excellent corrosion resistance properties of 7075 Al alloy via ultrasonic surface rolling treatment10.1016/j.jallcom.2022.165009 ↗
65. Effects of Sc and Zr microalloying additions and aging time at 120 °C on the corrosion behaviour of an Al–Zn–Mg alloy10.1016/j.corsci.2012.08.024 ↗
66. Effect of grain boundary characteristics on intergranular corrosion resistance of 6061 aluminum alloy extrusion10.1007/s11661-002-0274-3 ↗
67. Improvement of Mechanical Properties of 7475 Based Aluminum Alloy Sheets by Controlled Warm Rolling10.2320/matertrans.45.69 ↗
68. Sequence of steps in the pitting of aluminum by chloride ions10.1016/S0010-938X(02)00231-7 ↗
69. In-situ nanoscopic observations of dealloying-driven local corrosion from surface initiation to in-depth propagation10.1016/j.corsci.2020.108912 ↗
70. Local corrosion mechanism of an Al-Zn-Mg-Cu alloy in oxygenated chloride solution: Cathode activity of quenching-induced η precipitates10.1016/j.corsci.2021.109743 ↗