Intrinsic control mechanism of impact toughness and fracture toughness in X80 pipeline girth weld with heterogeneous microstructure
Source abstract
Abstract
Two different heterogeneous microstructures were designed in X80 pipeline girth weld to investigate the control mechanism of impact toughness and fracture toughness. The results show that abundant dislocations in coarse network grain boundary ferrite can slip and accumulate during the slow fracture toughness process, forming large plastic zone and high hardness increase, which significantly improves fracture toughness. However, in the process of rapid Charpy impact process, the dislocation of coarse network grain boundary ferrite is difficult to slip and accumulate, and a large number of secondary cracks are generated here, resulting in impact toughness much lower than weld metals containing fine network ferrite.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Room temperature creep behaviors of base metal and welding materials for X80 pipeline steel10.1016/j.msea.2022.144038 ↗
2. The occurrence of deformation induced ferrite transition (DIFT) during back heating assisted friction stir welding pipeline steel: the influence on the toughness of welded joint10.1016/j.msea.2022.142697 ↗
3. Effects of different microstructural parameters on the corrosion and cracking resistance of pipeline steels: a review10.1016/j.engfailanal.2024.108065 ↗
4. Pipeline failures in corrosive environments – a conceptual analysis of trends and effects10.1016/j.engfailanal.2015.03.004 ↗
5. A quantitative relation for the ductile-brittle transition temperature in pipeline steel10.1016/j.scriptamat.2024.116023 ↗
6. Fatigue properties of ferrite/bainite dual-phase X80 pipeline steel welded joints10.1080/13621718.2016.1219120 ↗
7. Effect of deviation of welding parameters on mechanical properties of X80 steel girth weld10.1016/j.jmrt.2022.12.158 ↗
8. Oil pipeline leakage monitoring developments in China
9. Hydrogen embrittlement in hydrogen-blended natural gas transportation systems: a review10.1016/j.ijhydene.2023.04.266 ↗
10. Review and discussion of strength mismatch of girth welds in high strength pipelines10.1016/j.ijpvp.2023.105118 ↗
11. Simultaneously enhancing strength and fracture toughness via tailoring the microstructure in X80 girth weld metal10.1016/j.jmrt.2024.01.283 ↗
12. Effect of strain aging on mechanical properties and engineering critical assessment of X80 girth weld metal10.1016/j.ijpvp.2023.105071 ↗
13. Effect of heat input and heat treatment on the microstructure and toughness of pipeline girth friction welded API 5L X65 steel10.1016/j.msea.2021.142588 ↗
14. Effect of welding heat input on grain boundary evolution and toughness properties in CGHAZ of X90 pipeline steel10.1016/j.msea.2018.03.029 ↗
15. Effect of grain boundary ferrite morphologies on impact toughness of X80 girth weld10.1016/j.matlet.2024.137412 ↗
16. Evaluation of the fracture toughness of X70 pipeline steel with ferrite-bainite microstructure10.1016/j.msea.2017.01.043 ↗
17. Effects of Cr and Ni addition on critical crack tip opening displacement (CTOD) and supercritical CO2 corrosion resistance of high-strength low-alloy steel (HSLAs)10.1016/j.msea.2024.146772 ↗
18. Pressure reduction strategy based on a new CTOD model considering room temperature creep for X80 pipeline steel10.1016/j.engfracmech.2023.109479 ↗
19. Microstructure and properties of the interlayer heat-affected zone in X80 pipeline girth welds10.1016/j.pnsc.2019.08.010 ↗
20. Embrittlement mechanism of 460 MPa-grade nuclear power steel deposited after heat treatment10.1016/j.ijpvp.2023.104920 ↗
21. Hydrogen embrittlement susceptibility of X70 pipeline steel weld under a low partial hydrogen environment10.1016/j.ijhydene.2020.06.199 ↗
22. Study on the effect of microstructure on toughness dispersion of X70 steel girth weld10.1016/j.engfailanal.2024.108671 ↗
23. Comparative study of microstructure and toughness of automatic welded joints of X70 pipeline steel with no slope and 25° slope10.1016/j.ijpvp.2023.105054 ↗
24. Evolution of weld metal microstructure in shielded metal arc welding of X70 HSLA steel with cellulosic electrodes: a case study10.1016/j.matchar.2015.07.032 ↗
25. Influence of the interpass temperature on the microstructure and mechanical properties of the weld metal (AWS A5.18 ER70S-6) of a narrow gap welded API 5L X70 pipe joint10.1016/j.ijpvp.2022.104690 ↗
26. Computational prediction of mechanical properties of a C-Mn weld metal based on the microstructures and micromechanical properties10.1016/j.msea.2017.01.023 ↗
27. Effect of bainite morphology on deformation compatibility of mesostructure in ferrite/bainite dual-phase steel: Mesostructure-based finite element analysis10.1016/j.matdes.2019.107870 ↗
28. FEM modeling of the flow curves and failure modes of dual phase steels with different martensite volume fractions using actual microstructure as the representative volume10.1016/j.commatsci.2012.07.032 ↗
29. Fracture mechanism of 316L/BNi-2 brazed joints using experiment and microstructure-based model10.1016/j.jmapro.2023.07.005 ↗
30. Improved microstructure heterogeneity and low-temperature fracture toughness of C–Mn weld metal through post weld heat treatment10.1016/j.msea.2019.138541 ↗
31. Correlation between heterogeneous micromechanical properties and fracture toughness in X80 girth weld
32. Correlation between the strain rate sensitivity exponent m and microstructure evolution during hot deformation of an as-cast TiAl alloy10.1016/j.matchar.2023.113050 ↗
33. Coupling effects of temperature and strain rate on the mechanical behavior and microstructure evolution of a powder-plasma-arc additive manufactured high-entropy alloy with multi-heterogeneous microstructures10.1016/j.actamat.2024.120147 ↗
34. The transition from strain rate insensitivity to sensitivity of Ti–6Al–4V alloys deformed at cryogenic temperature10.1016/j.msea.2024.146627 ↗
35. Strain-rate and size dependence of gradient lamellar nickel investigated by in-situ micropillar compression10.1016/j.jmrt.2024.08.129 ↗
36. Effect of heat treatment on tensile properties, impact toughness and plane-strain fracture toughness of sand-cast mg-6Gd-3Y-0.5Zr magnesium alloy10.1016/j.msea.2017.08.100 ↗
37. Evaluation of fracture toughness and impact toughness of laser rapid manufactured Inconel-625 structures and their co-relation10.1016/j.matdes.2014.03.013 ↗
38. Intrinsic control mechanism of tensile and impact toughness of TC21 titanium alloy
39. Mechanisms of toughness improvement in Charpy impact and fracture toughness tests of non-heat-treating cold-drawn steel bar10.1016/j.msea.2013.02.011 ↗
40. Method for manufacturing super large diameter thick wall X80 steel grade spiral submerged arc welded pipe, involves unwinding and leveling, where shielding gas is mixed gas of argon and welding process comprises internal welding process
41. ISO 15653:2018 · 2018
42. ISO 148-1:2016 · 2016
43. ISO 26843:2015 · 2015
44. ISO 6892-1:2019 · 2019
45. Mn-controlled martensitic variant selection significantly affects the strength and toughness of 2.3 GPa ultra-high strength spring steel10.1016/j.msea.2024.147131 ↗
46. Deformation behaviors and cyclic strength assessment of AZ31B magnesium alloy based on steady ratcheting effect10.1016/j.msea.2018.03.023 ↗
47. Ce addition enabling superior strength and ductility combination of a low-carbon low-manganese transformation-induced plasticity steel10.1016/j.msea.2022.143474 ↗
48. Geometrically necessary boundaries, incidental dislocation boundaries and geometrically necessary dislocations10.1016/S1359-6462(02)00358-5 ↗
49. Effects of local-brittle-zone (LBZ) microstructures on crack initiation and propagation in three Mo-added high-strength low-alloy (HSLA) steels10.1016/j.msea.2019.05.120 ↗
50. Effect of hydrogen on microstructure evolution and properties of high-strain pipeline steel under cyclic strain loading10.1016/j.corsci.2024.112148 ↗
51. In-situ EBSD study of the coordinated deformation behavior of 2205 duplex stainless steel fabricated via laser powder bed fusion during the tensile process10.1016/j.msea.2024.146572 ↗
52. The conflicts between strength and toughness10.1038/nmat3115 ↗
53. Extraordinary fracture toughness in nickel induced by heterogeneous grain structure10.1016/j.msea.2021.142313 ↗
54. Superior fracture toughness with high yield strength in a high-Mn steel induced by heterogeneous grain structure10.1016/j.matdes.2022.111473 ↗
55. Effect of bimodal microstructure on the tensile properties and fracture toughness of extruded mg-9Gd-4Y-0.5Zr alloy10.1016/j.msea.2023.145587 ↗